The study of the technological characteristics of the formation of a composite ma-terial based on aluminum alloy using microplastic deformation

Karmyshev I.E., Krasnov E.I.
Karmyshev I.E., Krasnov E.I. The study of the technological characteristics of the formation of a composite ma-terial based on aluminum alloy using microplastic deformation // Proceedings of VIAM. 2015. No. 11. DOI: 10.18577/2307-6046-2015-0-11-3-3. URL: https://www.viam-works.ru/en/journal/2015/11/3
Abstract

The paper presents the results of a study of the technological characteristics of the formation of a composite material based on aluminum, reinforced with discrete boron fibers. Since boron has anomalously large neutron- absorption cross- section, the coating of a composite material with the addition of boron can be used as protection against thermal neutrons of gamma detectors of the outer surface of downhole geophysical devices. With the development of new technologies equipment decreases in size, the number of devices increases and free space in which protection system is placed becomes less. The use of this material allows manufacturing protective coating with a thickness of 1,5 mm and it provides much higher attenuation of the thermal neutron flux than currently used materials with a layer thickness of 5 mm. The results of test for thermocycling of composite material samples with different volume fraction of reinforcing agent (from 30 to 50 vol. %) are shown.

Reference list
  1. Alyuminievye splavy [Aluminium alloys] /V kn. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i ljudi; Pod obshh. red. E.N. Kablova. M.: VIAM. 2012. S. 143–156.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – a basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  6. Tarasov Ju.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [New materials VIAM – for the perspective aircraft equipment of production of JSC «OAK»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  7. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol napravlennoj kristallizacii v resursosberegayushhej tehnologii proizvodstva detalej GTD [Role of the directed solidification in the resource-saving production technologies of details of GTE] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
  8. Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  9. Kurganova Ju.A. Perspektivy razvitija metallomatrichnyh kompozicionnyh materialov promyshlennogo naznacheniya [Prospects of development of metalmatrix composite materials of industrial function] //Servis v Rossii i za rubezhom. 2012. T. 30. №3. S. 235–240.
  10. Kurganova Ju.A., Chernysheva T.A., Kobeleva L.I., Kurganov S.V. Jekspluatacionnye harakteristiki aljumomatrichnyh dispersnouprochnennyh kompozicionnyh materialov i perspektivy ih ispolzovaniya na sovremennom rynke konstrukcionnyh materialov [Operational characteristics the alum-matrix the disperse hardened of composite materials and prospect of their use in the modern market of constructional materials] //Metally. 2011. №4. S. 71.
  11. Chawla N., Chawla K.K. Metal Matrix Composites /In: Springer Sсience+Business Media. Inc. 2006. 401 p.
  12. Filippov E.M., Polak L.S. Prikladnaya yadernaya geofizika [Applied nuclear geophysics]. M.: Izd-vo AN SSSR. 1962. 579 s.
  13. Aliev A.N., Drynkin V.I., Lejkunskaja D.I., Kasatkin V.A. Yaderno-fizicheskie konstanty dlya nejtronnogo aktivacionnogo analiza [Nuclear and physical constants for the neutron activation analysis]: Spravochnik. M.: Atomizdat. 1969. 326 s.