Chutskova E.U., Aleksashin V.M., Barinov D.Y., Dement’eva L.A. The differential scanning calorimetry application for kinetic regularities investigation of the epoxy adhesive VK-36R curing process // Proceedings of VIAM. 2015. No. 1. DOI: 10.18577/2307-6046-2015-0-1-12-12. URL: https://www.viam-works.ru/en/journal/2015/1/12
Abstract
The reaction heat of the curing epoxy adhesive VK-36R was measured by differential scanning calorimetry. Kinetic calculations based on them were produced. A kinetic model of the curing reaction of the epoxy binder was developed. On the basis of the kinetic model change in concentrations of reactants and the degree of conversion in the polymerization process according to the selected kinetic model were evaluated. The study features of the epoxy adhesive multi-stage curing reaction were revealed.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and processing technologies for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Aleksashin V.M., Antjufeeva N.V. Razvitie metodov termicheskogo analiza v issledovanijah polimernyh kompozicionnyh materialov [Development of thermal analysis studies polymeric composite materials] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj. nauch.-tehnich. sb. M.: VIAM. 2007. S. 245–249.
- ASTM E 698–05. Standard Test Method for Arrehenius Kinetic Constants for Thermally Unstable Materials.
- ASTM E 2041–04. Standard Test Method for Heat of Reaction of Thermally Reactive Materials by Differential Scanning Calorimetry (DSC).
- RTM 1.2.161–98. Opredelenie reakcionnoj sposobnosti termoreaktivnyh svjazujushhih i prepregov metodom differencial'noj skanirujushhej kalorimetrii [Determination of the reactivity of the thermosetting binder and the prepregs using differential scanning calorimetry]. M.: VIAM. 1998.
- DIN 65467–1999. Sistemy polimernye s usileniem i bez usilenija aviacionno-kosmicheskogo naznachenija. Metod ispytanija s pomoshh'ju differencial'noj skanirujushhej kalorimetrii [Polymeric systems with and without amplification gain aerospace. Test method using differential scanning calorimetry].
- ISO 11357-2:1999. Plastmassy. Differencial'naja skanirujushhaja kalorimetrija (DSC). Chast' 2. Opredelenie temperatury steklovanija [Plastics. Differential Scanning Calorimetry (DSC). Part 2: Determination of glass transition temperature].
- ISO 11357-5:1999. Plastmassy. Differencial'naja skanirujushhaja kalorimetrija (DSC). Chast' 5. Opredelenie harakteristicheskih temperatur i vremeni po krivym reakcii, opredelenie jental'pii reakcii i stepeni prevrashhenija [Plastics. Differential Scanning Calorimetry (DSC). Part 5: Determination of characteristic temperatures and the time for the reaction curve, the determination of the enthalpy of reaction and degree of conversion].
- Loshhinin Ju.V., Pahomkin S.I., Fokin A.S. Vlijanie skorosti nagrevanija pri issledovanii fazovyh prevrashhenij v aljuminievyh splavah metodom DSK [Effect of heating rate in the study of phase transformations in aluminum alloys by DSC] //Aviacionnye materialy i tehnologii. 2011. №2. S. 3–6.
- Akatenkov R.V., Kondrashov S.V., Fokin A.S., Marahovskij P.S. Osobennosti formirovanija polimernyh setok pri otverzhdenii jepoksidnyh oligomerov s funkcializovannymi nanotrubkami [Features of formation of polymer networks when cured epoxy oligomers with funktsializovannymi nanotubes] //Aviacionnye materialy i tehnologii. 2011. №2. S. 31–37.
- Aleksashin V.M. Osobennosti vzaimodejstvija komponentov i vlijanie ih na processy i tehnologiju formirovanija jepoksidnyh organoplastikov [Features of interaction of the components and their influence on the processes and technologies of epoxy organic plastics]: Avtoref. dis. k.t.n. M.: VIAM. 2001. 27 s.
- Antjufeeva N.V., Komarova O.A., Pavlovskij K.A., Aleksashin V.M. Opyt primenenija kalorimetricheskogo kontrolja reakcionnoj sposobnosti preprega KMU-11tr [Experience of using colorimetric reaction control prepreg CMU-11tr] //Trudy VIAM. 2014. №2. St. 06 (viam-works.ru).
- Aleksashin V.M., Aleksandrova L.B., Matveeva N.V., Mashinskaja G.P. Primenenie termicheskogo analiza dlja kontrolja tehnologicheskih svojstv termoreaktivnyh prepregov konstrukcionnyh polimernyh kompozicionnyh materialov [Application of thermal analysis to control the processing properties of thermoset prepregs structural polymer composite materials] //Aviacionnaja promyshlennost'. 1997. №5–6. S. 38–43.
- Antjufeeva N.V., Aleksashin V.M., Zhelezina G.F., Stoljankov Ju.V. Metodicheskie podhody termoanaliticheskih issledovanij dlja ocenki svojstv prepregov i ugleplastikov [Methodological approaches thermoanalytical studies to assess the properties of prepregs and carbon fiber reinforced plastics] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №4. C. 18–27.
- Aleksashin V.M., Antjufeeva N.V. Primenenie metodov termicheskogo analiza dlja issledovanija kleevyh kompozicij [Application of thermal analysis to study the adhesive compositions] //Klei. Germetiki. Tehnologii. 2005. №12. C. 28–31.
- Opfermann J., Delesky H. Optimization of the curing process of epoxy-resin-based casting compounds using the DSC and kinetic analysis //NETZSCH Applications Service. 1995. 30 p.
- Hajrulin I.I., Aleksashin V.M., Petrova A.P. Primenenie metodov termicheskogo analiza dlja issledovanija kleja-rasplava [Application of thermal analysis for the study of hot melt adhesive] //Klei. Germetiki. Tehnologii. 2006. №5. S. 26–30.
- Lukina N.F., Petrova A.P., Kotova E.V. Termostojkie klei dlja izdelij aviakosmicheskoj tehniki [Heat-resistant adhesives for aerospace products] //Trudy VIAM. 2014. №3. St. 06 (viam-works.ru).
- Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [The adhesive prepreg and laminates based on them] //Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
- Prepreg i izdelie, vypolnennoe iz nego [Prepreg and article made from it]: pat. 2427594 Ros. Federacija; opubl. 27.08.2011.
- Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions forming the sixth technological order] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
- Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.