Application of braided preforms for polymer composite materials in civil industries (review)

Vlasenko F.S., Raskutin A.E., Donetskiy K.I.
Vlasenko F.S., Raskutin A.E., Donetskiy K.I. Application of braided preforms for polymer composite materials in civil industries (review) // Proceedings of VIAM. 2015. No. 1. DOI: 10.18577/2307-6046-2015-0-1-5-5. URL: https://www.viam-works.ru/en/journal/2015/1/5
Abstract

The article considers examples of braided preforms application for PCM in various branches of economy , such as construction, machine building, sports and leisure, aero-space industry. Considered the advantages of PCM based on braided preforms as com-pared to composite materials produced by alternative technologies and traditionally used materials.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and processing technologies for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S.
  2. S. 7–17.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  5. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for advanced manufacturing methods of structural fiber PKM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  6. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  7. Kablov E.N., Kondrashov S.V., Jurkov G.Ju. Perspektivy ispol'zovanija uglerodsoderzhashhih nanochastic v svjazujushhih dlja polimernyh kompozicionnyh materialov [Prospects for the use of carbonaceous nanoparticles in binders for polymer composites] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  8. Dushin M.I., Hrul'kov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovlenija izdelij iz PKM metodom propitki pod davleniem [Especially the manufacture of PCM by pressure impregnation] //Aviacionnye materialy i tehnolo-gii. 2012. №1. C. 18–26.
  9. Low-Toxicity, high-temperature polyimides: pat. 99/36462 WO; pabl. 22.07.1999.
  10. Composition of and method for making high performance resins for infusion and transfer molding processes: pat. 6359107 US; pabl. 19.03.2002.
  11. Postnova M.V., Postnov V.I. Opyt razvitija bezavtoklavnyh metodov formovanija PKM [Experience in the development of methods of forming RMB bezavtoklavnogo] //Trudy VIAM. 2014. №4. St. 06 (viam-works.ru).
  12. Borshhev A.V., Hrul'kov A.V., Halturina D.S. Izgotovlenie nizkoporistogo polimernogo kompozicionnogo materiala dlja primenenija v slabo- i srednenagruzhennyh konstrukcijah [Production of low porosity of the polymer composite material for use in low- and moderate constructions] //Trudy VIAM. 2014. №7. St. 03 (viam-works.ru).
  13. Doneckij K.I., Hrul'kov A.V., Kogan D.I. i dr. Primenenie ob`emno-armirujushhih preform pri izgotovlenii izdelij iz PKM [Use volumetric reinforcing preforms in the manufacture of PCM articles] //Aviacionnye materialy i tehnologii. 2013. №1. S. 35–39.
  14. Internet resurs www.braider.com.
  15. Perepelkin K.E. Armirujushhie volokna i voloknistye polimernye kompozity [Reinforcing fibers and fibrous polymer composites]. SPb.: Nauchnye osnovy tehnologii. 2009. 380 s.
  16. Rapidly deployable lightweight load resisting arch system: pat. 2006/0174549A1 US; pabl. 10.08.2006.
  17. Composite construction members and method of making: pat. 2011/0012282A1 US; pabl. 20.01.2011.
  18. Internet resurs http://www.maine.gov/mdot/tr/bridgebackpack.htm.
  19. Internet resurs http://www.aitbridges.com/compositebridgesystem.
  20. Zdraveva E., Gonilho-Pereira C., Lanceros-Mendez S. et al. Вraided composite rods for civil construction applications //Advanced Materials Research. 2010. V. 123–125. P. 149–152.
  21. Kollmannsberger A., Brand M., Drechsler K. Braiding a convertible windscreen frame with concave sections //JEC Composite Magazine. 2012. №74. P. 24–25.
  22. Carbon/magnesium wheels for high-performance vehicles //JEC Composite Magazine. 2012. №71. P. 36–37.
  23. Inai R., Chirwa E.C., Saito H., Uozumi T., Nakai A., Hamada H. Experimental investigation on the crushing properties of carbon fibre braided composite tubes //International Journal of Crashworthiness. 2003. V. 8. №5. P. 513–521.
  24. Huawu Liu, Yongxin Yang, Shijie Shen et al. Crash Energy Absorption of Braided Composite Tubes and its Application in Vehicle Passive Safety //Advanced Materials Research. 2012. V. 627. P. 659–671.
  25. Okano M., Sugimoto K., Saito H. et al. Effect of the braiding angle on the energy absorption properties of a hybrid braided FRP tube /Proceedings of the Institution of Mechanical Engineers. Part L. 2005. V. 219. №1. P. 59.
  26. Erber А., Birkefeld K., Drechsler K. The influence of braiding configuration on damage tolerance of drive shafts /SAMPE EUROPE 30-th international Jubilee Conference and Forum. Paris. 2010. P. 364–371.
  27. Braided reinforcement for aircraft fuselage frames and method of producing the same: pat. 8210086B2 US; pabl. 03.07.2012.
  28. Griffiths B. Composite fan blade containment case //High-performance Composites. 2005. №5. P. 76–78.
  29. JEC Innovation Awards Program 2012: Innovation awards winners //JEC Composite Magazine. 2012. №71. P. 51.