High-temperature flexible fibrous insulation material

Babashov V.G., Varrik N.M.
Babashov V.G., Varrik N.M. High-temperature flexible fibrous insulation material // Proceedings of VIAM. 2015. No. 1. DOI: 10.18577/2307-6046-2015-0-1-3-3. URL: https://www.viam-works.ru/en/journal/2015/1/3
Abstract

Main methods of manufacture of flexible high-temperature fibrous materials for seal-ing and thermal insulation are considered. The method of manufacture of flexible thermal insulation of high-temperature alumina fiber with addition of low-cost and durable quartz fiber was offered and tested, basic properties of the manufactured material are studied. Results of research showed that the suggested method allows to produce an inexpensive flexible heat-insulating material for using at temperatures up to 1400°С on the basis of home raw materials, which is not inferior to world analogs in characteristics.

Reference list
  1. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotempera-turnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  5. Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic alumina fibers and materials based on them] //Steklo i keramika. 2012. №4. S. 32–36.
  6. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature insulating and heat-proof materials for fiber-based refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  7. Balinova Ju.A., Kirienko T.A. Nepreryvnye vysokotemperaturnye oksidnye volokna dlja teplozashhitnyh, teploizoljacionnyh i kompozicionnyh materialov [Continuous high temperature oxide fibers for thermal protection, thermal insulation and composite materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №4. S. 24–29.
  8. Sposob poluchenija vysokotemperaturnogo volokna na osnove oksida aljuminija [A method for producing high-fiber alumina-based]: pat. 2212388 Ros. Federacija; opubl. 20.09.2003. Bjul. №34. 6 s.
  9. Balinova Ju.A. Nepreryvnye polikristallicheskie volokna oksida aljuminija dlja kompozicionnyh materialov [Continuous polycrystalline alumina fibers for composite materials]: Avtoref. dis. k.t.n. M.: VIAM. 2012. 19 s.
  10. Shhetanov B.V., Shheglova T.M., Balinova Ju.A. Izgotovlenie, struktura i svojstva polikristallicheskih volokon oksida aljuminija [Manufacturing, Structure and properties of polycrystalline alumina fibers] /V sb. materialov 29-j Mezhdunarodnoj konf. «Kompozicionnye materialy v tehnologii». Jalta. 2009. S. 148–150.
  11. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous fibers of polycrystalline α-Al2O3] //Aviacionnye materialy i tehno-logii. 2012. №1. S. 13–17.
  12. Balinova Ju.A., Shheglova T.M., Ljuljukina G.Ju., Timoshin A.S. Osobennosti formiro-vanija α-Al2O3 v polikristallicheskih voloknah s soderzhaniem oksida aljuminija 99% v prisutstvii dobavok Fe2O3, MgO, SiO2 [Features of forming α-Al2O3 in polycrystalline fibers with an alumina content of 99% in the presence of additives Fe2O3, MgO, SiO2] //Trudy VIAM. 2014. №3. St. 03 (viam-works.ru).
  13. Alumina fiber structure and process for production: pat. 4931239 US; pabl. 05.06.1990.
  14. Flexible nonwowen mat: pat. 5380580 US; pabl. 10.06.1995.
  15. Method of making of fibre-based products and their used: pat. 6733628 UK; pabl. 11.05.2004.
  16. Ivahnenko Ju.A., Babashov V.G., Basargin O.V., Butakov V.V. Model' povedenija volokni-stogo materiala pri izgibe [Model behavior flexural fibrous material] //Vse materialy. Jenciklopedicheskij spravochnik. Prilozhenie «Kommentarii k standartam, TU, sertifikatam». 2012. №12. S. 12–15.
  17. Lugovoj A.A., Babashov V.G., Karpov Ju.V. Temperaturoprovodnost' gradientnogo teploizoljacionnogo materiala [The thermal diffusivity of the gradient insulating material] //Trudy VIAM. 2014. №2. St. 02 (viam-works.ru).
  18. Process for producing laminated sheet comprising alumina fiber precursor: pat. 6602369 US; pabl. 10.07.2003.
  19. Alumina fiber aggregate and its production method: pat. 6746979 US; pabl. 08.06.2004.
  20. Process for producing continuous alumina fiber blanket: pat. 7033537 US; pabl. 25.04.2006.
  21. Varrik N.M. Termostojkie volokna i teplozvukoizoljacionnye ognezashhitnye materialy [Heat-resistant fibers and sound insulation fireproofing materials] //Trudy VIAM. 2014. №6. St. 07 (viam-works.ru).