The aramid layered and woven material for protection against impact and ballistic influences

Shuldeshova P.M., Zhelezina G.F.
Shuldeshova P.M., Zhelezina G.F. The aramid layered and woven material for protection against impact and ballistic influences // Proceedings of VIAM. 2014. No. 9. DOI: 10.18577/2307-6046-2014-0-9-6-6. URL: https://www.viam-works.ru/en/journal/2014/9/6
Abstract

Article is devoted to research of the aramid layered and woven material intended for protective structures, in particular for reinforcements of the fan frame of an aviation turbojet. The material will provide the impenetrability of the frame in case of fan blades failure. An influence of composition and structure of the layered and woven material on its impact and ballistic resistance is considered.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Gunjaev G.M., Krivonos V.V., Rumjancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukcijah letatel'nyh apparatov [Polymer composite materials in the construction of aircraft] //Konversija v mashinostroenii. 2004. №4 (65). S. 65–69.
  4. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aircraft equipment] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  5. Zhelezina G.F. Konstrukcionnye i funkcional'nye organoplastiki novogo pokolenija [Structural and Functional organoplastics new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  6. Zhelezina G.F. Osobennosti razrushenija organoplastikov pri udarnyh vozdejstvijah [Features destruction organic plastics under Impact] //Aviacionnye materialy i tehnologii. 2012. №S. S. 272–277.
  7. Shul'deshova P.M., Zhelezina G.F. Vlijanie atmosfernyh uslovij i zapylennosti sredy na svojstva konstrukcionnyh organoplastikov [Effects of atmospheric conditions and dusty environment on the structural properties of organic plastics] //Aviacionnye materialy i tehnologii. 2014. №1. S. 64–68.
  8. Zhelezina G.F., Shul'deshova P.M. Konstrukcionnye organoplastiki na osnove plenochnyh kleev [Structural organoplastics based film adhesives] //Klei. Germetiki. Tehnologii. 2014. №2. S. 9–14.
  9. Prepreg i stojkoe k udaru i ballisticheskomu vozdejstviju izdelie, vypolnennoe iz nego [Prepreg and resistant to impact and ballistic impact of a product made from it]: pat. 2304270 Ros. Federacija; opubl. 27.02.08.
  10. Zhelezina G.F., Solov'eva N.A., Orlova L.G., Vojnov S.I. Ballisticheski stojkie aramidnye sloisto-tkanye kompozity dlja aviacionnyh konstrukcij [Ballistic aramid-layered woven composites for aircraft structures] //Vse materialy. Jenciklopedicheskij spravochnik. Kompozicionnye materialy. 2012. №12. S. 23–26.
  11. Deev I.S., Kobec L.P. Issledovanie mikrostruktury i osobennostej razrushenija jepoksidnyh polimerov i kompozicionnyh materialov na ih osnove. Ch. 1 [The microstructure and fracture features of epoxy polymers and composite materials based on them] //Materialovedenie. 2010. №5. S. 8–16.
  12. Deev I.S., Kobec L.P. Issledovanie mikrostruktury i osobennostej razrushenija jepoksidnyh polimerov i kompozicionnyh materialov na ih osnove. Ch. 2 [The microstructure and fracture features of epoxy polymers and composite materials based on them] //Materialovedenie. 2010. №6. S. 13–18.
  13. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Research and development and autoclave molding technology bezavtoklavnogo RMB] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  14. Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokolenija [Modern technologies of production of polymer composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  15. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Structural and heat-resistant adhesives] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  16. Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, poluchennye putem propitki plenochnym svjazujushhim [Polymer composite material obtained by impregnating a film binder] //Vse materialy. Jenciklopedicheskij spravochnik. Kompozicionnye materialy. 2011. №11. S. 2–6.
  17. Kogan D.I., Chursova L.V., Petrova A.P. Tehnologija izgotovlenija PKM sposobom propitki plenochnym svjazujushhim [Manufacturing technology RMB impregnation method binder film] //Klei. Germetiki. Tehnologii. 2011. №6. S. 25–29.
  18. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Melt binders for advanced methods of manufacturing a new generation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  19. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binders for the promising methods for the manufacture of structural fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.