Bespalova E.E., Beljaev А.А., Romanov A.M., Shirokov V.V. Investigation of the dielectric characteristics of designed for anechoic chambers laminated radar absorbing material layers based with carbonized fiber filled foam asbestos // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-12-12. URL: https://www.viam-works.ru/en/journal/2014/8/12
Abstract

Experimental investigation of the dielectric characteristics of designed for lining of anechoic chambers laminated radar absorbing material layers is performed. The results of measurements on 3 frequencies are compared with the results of calculations. Analysis comparing the measured and calculated characteristics showed close agreement and confirmed the selection of empirical coefficients in the formulas for the calculation of the permittivity of the foam asbestos filled with carbonized fiber.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Beljaev A.A., Kondrashov S.V., Lepeshkin V.V., Romanov A.M. Radiopogloshhajushhie materialy [Radio-absorbing materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 348–352.
  5. Micmaher M.Ju., Torgovanov V.A. Bezjehovye kamery SVCh [Microwave anechoic chambers]. M.: Radio i svjaz'. 1982. 129 s.
  6. Maslov M.Ju., Semakov L.M., Skachkov D.V. Ispytatel'naja bezjehovaja kamera diapazona 30–1200 MGc [Anechoic test range 30-1200 MHz] //Telekommunikacii i transport. 2009. Spec. vyp. «Tehnologii informacionnogo obshhestva». S. 123–125.
  7. Latypova A.F., Kalinin Ju.E. Analiz perspektivnyh radiopogloshhajushhih materialov [Analysis of promising absorbing materials] //Vestnik Voronezhskogo gos. tehn. un-ta. 2012. T. 8. №6. S. 70–76.
  8. Radiopogloshhajushhij material [Radar absorbing material]: pat. 2417491 Ros. Federacija; opubl. 27.04.2011.
  9. Bibikov S.B., Prokof'ev M.V., Kulikovskij K.Je., Zhuravlev V.A. Razrabotka materialov i pokrytij, ispol'zuemyh dlja provedenija radiotehnicheskih ispytanij i obespechenija jelektromagnitnoj sovmestimosti [Development of materials and coatings used for radio testing and electromagnetic compatibility] //Voprosy oboronnoj tehniki. Ser. «Tehnicheskie sredstva protivodejstvija terrorizmu». 2013. №5–6. S. 56–64.
  10. Beljaev A.A., Bespalova E.E., Romanov A.M. Pozharobezopasnye radiopogloshhajushhie materialy dlja bezjehovyh kamer [Fireproof materials for radio-anechoic chambers] //Aviacionnye materialy i tehnologii. 2013. №1. S. 53–55.
  11. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [The possibility of using a silica fiber as a binder in the preparation of a lightweight heat-fiber-based material Al2O3] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8–14.
  12. Volkov V.P., Zeleneckij A.N. i dr. Poluchenie radiozashhitnyh polimernyh materialov ponizhennoj gorjuchesti [Getting radioprotective reduced flammability of polymeric materials] //Plasticheskie massy. 2008. №6. S. 42–46.
  13. Agafonova A.S., Beljaev A.A., Kondrashov Je.K., Romanov A.M. Osobennosti formirovanija monolitnyh konstrukcionnyh radiopogloshhajushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of formation of monolithic structural radar absorbing materials based composites filled with resistive fiber] //Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
  14. Bibikov S.B., Titov A.N., Cherepanov A.K. Sintez materiala s zadannym kojefficientom otrazhenija v shirokom diapazone chastot i uglov padenija [Synthesis of a material with a specified reflectivity in a wide range of frequencies and angles of incidence] /V sb. materialov 15-j Mezhdunarodnoj nauch.-tehnich. konf. «Radiolokacija, navigacija, svjaz'». Voronezh. 2009. S. 1578–1584.
  15. Bibikov S.B., Zasovin Je.A., Cherepanov A.K., Hmel'nik G.I. Matematicheskoe modelirovanie parametrov mnogoslojnyh radiopogloshhajushhih pokrytij [Mathematical modeling of radar parameters of multilayer coatings] /V sb. materialov 15-j Mezhdunarodnoj nauch.-tehnich. konf. «Radiolokacija, navigacija, svjaz'». Voronezh. 2009.
  16. S. 1585–1595.
  17. Oreshkin P.T. Fizika poluprovodnikov i dijelektrikov [Physics of semiconductors and dielectrics]. M.: Vyssh. shkola. 1977. S. 380–392.
  18. King R., Smit G. Antenny v material'nyh sredah [Antennas in material media]. Ch. 1. M.: Mir. 1984. S. 379–384.
  19. Hmel'nik G.I., Bibikov S.B. Statisticheskij analiz zavisimosti parametrov raspredelenija Debaja ot udel'nyh soprotivlenij sloev mnogoslojnogo RPP [Statistical analysis of the relationship of the distribution parameters of the Debye resistivity layers of the multilayer RPP] //Tehnologii jelektromagnitnoj sovmestimosti. 2012. №4 (43). S. 45–51.
  20. Bespalova E.E., Kondrashov Je.K. Osobennosti korrektirovki receptury pozharobezopasnogo materiala dlja bezjehovyh kamer pri izmenenii parametrov radiopogloshhajushhego napolnitelja [Features corrections recipe fireproof material for anechoic chambers when the parameters radar absorbing filler] //Aviacionnye materialy i tehnologii. 2014. №2. S. 48–71.
  21. Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik steklosotoplasta volnovodnym metodom [Investigation of the dielectric characteristics of the waveguide method steklosotoplasta] //Aviacionnye materialy i tehnologii. 2013. №4.
  22. S. 62–68.
  23. Beljaev A.A., Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik monolitnyh stekloplastikov radiotehnicheskogo naznachenija [Investigation of the dielectric characteristics of monolithic GRP radiotechnical destination] //Kompozitnyj mir. 2014 (v pechati).
  24. Beljaev A.A., Romanov A.M., Shirokov V.V., Shul'deshov E.M. Izmerenie dijelektricheskoj pronicaemosti steklosotoplasta v svobodnom prostranstve [Measurement of the permittivity in free space steklosotoplasta] //Trudy VIAM. 2014. №5. St. 06 (viam-works.ru).