Research of the reasons of emergence of sites with different morphology of a break in shod preparations from steel 38HN3MFA

Grigorenko V.B., Morozova L.V., Orlov M.R.
Grigorenko V.B., Morozova L.V., Orlov M.R. Research of the reasons of emergence of sites with different morphology of a break in shod preparations from steel 38HN3MFA // Proceedings of VIAM. 2014. No. 8. DOI: 10.18577/2307-6046-2014-0-8-11-11. URL: https://www.viam-works.ru/en/journal/2014/8/11
Abstract

Destruction surface of shod preparations from steel 38ХН3МФА with the lowered sulfur content and phosphorus are investigated. The reasons of formation of sites of dif-ferent morphology in breaks are established.

Reference list
  1. Kablov E.N. Konstrukcionnye i funkcional'nye materialy – osnova jekonomicheskogo i nauchno-tehnicheskogo razvitija Rossii [Structural and functional materials - the basis of economic, scientific and technical development of Russia] //Voprosy materialovedenija. 2006. №1. S. 64–67.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhenyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2.
  4. S. 13–19.
  5. Artes A.Je., Sosenushkin E.N. Problemy proizvodstva krupnyh pokovok v otechestvennom mashinostroenii [Problems of production of large forgings in domestic engineering] //Tehnologija mashinostroenija. 2012. №1. S. 11–15.
  6. Odesskij P.D., Filippov G.A., Livanova O.V., Egorova A.A. Prochnost' sovremennyh stalej dlja osej bol'shogo diametra, primenjaemyh v unikal'nyh inzhenernyh sooruzhenijah [Strength steels for modern large diameter axles used in unique engineering structures] //Problemy chernoj metallurgii i materialovedenija. 2012. №2. S. 31–38.
  7. Shevcova O.A., Zjuban N.A., Ruckij D.V. Osobennosti formirovanija sul'fidnyh vkljuchenij i ih vlijanija na kachestvo nizkolegirovannyh konstrukcionnyh stalej [Features of formation of sulphide inclusions and their impact on the quality of low-alloy structural steels] //Metallurg. 2010. №12. S. 54–57.
  8. Zjuban N.A., Krjuchkov O.B. Vlijanie vakuumirovanija na osobennosti formirovanija sul'fidnyh vkljuchenij i svojstva izdelij iz nizkolegirovannyh konstrukcionnyh stalej [Effect of vacuum on the features of formation of sulfide inclusions and properties of the products of low-alloy structural steels] //Izvestija vuzov. Chernaja metallurgija. 2008. №5. S. 15–18.
  9. Smirnov M.A., Schastlivcev V.M., Zhuravlev L.G. Osnovy termicheskoj obrabotki stali [Fundamentals of heat treatment of steel]. M.: Nauka i tehnologii. 2002. 519 s.
  10. Borisov I.A., Dub A.V. Vlijanie prodolzhitel'nosti vysokogo otpuska na teksturu i zerno peregretoj rotornoj stali [Effect of high-temperature tempering the texture and grain of superheated steel rotor] //MiTOM. 2013. №3. S. 3–9.
  11. Odesskij P.D., Egorova A.A., Todorova E.V. Analiz avarijnogo izloma jelementa stal'noj konstrukcii [Emergency break element analysis of the steel structure] //Deformacija i razrushenie materialov. 2010. №7. S. 45–48.
  12. Ruckij D.V., Gamanjuk S.B., Zjuban N.A., Poslamovskaja Ju.A. Vlijanie himicheskoj i fizicheskoj neodnorodnosti slitka massoj 24,2 t stali 38HN3MFA na mehanicheskie svojstva trubnyh zagotovok [Effect of chemical and physical heterogeneity ingot weighing 24.2 tons of steel 38HN3MFA on mechanical properties of tubular billets] //Izvestija Samarskogo nauchnogo centra RAN. 2010. T. 12. №1–2. S. 489–492.
  13. Ruckij D.V., Gamanjuk S.B., Zjuban N.A., Chubukov M.Ju. Analiz vnutrennih defektov slitka massoj 103 t stali 38HN3MFA i ocenka ih vlijanija na kachestvo pokovok rotorov turbogeneratorov [Analysis of internal defects ingot weighing 103 tons of steel 38HN3MFA and assess their impact on the quality of forgings turbogenerator rotors] //Tehnologija metallov. 2010. №10. S. 15–18.
  14. Orlov M.R., Ospennikova O.G., Gromov V.I. Zamedlennoe razrushenie stali 38HN3MA v processe dlitel'noj jekspluatacii [Delayed fracture steel 38HN3MA during long operation] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 5–12.
  15. Klevcov G.V., Botvina L.R., Klevcova N.A., Limar' L.V. Fraktodiagnostika razrushenija metallicheskih materialov i konstrukcij [Fraktodiagnostika fracture of metallic materials and structures]. M.: MISiS. 2007. 259 s.
  16. Zhegina I.P., Kotel'nikova L.V., Grigorenko V.B., Zimina Z.N. Osobennosti razrushenija deformiruemyh nikelevyh splavov i stalej [Features destruction wrought nickel alloys and steels] //Aviacionnye materialy i tehnologii. 2012. №S. S. 455–465.
  17. Orlov M.R., Ospennikova O.G., Gromov V.I. Razvitie mehanizmov vodorodnoj i bejnitnoj hrupkosti konstrukcionnoj stali v processe jekspluatacii krupnogabaritnyh konstrukcij [Development of mechanisms for hydrogen brittleness and bainitic structural steel in the operation of large structures] //Aviacionnye materialy i tehnologii. 2012. №S. S. 88–93.
  18. Turchenkov V.A., Baranov D.E., Gagarin M.V., Shishkin M.D. Metodicheskij podhod k provedeniju jekspertizy materialov [Methodical approach to the examination of materials] //Aviacionnye materialy i tehnologii. 2012. №1. S. 47–53.
  19. Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  20. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and X-ray analysis for the study of structural phase state materials] //Trudy VIAM. 2013. №5. St. 06. (viam-works.ru).