Development of VIAM federal state unitary enterprise in the field of adhesives of industrial rubber assignment and being self-glued materials

Tyumeneva T.Y., Zhadova N.S., Lukina N.F.
Tyumeneva T.Y., Zhadova N.S., Lukina N.F. Development of VIAM federal state unitary enterprise in the field of adhesives of industrial rubber assignment and being self-glued materials // Proceedings of VIAM. 2014. No. 7. DOI: 10.18577/2307-6046-2014-0-7-4-4. URL: https://www.viam-works.ru/en/journal/2014/7/4
Abstract

Properties of adhesives of industrial rubber assignment developed in VIAM Federal State Unitary Enterprise, in comparison with domestic and foreign analogs are given. Being self-adhesive materials for temporary operational repair of exterior surface of products of aviation engineering are provided.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kardashov D.A., Petrova A.P. Polimernye klei [Polymer adhesives]. M.: Himija. 1983. 256 s.
  3. Petrova A.P., Donskoj A.A., Chalyh A.E., Shherbina A.A. Klejashhie materialy. Germetiki [Adhesives. Sealants]: Spravochnik. SPb.: NPO «Professional». 2008. 589 s.
  4. Petrova A.P. Osnovnye jetapy tehnologii skleivanija [Main stages of bonding technology] //Klei. Germetiki. Tehnologii. 2014. №2. S. 24–30.
  5. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoj konferencii po klejam i germetikam (WAC-2012, Francija) [Browse by materials of the international conference on adhesives and sealants (WAC-2012, France)] //Trudy VIAM. 2013. №8. St. 06 (viam-works.ru).
  6. Lukina N.F., Anihovskaja L.I., Dement'eva L.A., Petrova A.P., Tjumeneva T.Ju. Klei i klejashhie materialy dlja izdelij aviacionnoj tehniki [Glues and adhesives for aircraft products] //Svarochnoe proizvodstvo. 2007. №5. S. 19–27.
  7. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Structural and heat-resistant adhesives] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  8. Lukina N.F., Dement'eva L.A., Petrova A.P., Tjumeneva T.Ju. Svojstva kleev i klejash-hih materialov dlja izdelij aviacionnoj tehniki [Properties of adhesives and adhesives for aircraft products] //Klei. Germetiki. Teh-nologii. 2009. №1. S. 14–24.
  9. Petrova A.P., Lukina N.F., Dement'eva L.A., Tjumeneva T.Ju., Avdonina I.A., Zhadova N.S. Klei dlja aviacionnyh materialov [Adhesives for aircraft materials] //Rossijskij himicheskij zhurnal. 2010. T. IV. №1. S. 46–52.
  10. Lukina N.F., Dement'eva L.A., Petrova A.P., Tyumeneva T.Y. Rroperties of adhesives and adhesive materials used in aviation industry //Polymer Science. Series D. 2009. V. 2. №3. P. 147–154.
  11. Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Adhesives for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
  12. Petrova A.P., Lukina N.F., Dement'eva L.A., Tyumeneva T.Y., Avdonina I.A., Zhadova N.S. Adhesives for aviation equipment //Russian Journal of General Chemistry. 2011. T. 81. №5. P. 1014–1021.
  13. Tjumeneva T.Ju., Kogtjonkov A.S., Lukina N.F., Chursova L.V. Uspehi v oblasti razrabotki kleev i tehnologij dlja izgotovlenija rezinotehnicheskih izdelij aviacionnogo naznachenija [Progress in the development of adhesives and technologies for the manu-facture of rubber products aviation applications] //Klei. Germetiki. Tehnologii. 2013. №10. S. 7–10.
  14. Tyumeneva T.Y., Lukina N.F. VKR-95 cold-setting adhesive with enhanced strength //Polymer Science. Series D. 2010. T. 3. №2. S. 114–116.
  15. Tjumeneva T.Ju., Lukina N.F. Klei dlja skleivanija rezin mezhdu soboj i s drugimi ma-terialami [Adhesives for bonding rubber between themselves and with other materials] /V sb. materialov dokladov seminara. CRDZ. 2008. S. 11–12.
  16. Sytyj Ju.V., Sagomonova V.A., Kisljakova V.I., Bol'shakov V.A. Novye vibropo-gloshhajushhie materialy [New vibration-absorbing materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 51–54.
  17. Sharova I.A., Zhadova N.S., Lukina N.F. Klejashhie materialy i tehnologii dlja vremennogo operativnogo remonta sotovyh agregatov iz polimernyh kompozicionnyh materialov [Adhesives and technologies for the repair of cellular interim operational units of the polymer composites] //Klei. Germetiki. Tehnologii. 2012. №5. S. 36–39.
  18. Kleevaja kompozicija [The adhesive composition]: pat. 2296789 Ros. Federacija; opubl. 10.04.2007.
  19. Kleevaja kompozicija [The adhesive composition]: pat. 2471842 Ros. Federacija; opubl. 11.05.2011.
  20. Tjumeneva T.Ju., Kogtjonkov A.S., Lukina N.F., Chursova L.V. Vlijanie napolnitelej na svojstva kleev rezinotehnicheskogo naznachenija [Effect of fillers on the properties of rubber-purpose adhesives] //Trudy VIAM. 2014. №4. St. 05 (viam-works.ru).
  21. Dement'eva L.A., Tjumeneva T.Ju., Sharova I.Ju. Klei s ponizhennoj gorjuchest'ju dlja aviacionnoj tehniki [Adhesives with reduced flammability for aircraft] /V sb. dokladov VI Mezhdunarodnoj konf. «Polimernye materialy ponizhennoj gorjuchesti». VoGTU. 2011. S. 127–128.
  22. Samoklejashhijsja material [Self-adhesive material]: pat. 2435812 Ros. Federacija; opubl. 02.06.2010.
  23. Zhadova N.S., Lukina N.F., Tjumeneva T.Ju. Samoklejashhiesja materialy dlja vremennogo operativnogo remonta vneshnej poverhnosti izdelij aviacionnoj tehniki [Self-adhesive materials for temporary operative repair external surfaces of products aircraft] //Klei. Germetiki. Tehnologii. 2012. №6. S. 2–4.