Tear (mode III) of thin laminate polymer composite materials for aircraft
Yakovlev N.O., Erasov V.S., Popov J.O., Kolokoltseva T.V. Tear (mode III) of thin laminate polymer composite materials for aircraft // Proceedings of VIAM. 2014. No. 6. DOI: 10.18577/2307-6046-2014-0-6-12-12. URL: https://www.viam-works.ru/en/journal/2014/6/12
Abstract
For with thin (0,30–0,47 mm) layered (2–4 layers) polymer composite materials with diffe-rent ply orientation direction, including single-ended, on samples with a stress concentrator, created the cut, determined the tear resistance (mode III), analyze the fracture behavior.
Reference list
- Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Carbon and fiberglass new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
- Gunjaev G.M., Krivonos V.V., Rumjancev A.F., Zhelezina G.F. Polimernye kompozicionnye materialy v konstrukcijah letatel'nyh apparatov [Polymer composite materials in aircraft structures] //Konversija v mashinostroenii. 2004. №4 (65). S. 65–69.
- Popov Ju.O., Kolokol'ceva T.V., Bespalova L.S., Hrul'kov A.V., Kogan D.I. Stekloplastik VPS-31 i gibridnyj kompozicionnyj material VKG-5 iz odnonapravlennyh prepregov na osnove rasplavnogo svjazujushhego i zhgutovyh ugle-, steklonapolnitelej [Fiberglass AMS-31 and hybrid composite VCG-5 of unidirectional prepregs based on a melt binder and carbon roving, glass] /V sb. Aviacionnye materialy i tehnologii. 2006. №1. S. 10–20.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
- Davydova I.F., Kavun N.S. Stekloplastiki – mnogofunkcional'nye kompozicionnye materialy [GRP – multifunctional composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
- Antipov V.V., Senatorova O.G., Lukina N.F., Sidel'nikov V.V., Shestov V.V. Sloistye metallopolimernye kompozicionnye materialy [Layered metal-composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
- Antipov V.V., Senatorova O.G., Sidel'nikov V.V. Issledovanie pozharostojkosti sloistyh gibridnyh aljumostekloplastikov klassa SIAL [Flammability Study of layered hybrid class alyumostekloplastikov Sial] //Aviacionnye materialy i tehnologii. 2011. №3. S. 36–41.
- Linxia Gu, Ananth Ram, Mahanth Kasavajhala, Shijia Zhao. Finite element analysis of cracks in aging aircraft structures with bonded //Composites: Part B. 2011. №42. S. 505–510.
- Bachir Bouiadjra B., Ouinas D., Serier B., Benderdouche N. Disbond effects on bonded boron/epoxy composite repair to aluminium plates //Computational Materials Science. 2008. №42. S. 220–227.
- Zhelezina G.F. Konstrukcionnye i funkcional'nye organoplastiki novogo pokolenija [Structural and Functional organoplastics new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
- Zhelezina G.F., Vojnov S.I., Pletin' P.I., Veshkin E.A., Satdinov R.A. Razrabotka i proizvodstvo konstrukcionnyh organoplastikov dlja aviacionnoj tehniki [Development and production of organic plastics for structural aircraft] //Izvestija Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2012. T. 14. №4–2. S. 411–416.
- Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
- Zhelezina G.F. Osobennosti razrushenija organoplastikov pri udarnyh vozdejstvijah [Features destruction organic plastics under Impact] //Aviacionnye materialy i tehnologii. 2012. №S. S. 272–277.
- Krylov V.D. Metody ispytanij i osobennosti razrushenija tonkolistovyh materialov [Test methods and especially the destruction of thin materials] //Aviacionnye materialy i tehnologii. 2013. №4. S. 54–57.
- Jakovlev N.O., Chernatkin S.E., Kuz'ko E.I., Arsenkin A.M., Shtremel' M.A. Oprede-lenie soprotivlenija KIII razdiru tonkih listov [Determination of resistance to tearing of thin sheets KIII] //Zavodskaja laboratorija. 2008. T. 74. №5. S. 54–57.
- Chernatkin S.E., Jakovlev N.O., Kuz'ko E.I., Shtremel' M.A. Sootnoshenija podobija pri razrushenii tonkolistovyh materialov [Similarity relations in the destruction of thin mate-rials] //Fizika metallov i metallovedenie. 2009. T. 108. №2. S. 217–221.
- Borodulin A.S. Svojstva i osobennosti struktur stekljannyh volokon, ispol'zuemyh dlja izgotovlenija stekloplastikov [Properties and features structures of glass fibers used for the manufacture of GRP] //Materialovedenie. 2012. №7. S. 34–37.