Recovery of technology for the beryllium-containing steel VNS-32-VI obtaining
UDC
669.14.018.295:621.78
DOI
10.18577/2307-6046-2014-0-5-1-1
Article PDF (Russian)
(1.05 MB)
How to cite
Shcherbakov A.I., Mosolov A.N., Kalitsev V.A. Recovery of technology for the beryllium-containing steel VNS-32-VI obtaining // Proceedings of VIAM. 2014. No. 5. DOI: 10.18577/2307-6046-2014-0-5-1-1. URL: https://www.viam-works.ru/en/journal/2014/5/1
Abstract
This paper studied metallurgic features of the high-strength beryllium-containing steel VNS-32-VI obtaining including smelting in the vacuum induction furnaces, forging and rolling processes, heat treatment modes of hot-rolled bars with diameter 10–27 mm and forged to 50 mm, intended for hardwearing elements of fuel control apparatus. There were optimized temperature-time parameters of deformation and thermal treatment of bars working. These parameters provided the stability of the mechanical properties and low level of non-metallic inclusions. There were identified the ways of δ-ferrite embrit-tlement phase content decreasing in the steel.
Reference list
- Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [The crea-tion of modern high-temperature materials and manufacturing technologies for aircraft engine] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
- Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhen-nyh detalej gazoturbinnyh dvigatelej [Materials for high-thermal components of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technolo-gies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
- Ospennikova O.G. Strategija razvitija zharoprochnyh splavov i stalej special'nogo naznachenija, zashhitnyh i teplozashhitnyh pokrytij [The development strategy of sup-eralloys and special steel, protective and thermal barrier coatings] //Aviacionnye mate-rialy i tehnologii. 2012. №S. S. 19–36.
- Tonysheva O.A., Voznesenskaja N.M., Shal'kevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnolog-icheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali perehodnogo klassa s povyshennym soderzhaniem azota [Investigation of the influence of high-temperature thermomechanical treatment on the structure, process, mechanical and corrosion properties of high-grade stainless steel transition with a high content of nitrogen] //Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
- Salahova R.K. Korrozionnaja stojkost' stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [The corrosion resistance of steel with 30KhGSA «trivalent» chromium plated in natural and artificial environments] //Aviacionnye materialy i tehnologii. 2012. №2. S. 59–66.
- Bratuhin A.G. Demchenko O.F., Dolzhenkov N.N., Krivonogov G.S. Vysokoprochnye korrozionnostojkie stali sovremennoj aviacii [High-strength corrosion-resistant steel of modern aviation]. M.: MAI. 2006. S. 112–121, 130–143.
- Solncev St.S., Rozenenkova V.A., Mironova N.A., Kas'kov V.S. Kompleksnaja sistema zashhity berillija ot okislenija [Comprehensive system protection against oxidation of beryllium] //Aviacionnye materialy i tehnologii. 2010. №1. S. 12–16.
- Erasov V.S., Grinevich A.V., Senik V.Ja., Konovalov V.V., Trunin Ju.P., Nesterenko G.I. Raschetnye znachenija harakteristik prochnosti aviacionnyh materialov [Calculated values of the strength characteristics of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.
- Voznesenskaja N.M., Izotov V.I., Ul'janova N.V., Popova L.S., Potak Ja.M. Struktura i svojstva vysokoprochnoj nerzhavejushhej stali 1H15N4AM3 [Structure and properties of high strength stainless steel 1H15N4AM3] //MiTOM. 1971. №1. S. 32–35.
- Savvina N.A., Kosarina E.I., Miroshin K.G., Stepanov A.V. Teoreticheskij raschet i prakticheskie sposoby opredelenija verojatnosti obnaruzhenija defektov v aviacionnyh materialah [Theoretical calculation and practical ways to determine the probability of detection of defects in aircraft materials] //Aviacionnye materialy i tehnologii. 2005. №1. S. 16–22.
- Krivonogov G.S., Kablov E.N. Granicy zeren i ih rol' v ohrupchivanii vysokoprochnyh korrozionnostojkih stalej [Grain boundaries and their role in the embrittlement of high-strength stainless steels] //Metally. 2002. №1. S. 35–45.
- Wagatsuma K., Hirokawa Kh. Observation of ion nitriding on Fe–Cr, Fe–Ni and Ni–Cr alloy surfaces in a glow discharge plasma //Surface and interface analisis. 2012. V. 8. №1. P. 37–42.
- Potak Ja.M., Sagalevich E.A. Strukturnaja diagramma deformiruemyh nerzhavejushhih stalej [Structure diagram deformable stainless steels] //MiTOM. 1971. №9. S. 12–16.
- Krivonogov G.S., Kablov E.N. Matematicheskaja model' strukturnoj diagrammy malouglerodistyh korrozionnostojkih stalej i ee primenenie pri razrabotke novyh mate-rialov [Mathematical model of the structural diagram of low carbon stainless steels and its application in the development of new materials] //Metally. 2001. №5. S. 42–48.
- Tonysheva O.A., Voznesenskaja N.M., Eliseev Je.A., Shal'kevich A.B. Novaja vysoko-prochnaja jekonomnolegirovannaja azotsoderzhashhaja stal' povyshennoj nadezhnosti [New high ehkonomnolegirovannyh nitrogen-containing steel increased reliability] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
- Smoljakova M.Ju., Vershinin D.S., Tregubov I.M. Issledovanie vlijanija nizkotempera-turnogo azotirovanija na strukturno-fazovyj sostav i svojstva austenitnoj stali [Investiga-tion of the influence of low-temperature nitridation on the structural and phase composi-tion and properties of austenitic steel] /V sb. dokladov 9-oj Mezhdunarodnoj konf. «Vzaimodejstvie izluchenij s tverdym telom». Minsk. 2011. S. 176–177.
- Kosolapov G.F., Gerasimov S.A. O strukture α-fazy azotirovannogo sloja stali 38H2MJuA i 10H13 [The structure of α-phase steel nitrided layer 38H2MYUA and 10X13] //MiTOM. 2011. №5. S. 71–73.
- Gerasimov S.A., Kuksenova L.I., Lapteva V.G. Struktura i iznosostojkost' azotiro-vannyh konstrukcionnyh stalej i splavov [Structure and wear resistance of nitrided structural steels and alloys]. M.: MGTU im. N.Je. Baumana. 2012. S. 508–509.