High-temperature tensile strength determination of single crystal alumina fibers
Basargin O.V., Shcheglova T.M., Nikitina V.J., Svistunov V.I. High-temperature tensile strength determination of single crystal alumina fibers // Proceedings of VIAM. 2014. No. 4. DOI: 10.18577/2307-6046-2014-0-4-3-3. URL: https://www.viam-works.ru/en/journal/2014/4/3
Abstract
The description of high-temperature tensile strength determination of alumina single crystal fibers in gold image furnace is presented in this paper.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Development Strategy composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
- Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fiber for high temperature ceramic compo-sites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
- Svetlov I.L. Vysokotemperaturnye Nb–Si-kompozity //Materialovedenie. 2010. №9. S. 29–38.
- Orlov M.R. Strategicheskie napravlenija razvitija Ispytatel'nogo centra FGUP «VIAM» [Strategic directions of development of the Testing Center FSUE «VIAM»] //Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
- Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification testing and research strength of aircraft materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
- Instron series 5800-8800 Test Control Systems Reference Manual M21-13770-En Rev. C. 2009.
- Rossolenko S.N., Kurlov V.N., Asrian A.A. Analysis of the profile curves of the menisci for the sapphire tubes growth by EFG (Stepanov) technique //Crystal Research and Technology. 2009. V. 44. №7. P. 689–700.
- Rossolenko S.N., Kurlov V.N., Asrian A.A. Analysis of the profile curves of the menisci for the sapphire capillaries and fibers growth by EFG (Stepanov) technique //Crystal Research and Technology. 2009. V. 44. №7. P. 701–706.
- Rossolenko S.N., Kurlov V.N., Asrjan A.A. Issledovanie profil'nyh krivyh meniskov dlja processa vyrashhivanija kristallov po sposobu Stepanova [Study profile curves meniscus for process of crystal growth in a manner of Stepanov] //Izvestija RAN. 2009. T. 73. №10. S. 1398–1402.
- Kablov E.N., Shhetanov B.V. Metody poluchenija monokristallicheskih volokon oksida aljuminija dlja kompozicionnyh materialov [Methods for producing single crystal alumina fibers for composite materials] /V sb. materialov 29 ezhegodnoj Mezhdu-narodnoj konf. i seminara «Kompozicionnye materialy v promyshlennosti». Jalta. 2009. S. 150–155.
- Milejko S.T., Serebrjakov A.V., Kijko V.M., Kolchin A.A., Kurlov V.N., Novohatskaja N.I., Tolstun A.N. Monokristallicheskie volokna mullita, poluchaemye metodom vnutrennej kristallizacii [Monocrystalline mullite fibers, obtained by internal crystalliza-tion] //Kompozity i nanostruktury. 2009. №2. S. 47–60.
- Shhetanov B.V., Kupcov R.S., Svistunov V.I. Metody poluchenija monokristallich-eskih volokon oksida aljuminija dlja sozdanija kompozicionnyh materialov i vysoko-temperaturnoj volokonnoj optiki [Methods of producing single crystal alumina fibers to create a high-temperature composite materials and fiber optics] //Trudy VIAM. 2013. №4. St. 01 (viam-works.ru).
- Basargin O.V., Nikitina V.Ju., Shheglova T.M., Kolyshev S.G. Osobennosti provedenija prochnostnyh ispytanij v pechi luchevogo nagreva [Features of the strength tests in beam heating furnace] //Steklo i keramika. 2013. №2. S. 6–9.
- Ulvac-Riko Infrared gold image furnace. Instruction manual. Ulvac-Riko, Inc. (www.ulvac.co.jp) 2010.
- Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Thermal insulation material on the basis of mullite-corundum and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
- Nikitina V.Ju., Kolyshev S.G., Kupcov R.S. Sposoby opredelenija ploshhadi sechenija monokristallicheskih volokon Al2O3 dlja rascheta prochnosti pri rastjazhenii [Methods for determining the cross-sectional area of single crystal Al2O3 fibers for calculating the tensile strength] //Trudy VIAM. 2014. №2. St. 03 (viam-works.ru).