Peculiar features of optimization of resonant radar-absorbing materials of nonmagnetic type
Romanov A.M., Beljaev А.А., Shirokov V.V. Peculiar features of optimization of resonant radar-absorbing materials of nonmagnetic type // Proceedings of VIAM. 2014. No. 11. DOI: 10.18577/2307-6046-2014-0-11-5-5. URL: https://www.viam-works.ru/en/journal/2014/11/5
Abstract
This article is devoted to numerical optimization of resonant narrow-band radar-absorbing materials based on polymer matrices of different density on a base of car-bonized fiber «UVZH-15C Echo» (Svetlogorsk PC«Khimvolokno», Belarus) with a di-ameter of filament 7 micron and specific resistivity 0,00003 Ohm•m. As a result of cal-culations, for a number of frequencies of centimeter and decimeter waves optimal mate-rial thickness, length and concentration of the fiber – filler were found. Features of res-onant materials optimization related to an ambiguity of definition of optimized parame-ters are taken into account. Because of that, the calculations allow you to select a type of matrix in terms of the minimum mass of 1 m2 of the material.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Kablov E.N. Himija v aviacionnom materialovedenii [Chemicals in aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Doroshevich A.A., Gal'perin V.E. Jelektromagnitnaja sovmestimost' sudovyh tehnicheskih sredstv [EMC marine hardware]: Uchebnik. SPb.: Izd-vo Sankt-Peterburgskogo GMTU. 2005. S. 68–78.
- Kirillov V.Ju. Raschet parametrov impul'snyh jelektromagnitnyh pomeh (JeMP) v blizhnej i dal'nej zonah [Calculation of parameters of pulsed electromagnetic interference (EMI) in the near and far field] /V sb. dokl. VI NTK JeMS TS i BO (JeMS-2000). SPb. 2000. S. 134–137.
- Saharov K.Ju., Turkin V.A., Miheev O.V., Suhov A.V., Lafishev M.A., Erashev D.I. Ap-paratura dlja monitoringa jelektromagnitnogo izluchenija v sverhkorotkom impul'snom dia-pazone dlitel'nostej [Apparatus for monitoring the electromagnetic radiation in the ultra-short pulse duration range] //Tehnologii JeMS. 2011. №4(39). S. 58–61.
- Bibikov S.B., Prokof'ev M.V., Kulikovskij K.Je., Zhuravlev V.A. Razrabotka materialov i pokrytij, ispol'zuemyh dlja provedenija radiotehnicheskih ispytanij i obespechenija jelektromagnitnoj sovmestimosti [Development of materials and coatings used for the testing of radio and electromagnetic compatibility] //Voprosy oboronnoj tehniki. Ser. «Tehnicheskie sredstva protivodejstvija terrorizmu». 2013. №5–6. S. 56–64.
- Lushina M.V., Parshin S.G., Rzhevskij A.A. Sovremennye jekranirujushhie i radiopogloshhajushhie materialy [Modern shielding and radio absorbing materials] //Sistemy upravlenija i obrabotka informacii. 2011. №22. S. 208–214, 223.
- Nikol'skij V.V., Nikol'skaja T.I. Jelektrodinamika i rasprostranenie radiovoln [Electrodynamics and Propagation]. M.: URSS. 2012. S. 163–164.
- Bibikov S.B., Titov A.N., Cherepanov A.K. Sintez materiala s zadannym kojefficientom otrazhenija v shirokom diapazone chastot i uglov padenija [Synthesis of a material with a specified reflectivity in a wide range of frequencies and angles of incidence] /V sb. dokl. XV Mezhduna-rodnoj nauch.-tehnich. konf. «Radiolokacija. Navigacija. Svjaz'». Voronezh. 2009. S. 1578–1584.
- Korn G.A., Korn T.M. Spusk s vychisleniem koordinat gradient [Descent from the calculation of the coordinates of the gradient]: Spravochnik po matematike. M.: Nauka. 1984. 660 s.
- Rosenbrock H.H. An automatic method for finding the greatest or least value of a function //The Computer Journal. 1960. V. 3. Р. 175–184.
- Brehovskih A.M. Volny v sloistyh sredah [Waves in Layered Media]. M.: Nauka. 1957. S. 52–56.
- Odelevskij V.I. Raschet obobshhennoj provodimosti geterogennyh struktur. 1-matrichnye dvuhfaznye sistemy s nevytjanutymi vkljuchenijami [Calculation of the generalized conductivity of heterogeneous structures. 1-matrix two-phase systems with unstretched inclusions] //ZhTF. 1951. T. XXI. №5. S. 668–676.
- Salski B. The extension of the Maxwell Garnett mixing rule for dielectric composites with nonuniform orientation of ellipsoid inclusions //Progress In Electromagnetics Research Letters. 2012. V. 30. P. 173–184.
- Shirokov V.V., Romanov A.M. Issledovanie dijelektricheskih harakteristik steklosotoplasta volnovodnym metodom [Investigation of the dielectric characteristics of the glass-honeycomb by waveguide method] //Aviacionnye materialy i tehnologii. 2013. №4. S. 62–68.
- Beljaev A.A., Agafonova A.S., Antipova E.A., Botanogova E.D. Konstrukcionnyj radiopogloshhajushhij material trehslojnoj struktury s soglasujushhim sloem [Structural radar-absorbing material is a three-layer structure with a matching layer] //Trudy VIAM. 2013. №7. St. 02 (viam-works.ru).
- Oreshkin P.T. Fizika poluprovodnikov i dijelektrikov [Physics of semiconductors and dielectrics]. M.: Vyssh. shkola. 1977. S. 380–392.
- King R., Smit G. Antenny v material'nyh sredah [Antennas in material media]. Ch. 1. M.: Mir. 1984. S. 379–384.
- Hmel'nik G.I., Bibikov S.B. Statisticheskij analiz zavisimosti parametrov raspredelenija Debaja ot udel'nyh soprotivlenij sloev mnogoslojnogo RPP [Statistical analysis of the dependence of the distribution parameters of the Debye resistivity layers of the multilayer RPP] //Tehnologii jelektromagnitnoj sovmestimosti. 2012. №4 (43). S. 45–51.
- Agafonova A.S., Beljaev A.A., Kondrashov Je.K., Romanov A.M. Osobennosti formirovanija monolitnyh konstrukcionnyh radiopogloshhajushhih materialov na osnove kompozitov, napolnennyh rezistivnym voloknom [Features of the formation of monolithic structural radar absorbing materials based on composites filled with resistive fiber] //Aviacionnye materialy i tehnologii. 2013. №3. S. 56–59.
- Bespalova E.E., Kondrashov Je.K. Osobennosti korrektirovki receptury pozharobezopasnogo materiala dlja bezjehovyh kamer pri izmenenii parametrov radiopogloshhajushhego napolnitelja [Features correct formulation fireproof material for anechoic chambers when changing the radar absorbing filler] //Aviacionnye materialy i tehnologii. 2014. №2. S. 48–52.