Adhesive prepregs for laminated aluminum glass plastics (SIAL)

Lukina N.F., Dement’eva L.A., Anikhovskaya L.I.
Lukina N.F., Dement’eva L.A., Anikhovskaya L.I. Adhesive prepregs for laminated aluminum glass plastics (SIAL) // Proceedings of VIAM. 2014. No. 1. DOI: 10.18577/2307-6046-2014-0-1-5-5. URL: https://www.viam-works.ru/en/journal/2014/1/5
Abstract

The stages of work to improve the durability and the life of the aircraft technique are described. Distinctive features of adhesive prepregs are listed and the results of their application are described. The results of studies of a new class of alumopolymer layered materials brands SIAL – hybrid material based on thin sheets of aluminum structural alloys and plastic based on adhesive prepregs obtained by a melt-type adhesive bonding and fiberglass with different reinforcement structure – are described.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Petrova A.P., Lukina N.F. Klei dlya mnogorazovoy kosmicheskoy sistemy [Glues for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
  4. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstruktsionnye i termostoykie klei [Structural and heat-resistant glues] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 328–335.
  5. Dement'eva L.A., Serezhenkov A.A., Bocharova L.I., Anihovskaya L.I., Lukina N.F. Kompozitsionnye materialy kleevye na osnove steklyannyh i uglerodnyh napolniteley [Adhesive composite materials on the basis of glass and carbon fillers] //Klei. Germetiki. Tehnologii. 2009. №1. S. 24–27.
  6. Kutsevich K.E., Dement'eva L.A., Lukina N.F., Chursova L.V. Svoystva i naznachenie kleya VK-36RM dlya aviatsionnoy tehniki [Properties and functions of VК-36RМ glue for aviation equipment] //Klei. Germetiki. Tehnologii. 2013. №8. S. 5–6.
  7. Anihovskaya L.I., Minakov V.T. Klei i kleevye prepregi dlya perspektivnyh izdeliy aviakosmicheskoy tehniki [Adhesives and adhesive prepregs for advanced products of aerospace engineering] /V kn.: Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2002: Yubileynyj nauch.-tehnich. sb. M.: MISiS–VIAM. 2002. S. 315–326.
  8. Dement'eva L.A., Lukina N.F., Serezhenkov A.A., Kutsevich K.E. Osnovnye svoystva i naznachenie PKM na osnove kleevyh prepregov [Basic properties and functions of polymer composite materials based on adhesive prepregs] /V sb. tezisov dokl. XIX Mezhdunarodnoy nauch.-tehnich. konf. «Konstruktsii i tehnologiya polucheniya izdeliy iz nemetallicheskih materialov». Obninsk. 2010. S. 11–12.
  9. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kutsevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Аdhesive prepregs and laminated materials on their basis] //Aviatsionnye materialy i tehnologii. 2013. №2. S. 19–21.
  10. Lukina N.F., Dement'eva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidel'nikov V.V., Kutsevich K.E. Kleevye prepregi i kompozitsionnye materialy na ih osnove [Аdhesive prepregs and composite materials on their basis] //Rossiyskiy himicheskiy zhurnal. 2010. T. LIV. №1. S. 53–56.
  11. Prepreg i izdelie, vypolnennoe iz nego [Prepreg and a product made thereof]: pat. 2427594 Ros. Federatsiya; opubl. 23.07.13.
  12. Lukina N.F., Dement’eva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidel’nikov V.V., Kutsevich K.E. Adhesive prepregs and composite materials on their basis //Russian Journal of General Chemistry. 2011. T. 81. №5. P. 1022–1024.
  13. Dement'eva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kutsevich K.E., Petrova A.P. Svoystva kompozitsionnyh materialov na osnove kleevyh prepregov [Properties of composite materials based on adhesive prepregs] //Klei. Germetiki. Tehnologii. 2012. №6. S. 19–24.
  14. Dement'eva L.A., Serezhenkov A.A., Lukina N.F., Kutsevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Аdhesive prepregs and laminated materials on their basis] //Aviatsionnye materialy i tehnologii. 2013. №2. S. 19–21.
  15. Kablov E.N., Antipov V.V., Senatorova O.G., Lukina N.F. Novyj klass sloistyh alyumostekloplastikov na osnove alyuminiylitievogo splava 1441 s ponizhennoy plotnost'yu [New class of laminated aluminium glass-plastics based on 1441 low-density aluminum alloy] //Vestnik MGTU im. N.E. Baumana. 2011. Spets. vyp. «Perspektivnye konstruktsionnye materialy i tehnologii». S. 174–184.
  16. Fridlyander I.N., Anihovskaya L.I., Senatorova O.G., Sidel'nikov V.V., Dement'eva L.A. Kompozitsionnye kleevye i sloistye metallopolimernye kompozity [Composite adhesive and laminated metal-polymer composites] /Entsiklopediya «Tsvetnye metally i splavy. Kompozitsionnye metallicheskie materialy». M.: Mashinostroenie. 2001. S. 814–831.
  17. Anihovskaya L.I., Dement'eva L.A. /V sb. trudov Mezhdunarodnoy konf. «Sloistye kompozitsionnye materialy-98». Volgograd. 1998. S. 170–171.
  18. Senatorova O.G., Antipov V.V., Lukina N.F., Sidel'nikov V.V., Kotova E.V. Vysokoprochnye treschinostoykie legkie sloistye alyumostekloplastiki klassa SIAL – per-spektivnye materialy dlya aviatsionnyh konstruktsiy [High-strength crack-resistant light laminated aluminium glass-plastics of SIAL class as promising materials for aviation structures] //Tehnologiya legkih splavov. 2010. №1. S. 28–31.
  19. Fridlyander I.N., Anihovskaya L.I., Senatorova O.G., Sidel'nikov V.V. i dr. Kleenye metallicheskie i sloistye metallopolimernye kompozity [Glued metal and laminated metal-polymer composites] //Tsvetnye metally i splavy. Kompozitsionnye metallicheskie materialy. 2001. T. II-3. S. 814–832.
  20. Sloistyj kompozitsionnyj material i izdelie, vypolnennoe iz nego [Laminated composite material and a product made thereof]: pat. 2185964 Ros. Federatsiya; opubl. 15.04.2004.
  21. Fridlyander I.N., Senatorova O.G., Lukina N.F., Antipov V.V. Sloistye alyumopolimernye materialy SIAL [SIAL layered aluminum-bearing polymer materials] /V sb. 75 let. Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM. 2007. S. 188–192.
  22. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoy konferentsii po kleyam i germetikam. Frantsiya [Review of papers of the International conference on adhesives and sealants. France.] //Trudy VIAM. 2013. №8. St. 06 (viam-works.ru).