Selection of heat-resistant coating with metalloceramic barrier layer for protection of re-ru-bearing Nickel-based superalloy VZhM4

Gayamov A.M., Budinovskiy S.A., Muboyadzhyan S.A., Kosmin A.A.
Gayamov A.M., Budinovskiy S.A., Muboyadzhyan S.A., Kosmin A.A. Selection of heat-resistant coating with metalloceramic barrier layer for protection of re-ru-bearing Nickel-based superalloy VZhM4 // Proceedings of VIAM. 2014. No. 1. DOI: 10.18577/2307-6046-2014-0-1-1-1. URL: https://www.viam-works.ru/en/journal/2014/1/1
Abstract

Selection of heat-resistant coating with metalloceramic barrier layer for protection of details made of Re-Ru nickel-based superalloy operating at 1150°С is made. High-temperature tests of isothermic and cyclic heat-resistance and research of structure after these tests are made. Results show that the Ni–Cr–Al–Ta–Hf–Re–Y barrier layer containing tungsten carbide particles effectively suppresses forming of the secondary reaction zone. Heat-resistant coatings for Re-Ru superalloy reduce corrosion level up to a dosens of times.

Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye liteynye garoproshnye splavy novogo pokoleniya [Nickel heat-resistant casting alloys of new generation] //Aviatsionnye materialy i tekhnologii. 2012. №S. S. 36–52.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnykh splavov i staley special’nogo naznacheniya, zashchitnykh pokrytiy [Development strategy of heat-resistant alloys and special-purpose steels, protective and thermal-protective coatings] //Aviatsionnye materialy i tekhnologii. 2012. №S. S. 19–36.
  3. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tekhnologii ikh pere-rabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tekhnologii. 2012. №S. S. 7–17.
  4. Zharoprochnyy splav na nikelevoy osnove dlya monokristallicheskogo lit’ya [Nickel-based heat-resistant alloy for single crystal casting]: pat. 2439184 Ros. Federatsiya; opybl. 05.10.2010.
  5. Zharoprochnyy splav na osnove nikelya [Nickel-based heat-resistant alloy]: pat. 2402624 Ros. Federatsiya; opybl. 16.06.2009.
  6. Zharoprochnyy liteynyy splav na osnove nikelya i izdelie, vypolnennie is nego [Nickel-based heat-resistant alloy and a product made thereof]: pat. 2365656 Ros. Federatsiya; opybl. 30.01.2008.
  7. Kablov E.N., Muboyadzhyan S.A. Zhrostoykie i teplozashchitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnykh GTD [Heat-resistant and thermal-protective coatings for the high-pressure turbine blades of promising GTEs] //Aviatsionnye materialy i tekhnologii. 2012. №S. S. 60–70.
  8. Matveev P.V., Budinovskiy S.A., Muboyadzhyan S.A., Kos’min A.A. Zashchitny zharostoykie pokrytiya slya splavov na osnove intermetallidiv nikelya [Protective heat-resistant coatings for alloys based on nickel intermetallic compounds] //Aviatsionnye materialy i tekhnologii. 2012. №2. S. 12–15.
  9. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising gtes [Heat-resistant coatings for the high-pressure turbine blades of promising GTEs] //Russian metallurgy (Metally). 2012. №1. P. 1–7.
  10. Suzuki A., Rae C.M.F. Secondary reaction zone formations in coated Ni-base single crystal superalloys [Secondary reaction zone formations in coated Ni-base single crystal superalloys] //Journal of Physics: Conference Series 2009. Р. 165.
  11. Suzuki A., Rae C.M.F., Hobbs R.A., Murakami H. Secondary reaction zone formations in Pt-Aluminised fourth generation Ni-base single crystal superalloys [Secondary reaction zone formations in Pt-Aluminised fourth generation Ni-base single crystal superalloys] //Advanced Materials Research. 2011. V. 278. P. 78–83.
  12. Muboyadzhyan S.A., Budinovskiy S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostoykie pokrytiya i zharostoykie sloi dlya teplozashchitnykh pokrytiy [High-temperature heat-resistant coatings and heat-resistant layers for thermal-protective coatings] //Aviatsionnye materialy i tekhnologii. 2012. №1. S. 17–20.
  13. Budinovskiy S.A., Muboyadzhyan S.A., Gayamov A.M., Kos’min A.A. Zharostoykie ionnoplazmennye pokrytiya dlya lopatok turbin iz nikelevykh splavov, legirovannykh reniem [Heat-resistant plasma-ion coatings for the turbine blades made of rhenium-alloyed nickel alloys] //MiTOM. 2008. №6. S. 31–36.
  14. Budinovskiy S.A., Muboyadzhyan S.A., Gayamov A.M., Stepanova S.V. Ionno-plazmennye zharostoykie pokrytiya s kompozitsionnym bar’ernym sloem dlya zashchity ot okisleniya splava ZhS36VI [Heat-resistant plasma-ion coatings with composite barrier layer for protection of ZhS36VI alloy from oxidation] //MiTOM. 2011. №1. S. 34–40.
  15. Gayamov A.M. Zharostoykie pokrytiya s kompozitsionnym bar’ernym sloem dlya zashchity vneshney poverkhnosti rabochikh lopatok GTD iz reniysoderzhashchikh zharoprochnykh nikelevykh splavov [Heat-resistant coating with composite barrier layer to protect the outer surface of the GTE blades made of heat-resistant rhenium-bearing nickel alloys] /V sb. materialov XI Rossiyskoy ezhegodnoy konf. molodykh nautsnykh sotrudnikov i aspirantov „Fiziko-khimiya i tekhnologiya neorganicheskikh materialov”. M.: IMET RAN. 2012. S. 473–475.
  16. Muboyadzhyan S.A., Lutsenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povysheniya sluzhebnykh kharakteristik lopatok kompressora GTD metodom ionnogo modifitsirovaniya poverkhnosti [Study of possibility to improve the service performance of GTE compressor blades by the ionic-modification of surfaces] //Trudy VIAM. 2013. №1. St. 01 (viam-works.ru).