P. M. Putilina, A. Yu. Isaev Electron beam curing of polymer composite materials (review) // Proceedings of VIAM. 2026. No. 11 (165). С. 138-153. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-138-153.
Electron beam curing of polymer composite materials (review)
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
A review of the scientific and technical literature on the study of processes occurring during the with an electron beam of polymeric materials is presented. The technology of electron beam curing, its parameters and the equipment used are described. The advantages and disadvantages of the technology and its areas of application are highlighted. The types of electron beam curable polymers and polymerization initiators are examined. An analysis of the transformations of polymers under radiation processing and its impact on the properties of materials is provided.
Keywords
electron beam processing, radiation curing, electron accelerator, radical polymerization, ionic polymerization, polymerization initiators
Reference list
- Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122–144. Available at: http://www.journal.viam.ru (accessed: April 02, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
- Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), pp. 82–92. Available at: http://www.journal.viam.ru (accessed: April 02, 2026). DOI: 10.18577/2713-0193-2023-0-1-82-92.
- Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleinimide binders. Aviation materials and technologies, 2024, no. 4 (77), pp. 43–61. Available at: http://www.journal.viam.ru (accessed: April 02, 2026). DOI: 10.18577/2713-0193-2024-0-4-43-61.
- Donetskiy K.I., Karavaev R.Yu., Bystrikova D.V., Melnikov D.A., Gracheva A.D., Gorodilova N.A. Manufacturing of a draft element of a helicopter control system thrust using volume-reinforced woven carbon fiber preforms. Trudy VIAM, 2025, no. 8 (150), pp. 112–122. Available at: http://www.viam-works.ru (accessed: April 02, 2026). DOI: 10.18577/2307-6046-2025-0-8-112-122.
- Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), pp. 22–33. Available at: https://www.journal.viam.ru (accessed: April 02, 2026). DOI: 10.18577/2713-0193-2021-0-1-22-33.
- Wali A.S., Kumar S., Khan D. A review on recent development and application of radiation curing. Materials Today: Proceedings, 2023, vol. 82, pp. 68–74.
- Abou Elmaaty T., Okubayashi S., Elsisi H., Abouelenin S. Electron beam irradiation treatment of textiles materials: a review. Journal of Polymer Research, 2022, vol. 29, no. 117, pp. 1–19.
- Kashiwagi M., Hoshi Y. Electron beam processing system and its application. Sei Technical Review, 2012, no. 75, pp. 47–54.
- Zapka W. Inkjet Printing in Industry: Materials, Technologies, Systems, and Applications. Wiley-VCH, 2022, 1872 p.
- Hamm R.W., Hamm M.E. Industrial Accelerators and Their Applications. World Scientific, 2012, 421 p.
- Zapka W. Handbook of Industrial Inkjet Printing: A Full System Approach. Wiley-VCH, 2017, 984 p.
- Yoo S.H. Short review of utilization of electron-beam irradiation for preparing polyacrylonitrile-based carbon fibers and improving properties of carbon-fiber-reinforced thermoplastics. Carbon Letters, 2022, vol. 32, pp. 413–429.
- Hay J.N., O`Gara P. Recent developments in thermoset curing methods. Proceedings of the Institution of Mechanical Engineers, Part G: Journal of Aerospace Engineering, 2006, vol. 220 (3), pp. 187–195.
- Leach R.H., Pierce R.J., Hickman E.P. et al. The Printing Ink Manual. Dordrecht: Springer, 1993, 993 p.
- Javadi A., Mehr H.S., Sobani M., Soucek M.D. Cure-on-command technology: A review of the current state of the art. Progress in Organic Coatings, 2016, vol. 100, pp. 2–31.
- Lopata V., Saunders C., Singh A. et al. Electron-beam-curable epoxy resins for the manufacture of high-performance composites. Radiation Physics and Chemistry, 1999, vol. 56 (4), pp. 405–414.
- Pascault J., Williams R. Epoxy Polymers: New Materials and Innovations. Wiley-VCH, 2010, 367 p.
- Laricheva V.P., Stepanov V.I., Kovalev B.A., Smirnova L.A. Radiation technology of reinforced composite materials – a breakthrough technology for manufacturing products for aviation equipment at the present stage. Novosti materialovedeniya. Nauka i tekhnika, 2014, no. 3, art. 07. Available at: http://www.materialsnews.ru (accessed: March 27, 2026).
- Rizzolo R., Walczyk D., Kuppers J. et al. Rapid consolidation and curing of advanced composites using electron beam irradiation. Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture, 2019, vol. 233 (4), pp. 1168–1181.
- Wang B., Ming Y., Zhu Y. et al. Fabrication of continuous carbon fiber mesh for lightning protection of large-scale wind-turbine blade by electron beam cured printing. Additive Manufacturing, 2020, vol. 31, art. 100967.
- Zhang J., Duan Y., Zhao X., Wang B. Irradiation dose control for polymer-matrix composites fabricated by in situ curing with low energy electron beam. Journal of Applied Polymer Science, 2017, vol. 134 (24), art. 44944.
- Wolff-Fabris F., Altstädt V., Arnold U., Döring M. Electron Beam Curing of Composites. Hanser Publications, 2010, 136 p.
- Vautard F., Grappe H., Ozcan S. Engineered Interface Chemistry to Improve the Strength of Carbon Fiber Composites Cured by Electron Beam. Industrial & Engineering Chemistry Research, 2014, vol. 53 (32), pp. 12729–12736.
- Cadinot N., Boutevin B., Parisi J.P. et al. Electron-beam curable structural adhesives. Part 1: Study of acrylic resins for structural adhesive applications. International Journal of Adhesion and Adhesives, 1994, vol. 14, no. 4, pp. 237–241.
- Singh A.K., Mehra D.S., Niyogi U.K. et al. Breathability studies of electron beam curable polyurethane pressure sensitive adhesive for bio-medical application. Radiation Physics and Chemistry, 2014, vol. 103, pp. 75–83.
- Singh A.K., Mehra D.S., Niyogi U.K. et al. Effect of crosslinkers on adhesion properties of electron beam curable polyurethane pressure sensitive adhesive. International Journal of Adhesion and Adhesives, 2013, vol. 41, pp. 73–79.
- Ebe K., Sasaki T. Electron beam curing of aliphatic unsaturated polyesters. I. Mechanistic study on converting to pressure-sensitive adhesives. Journal of Applied Polymer Science, 2003, vol. 88 (7), pp. 1854–1857.
- Smirnova Yu.A. Electron-beam curing compositions for adhesive tapes: thesis abstract, Cand. Sc. (Chem.). St. Petersburg, 2005, 20 p.
- Smirnova Y.A., Vasil'eva I.V., Persinen A.A. Electron-Beam-Cured Adhesives Based on Low-Molecular-Weight Carboxylated Butadiene-Nitrile Rubber. Russian Journal of Applied Chemistry, 2005, vol. 78, pp. 1031–1033.
- Nishitsuji D.A., Marinucci G., Evora M.C., de Andrade e Silva L.G. Study of electron beam curing process using epoxy resin system. Nuclear Instruments and Methods in Physics Research, Section B: Beam Interactions with Materials and Atoms, 2007, vol. 265, no. 1, pp. 135–138.
- Glauser T., Johansson M., Hult A. A comparison of radiation and thermal curing of thick composites. Macromolecular Materials and Engineering, 2000, vol. 274 (1), pp. 25–30.
- Glauser T., Johansson M., Hult A. Electron-beam curing of thick thermoset composites: Effect of temperature and fiber. Macromolecular Materials and Engineering, 2000, vol. 274 (1), pp. 20–24.
- Pitarresi G., Alessi S., Tumino D. et al. Interlaminar Fracture Toughness Behavior of Electron-Beam Cured Carbon-Fiber Reinforced Epoxy-Resin Composites. Polymer Composites, 2014, vol. 35 (8), pp. 1529–1542.
- Kim H.B., Oh S., Jeong Y.G. et al. Effects of heat treatment on the microstructure and flexural mechanical properties of carbon fiber reinforced composite cured by electron beam. Materials Today Communications, 2023, vol. 37, art. 107181.
- Zhao X., Duan Y., Li D. et al. Investigation of curing characteristics of carbon fiber/epoxy composites cured with low-energy electron beam. Polymer Composites, 2014, vol. 36 (9), pp. 1731–1737.
- Berejka A.J., Eberle C. Electron beam curing of composites in North America. Radiation Physics and Chemistry, 2002, vol. 63 (3), pp. 551–556.
- Saunders C., Lopata V., Barnard J., Stepanik T. Electron beam curing — Taking good ideas to the manufacturing floor. Radiation Physics and Chemistry, 2000, vol. 57 (3), pp. 441–445.
The article was submitted
2026-06-17
approved and accepted for publication after reviewing
2026-07-20