N. M. Parashchenko, M. S. Kozhukharov Review of polymer-derived ceramics (PDC). Part 3. Microstructure and applications // Proceedings of VIAM. 2026. No. 11 (165). С. 110-124. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-110-124.

Review of polymer-derived ceramics (PDC). Part 3. Microstructure and applications

N. M. Parashchenko1, M. S. Kozhukharov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The article focuses on the study of the microstructure and applications of polymer-derived ceramic (PDC) materials. It examines microstructure analysis techniques, including spectroscopic and microscopic approaches, along with key aspects of the evolution of of the microstructure during high-temperature processing. Special attention is given to the role of nanodomains and free carbon in shaping PDC properties. Promising application areas for such materials are discussed, including composites, coatings, microelectronics, and energy technologies.

Keywords
PDC material, microstructure, nanodomains, functional properties, free carbon, pyrolysis

Reference list
  1. Kuznetsov B.Yu., Sorokin O.Yu., Vaganova M.L., Osin I.V. Synthesis of model high-temperature ceramic matrices by the method of spark plasma sintering and the study of their properties for the production of composite materials. Aviacionnye materialy i tehnologii, 2018, no. 4 (53), pp. 37–44. DOI: 10.18577/2071-9140-2018-0-4-37-44.
  2. Deynega G.I., Kuzmina I.G., Bityutskaya O.N., Narsky A.R. Foam ceramic filters based on domestic refractory materials. Part 2. Trudy VIAM, 2024, no. 2 (132), pp. 13–22. Available at: http://www.viam-works.ru (accessed: April 10, 2026). DOI: 10.18577/2307-6046-2024-0-2-13-22.
  3. Varrik N.M., Maksimov V.G., Yudin A.V., Babashov V.G. On the criteria of suitability of ceramic products for the manufacture of equipment for continuous casting of aluminum. Trudy VIAM, 2024, no. 2 (132), pp. 49–56. Available at: http://www.viam-works.ru (accessed: April 10, 2026). DOI: 10.18577/2307-6046-2024-0-2-49-56.
  4. Parashchenko N.M., Tupikov A.S., Lyzhenkov Z.A., Golovko D.S. Review of Polymer-Derived Ceramics (PDC). Part 1. Preceramic polymers and production of PDC materials. Trudy VIAM, 2025, no. 8 (150), рр. 134–151. Available at: http://www.viam-works.ru (accessed: May 15, 2026). DOI: 10.18577/2307-6046-2025-0-8-134-151.
  5. Parashchenko N.M., Tupikov A.S., Lyzhenkov Z.A., Golovko D.S. Review of Polymer-Derived Ceramics (PDC). Part 1. Preceramic polymers and production of PDC materials. Trudy VIAM, 2025, no. 8 (150), pp. 134–151. Available at: http://www.viam-works.ru (accessed: May 15, 2026). DOI: 10.18577/2307-6046-2026-0-4-104-120.
  6. Riedel R., Passing G., Schönfelder H., Brook R.J. Synthesis of dense silicon-based ceramics at low temperatures. Nature, 1992, vol. 355, no. 6362, pp. 714–717. DOI: 10.1038/355714a0.
  7. Mera G., Tamayo A., Nguyen H. et al. Nanodomain Structure of Carbon-Rich Silicon Carbonitride Polymer-Derived Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 4, pp. 1169–1175.
  8. Saha A., Raj R., Williamson D.L., Kleebe H.J. Characterization of Nanodomains in Polymer-Derived SiCN Ceramics Employing Multiple Techniques. Journal of the American Ceramic Society, 2005, vol. 88, no. 1, pp. 232–234. DOI: 10.1111/j.1551-2916.2004.00034.x.
  9. Ferrari A.C. Raman spectroscopy of graphene and graphite: Disorder, electron-phonon coupling, doping and nonadiabatic effects. Solid State Communications, 2007, vol. 143, no. 1–2, pp. 47–57. DOI: 10.1016/j.ssc.2007.03.052.
  10. Cançado L.G., Takai K., Enoki T. et al. General equation for the determination of the crystallite size La of nanographite by Raman spectroscopy. Applied Physics Letters, 2006, vol. 88, no. 16, p. 163106. DOI: 10.1063/1.2196057.
  11. Mera G., Riedel R., Poli F., Müller K. Carbon-rich SiCN ceramics derived from phenyl-containing poly(silylcarbodiimides). Journal of the European Ceramic Society, 2009, vol. 29, no. 13, pp. 2873–2883. DOI: 10.1016/j.jeurceramsoc.2009.03.026.
  12. Jiang T., Wang Y., Wang Y. et al. Quantitative Raman Analysis of Free Carbon in Polymer‐Derived Ceramics. Journal of the American Ceramic Society, 2009, vol. 92, no. 10, pp. 2455–2458. DOI: 10.1111/j.1551-2916.2009.03233.x.
  13. Riedel R., Mera G., Hauser R., Klonczynski A. Silicon-Based Polymer-Derived Ceramics: Synthesis Properties and Applications – A Review: Dedicated to Prof. Dr. Fritz Aldinger on the occasion of his 65th birthday. Nippon Seramikkusu Kyokai gakujutsu ronbunshi, 2006, vol. 114, no. 1330, pp. 425–444. DOI: 10.2109/jcersj.114.425.
  14. Iwamoto Y., Völger W., Kroke E. et al. Crystallization Behavior of Amorphous Silicon Carbonitride Ceramics Derived from Organometallic Precursors. Journal of the American Ceramic Society, 2001, vol. 84, no. 10, pp. 2170–2178. DOI: 10.1111/J.1151-2916.2001.TB00983.X.
  15. Michelle Morcos R., Mera G., Navrotsky A. et al. Enthalpy of Formation of Carbon-Rich Polymer-Derived Amorphous SiCN Ceramics. Journal of the American Ceramic Society, 2008, vol. 91, no. 10, pp. 3349–3354. DOI: 10.1016/J.JEURCERAMSOC.2021.01.042.
  16. Gervais C., Babonneau F., Ruwisch L. et al. Solid-state NMR investigations of the polymer route to SiBCN ceramics. Canadian Journal of Chemistry, 2003, vol. 81, no. 11, pp. 1359–1369. DOI: 10.1139/v03-167.
  17. Colombo P., Mera G., Riedel R., Sorarù G.D. Polymer-Derived Ceramics: 40 Years of Research and Innovation in Advanced Ceramics. Journal of the American Ceramic Society, 2010, vol. 93, no. 7, pp. 1805–1837. DOI: 10.1002/9783527631940.ch57.
  18. Dasgupta K., Sathiyamoorthy D. Disordered carbon – its preparation, structure, and characterisation. Materials Science and Technology, 2003, vol. 19, no. 8, pp. 995–1002. DOI: 10.1179/026708303225004693.
  19. Wan J., Gasch M.J., Mukherjee A.K. Silicon Nitride–Silicon Carbide Nancocomposites Fabricated by Electric-Field-Assisted Sintering. Journal of the American Ceramic Society, 2003, vol. 86, no. 3, pp. 526–528. DOI: 10.1111/j.1151-2916.2003.tb03335.x.
  20. Riedel R., Kienzle A., Dressler W. et al. A silicoboron carbonitride ceramic stable to 2,000°C. Nature, 1996, vol. 382, no. 6594, pp. 796–798. DOI: 10.1038/382796a0.
  21. Riedel R., Kleebe H.-J., Schönfelder H., Aldinger F. A covalent micro/nano-composite resistant to high-temperature oxidation. Nature, 1995, vol. 374, no. 6522, pp. 526–528. DOI: 10.1038/374526a0.
  22. Rouxel T., Soraru G., Vicens J. Creep Viscosity and Stress Relaxation of Gel‐Derived Silicon Oxycarbide Glasses. Journal of the American Ceramic Society, 2001, vol. 84, no. 5, pp. 1052–1058. DOI: 10.1111/J.1151-2916.2001.TB00789.X.
  23. Raj R., An L., Shah S. et al. Oxidation Kinetics of an Amorphous Silicon Carbonitride Ceramic. Journal of the American Ceramic Society, 2001, vol. 84, no. 8, pp. 1803–1810. DOI: 10.1111/j.1151-2916.2001.tb00918.x.
  24. Störmer H., Kleebe H.-J., Ziegler G. Metastable SiCN glass matrices studied by energy-filtered electron diffraction pattern analysis. Journal of Non-Crystalline Solids, 2007, vol. 353, no. 30–31, pp. 2867–2877. DOI: 10.1016/J.JEURCERAMSOC.2009.03.026.
  25. Kroke E., Li Y.-L., Konetschny C. et al. Silazane derived ceramics and related materials. Materials Science and Engineering: R: Reports, 2000, vol. 26, no. 4–6, pp. 97–199. DOI: 10.1016/S0927-796X(00)00008-5.
  26. Kleebe H.-J., Gregori G., Babonneau F. et al. Evolution of C-rich SiOC ceramics: Part I. Characterization by integral spectroscopic techniques: Solid-state NMR and Raman spectroscopy. International Journal of Materials Research, 2022, vol. 97: Evolution of C-rich SiOC ceramics, no. 6, pp. 699–709. DOI: 10.3139/ijmr-2006-0115.
  27. Saha A., Raj R., Williamson D.L. A Model for the Nanodomains in Polymer-Derived SiCO. Journal of the American Ceramic Society, 2006, vol. 89, no. 7, pp. 2188–2195. DOI: 10.1111/j.1551-2916.2006.00920.x.
  28. Dürr J., Lamparter P., Bill J. et al. An X-ray and neutron scattering investigation of precursor derived Si24C43N33 ceramics. Journal of Non-Crystalline Solids, 1998, vol. 232–234, pp. 155–161.
  29. Matsunaga K., Iwamoto Y., Fisher C.A.J., Matsubara H. Molecular Dynamics Study of Atomic Structures in Amorphous Si–C–N Ceramics. Journal of the Ceramic Society of Japan, 1999, vol. 107, no. 1251, pp. 1025–1031. DOI: 10.2109/JCERSJ.107.1025.
  30. Amkreutz M. On the Existence of Voids Within Precursor-derived Amorphous Si–C–N Ceramics. Soft Materials, 2007, vol. 4, no. 2–4, pp. 187–205. DOI: 10.1080/15394450701310046.
  31. Resta N., Kohler C., Trebin H. Molecular Dynamics Simulations of Amorphous Si –C–N Ceramics: Composition Dependence of the Atomic Structure. Journal of the American Ceramic Society, 2003, vol. 86: Molecular Dynamics Simulations of Amorphous Si–C–N Ceramics, no. 8, pp. 1409–1414. DOI: 10.1016/J.JNONCRYSOL.2016.05.024.
  32. Golczewski J.A., Aldinger F. Thermodynamic modeling of amorphous Si–C–N ceramics derived from polymer precursors. Journal of Non-Crystalline Solids, 2004, vol. 347, no. 1–3, pp. 204–210. DOI: 10.1016/j.jnoncrysol.2004.08.241.
  33. Kroll P. Modelling polymer-derived ceramics. Journal of the European Ceramic Society, 2005, vol. 25, no. 2–3, pp. 163–174.
  34. Kroll P. Modeling the «free carbon» phase in amorphous silicon oxycarbide. Journal of Non-Crystalline Solids, 2005, vol. 351, no. 12–13, pp. 1121–1126. DOI: 10.1016/j.jnoncrysol.2005.01.010.
  35. Krenkel W. Ceramic matrix composites: fiber reinforced ceramics and their applications. Weinheim: Wiley-VCH, 2008, 418 р. DOI: 10.1002/9783527622412.
  36. Cornu D., Bernard S., Duperrier S. et al. Alkylaminoborazine-based precursors for the preparation of boron nitride fibers by the polymer-derived ceramics (PDCs) route. Journal of the European Ceramic Society, 2005, vol. 25, no. 2–3, pp. 111–121. DOI: 10.1016/j.jeurceramsoc.2004.07.016.
  37. Kokott S., Heymann L., Motz G. Rheology and processability of multi-walled carbon nanotubes – ABSE polycarbosilazane composites. Journal of the European Ceramic Society, 2008, vol. 28, no. 5, pp. 1015–1021. DOI: 10.1016/j.jeurceramsoc.2007.09.035.
  38. Ishikawa T. Photocatalytic Fiber with Gradient Surface Structure Produced from a Polycarbosilane and Its Applications. International Journal of Applied Ceramic Technology, 2004, vol. 1, no. 1, pp. 49–55. DOI: 10.1111/j.1744-7402.2004.tb00154.x.
  39. Colombo P. Engineering porosity in polymer-derived ceramics. Journal of the European Ceramic Society, 2008, vol. 28, no. 7, pp. 1389–1395. DOI: 10.1016/j.jeurceramsoc.2007.12.002.
  40. Yeon S.-H., Reddington P., Gogotsi Y. et al. Carbide-derived-carbons with hierarchical porosity from a preceramic polymer. Carbon, 2010, vol. 48, no. 1, pp. 201–210. DOI: 10.1016/j.carbon.2009.09.004.
  41. Torrey J.D., Bordia R.K. Processing of Polymer-Derived Ceramic Composite Coatings on Steel. Journal of the American Ceramic Society, 2008, vol. 91, no. 1, pp. 41–45. DOI: 10.1111/j.1551-2916.2007.02019.x.
  42. Lewinsohn C.A., Elangovan S. Development of Amorphous, Non-Oxide Seals for Solid Oxide Fuel Cells. Ceramic Engineering and Science Proceedings. Eds. W.M. Kriven, H.-T. Lin. Hoboken: John Wiley & Sons, Inc., 2003, pp. 317–322. DOI: 10.1002/9780470294802.ch48.
  43. Colombo P. Polymer derived ceramics: from nano-structure to applications. Lancaster: DEStech Publications, 2010, 476 p.
  44. Liew L.-A., Liu Y., Luo R. et al. Fabrication of SiCN MEMS by photopolymerization of preceramic polymer. Sensors and Actuators A: Physical, 2002, vol. 95, no. 2–3, pp. 120–134.
  45. Kolb R., Fasel C., Liebau-Kunzmann V., Riedel R. SiCN/C-ceramic composite as anode material for lithium ion batteries. Journal of the European Ceramic Society, 2006, vol. 26, no. 16, pp. 3903–3908. DOI: 10.1016/j.jeurceramsoc.2006.01.009.
  46. Ceramic electric resistor: pat. US5961888A; appl. 10.08.98; publ. 05.10.99.
  47. Stern E., Heyder M., Scheffler F. Micropatterned Ceramic Surfaces by Coating with Filled Preceramic Polymers. Journal of the American Ceramic Society, 2009, vol. 92, no. 10, pp. 2438–2442. DOI: 10.1111/J.1551-2916.2009.03228.X.