Establishment of an optimal technological regime for manufacturing profiled flooring from PCM using different types of polymer matrices
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
The course of the research aimed at developing technology for manufacturing sheets of profiled fiberglass flooring is presented. The main stages of the manufacturing technology for structures made of PCM with dimensions of 3000×1500 mm based on epoxy and epoxy vinyl ester resins are described: the development of fiberglass, mathematical modeling of the infusion process and the establishment of an optimal technological regime of impregnation, taking into account the pot life of the resins, the determination of technological parameters for the manufacture of structure.
- Kablov E.N. New-Generation Materials and Digital Technologies for Their Processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
- Afanasyev D.V., Oshchepkov M.Yu. Out-of-Autoclave Technologies. Kompozitnyy mir, 2010, no. 5, pp. 28–37.
- Kablov E.N., Chursova L.V., Babin A.N. et al. Developments by FSUE «VIAM» in the Field of Melt-Processable Binders for Polymer Composite Materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37–42.
- Putilina P.M., Kutsevich K.E., Isaev A.Yu. Carbon fiber-reinforced and glass fiber-reinforced polymer composites for the manufacture of components for unmanned aerial vehicles and their developing prospects. Trudy VIAM, 2023, no. 8 (126), pp. 85–99. Available at: http://www.viamworks.ru (accessed: May 04, 2026). DOI: 10.18577/2307-6046-2023-0-8-85-99.
- Perepelkin K.E. Reinforcing Fibers and Fibrous Polymer Composites. Moscow: Nauchnye Osnovy i Tekhnologii, 2009, 386 p.
- Mikhailin Yu.A. Structural Polymer Composite Materials. Moscow: Nauchnye Osnovy i Tekhnologii, 2010, 822 p.
- Kogan D.I., Chursova L.V., Petrova A.P. Analysis of Manufacturing Technologies for Products Made of Continuously Reinforced Polymer Composites Using Non-Autoclave Methods (Review). Kompozitsionnye materialy, 2011, no. 11, pp. 2–6.
- Volnov O.I., Dudukin D.O. Fiberglass: History of Development, Production Technology, Part Forming, and Modern Applications. Trudy NGTU im. R.Ye. Alekseyeva, 2014, no. 5 (107), pp. 400–404.
- Vlasenko F.S., Raskutin A.E. Applying FRP in building structures. Trudy VIAM, 2013, no. 8, pp. 12–16. Available at: http://www.viam-works.ru (accessed: May 04, 2026).
- Sherriff M., Knibbs R.W., Langley P.G. Mechanism for the action of tackifying resins in pressure-sensitive adhesives. Journal of Applied Polymer Science, 1973, vol. 17, pp. 3423–3438.
- Allen K.W. A review of contemporary views of theories of adhesion. The Journal of Adhesion, 1987, vol. 21, pp. 261–277.
- Leong Y.C., Lee L.M.S., Gan S.N. The viscoelastic properties of natural rubber pressure-sensitive adhesive using acrylic resin as a tackifier. Journal of Applied Polymer Science, 2003, vol. 88, pp. 2118–2123.
- Fujita M., Takemura A., Ono H. et al. Effects of miscibility and viscoelasticity on shear creep resistance of natural-rubber-based pressure-sensitive adhesives. Journal of Applied Polymer Science, 2000, vol. 75, pp. 1535–1545.
- Fujita M., Kajiyama M., Takemura A. et al. Miscibility between natural rubber and tackifiers. I. Phase diagrams of the blends of natural rubber with rosin and terpene resins. Journal of Applied Polymer Science, 1987, vol. 64, pp. 2191–2197.
- Fujita M., Kajiyama M., Takemura A. et al. Miscibility between natural rubber and tackifiers. II. Phase diagrams of the blends of natural rubber and petroleum resins. Journal of Applied Polymer Science, 1998, vol. 67, pp. 221–229.
- Fujita M., Kajiyama M., Takemura A. et al. Effects of miscibility on peel strength of naturalrubber-based pressure-sensitive adhesives. Journal of Applied Polymer Science, 1998, vol. 70, pp. 777–784.
- Whitehouse R.S., Counsell P.J.C. Composition of rubber/resin adhesive films: 1. Surface composition as determined by ATR-IR spectroscopy. Polymer, 1976, vol. 17, pp. 699–704.
- Sherriff M. Peel adhesion and viscoelasticity of rubber-resin blends. Journal of Applied Polymer Science, 1980, vol. 18, pp. 2597–2608.
- Evdokimov A.A., Imametdinov E.Sh., Malakhovskiy S.S. Strengthening concrete building structure via reinforcement external system from carbon plastic. Trudy VIAM, 2020, no. 10 (92), рр. 73–80. Available at: http://www.viam-works.ru (accessed: May 04, 2026). DOI: 10.18577/2307-6046-2020-0-10-73-80.
- Evdokimov A.A., Venediktova M.A., Vakhrusheva Ya.A. et al. Experience in the Use of Polymeric Materials for the Construction of Rapidly Assembled Arch Bridges. Proc. Int. Sci.-Pract. Conf. «Materials Science, Shaping Technologies, and Equipment». Simferopol, 2024, pp. 127–136.
- Evdokimov A.A., Petrova A.P., Raskutin A.E. et al. Polymer Composite Materials for Use in the Construction Industry. Coll. Abstracts of the VIII All-Rus. Youth Scientific Forum «OpenScience 2021». Gatchina, 2021, p. 124.
- Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), pp. 22–33. Available at: https://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/2713-0193-2021-0-1-22-33.
- Sedov L.N., Mikhailova Z.V. Unsaturated polyesters. Moscow: Khimiya, 1977, 232 p.
- Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
- Bobylev V.A. Specialty epoxy resins for adhesives and sealants. Klei. Germetiki. Tekhnologii, 2005, no. 5, pp. 8–11.
- Bolshakov V.A., Antyufeeva N.V. Evaluation of the curing process model of the adhesive binder in prepreg. Aviation materials and technologies, 2023, no. 4 (73), pp. 66–77. Available at: http://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/2713-0193-2023-0-4-66-77.
- Evdokimov A.A., Raskutin A.E., Mishkin S.I. et al. Arch bridges using carbon-fiber-reinforced plastic (CFRP) arch elements. Konstruktsii iz kompozitsionnykh materialov, 2019, no. 2 (154), pp. 22–29.
- Mikhaldykin E.S. Application of concrete-filled tubular structures with shells made of polymer composite materials in the construction of small-span bridges: thesis, Cand. Sc. (Tech.). Moscow, 2021, 111 p.
- Kablov E.N. The role of fundamental research in the creation of new-generation materials. Abstracts of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
- Design, Construction and Testing of the Neal Bridge in Pittsfield, maine: Final Report. Available at: https://aewc.unaine.edu.com (accessed: May 04, 2026).
- Kirillov V.N., Startsev O.V., Efimov V.A. Climatic firmness and damageability of polymeric composite materials, problems and solutions. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 412–423.
- Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), pp. 70–80. Available at: http://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/2713-0193-2021-0-4-70-80.
- Startsev V.O. The degradation of polymer composite materials in seawater (review). Aviation materials and technologies, 2023, no. 1 (70), pp. 148–170. URL: http://www.journal.viam.ru (accessed: May 04, 2026). DOI: 10.18577/2713-0193-2023-0-1-148-170.
- Petrova A.P., Malysheva G.V. Adhesives, Adhesive Binders, and Adhesive Prepregs: A Textbook. Ed. by E.N. Kablov. Moscow: VIAM, 2017, 472 p.
- Raskutin A.E., Goncharov V.A. Computer modeling of technological process of manufacturing of PCM by method of vacuum infusion. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 286–291.
- Tkachuk A.I., Zagora A.G., Donetsky K.I., Evdokimov A.A. Polymeric matrixes for composite materials used in the construction of quickly built bridge structures. Trudy VIAM, 2020, no. 12 (94), pp. 67–74. Available at: http://www.viam-works.ru (accessed: May 04, 2026). DOI: 10.18577/2307-6046-2020-0-12-67-74.