M. S. Yashin, D. V. Kapitanenko, A. S. Shpagin, A. V. Vostrikov Development of isothermal deformation technology for a heat-resistant nickel-based alloy using computer modeling method // Proceedings of VIAM. 2026. No. 11 (165). С. 42-51. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-11-42-51.

Development of isothermal deformation technology for a heat-resistant nickel-based alloy using computer modeling method

M. S. Yashin1, D. V. Kapitanenko1, A. S. Shpagin1, A. V. Vostrikov1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

This article presents the results of a computer simulation of the isothermal deformation of blanks made of EI698 heat-resistant nickel alloy. Analysis of plastic deformation, temperature, shape, dimensions, energy-force parameters and trace lines allowed to plot a technological deformation process for the blank with optimal deformation parameters. After manufacturing forgings from EI698 alloy under isothermal conditions, the mechanical properties were evaluated. The test results confirmed the computer simulation results.

Keywords
isothermal deformation, computer modeling, pressure treatment, heat-resistant nickel alloys, finite element method, stamping, deformation



Reference list
  1. Echin A. B., Bondarenko Yu. A., Kolodyazhny M. Yu., Surova V. A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: July 13, 2026). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  2. Kablov E. N., Ospennikova O. G., Lomberg B. S. Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 129–141.
  3. Aviation Materials: Handbook in 9 vols. Ed. R. E. Shalin. 6th ed. Moscow: ONTI VIAM, 1989, vol. 3: Heat-Resistant Steels and Alloys Based on Refractory Metals, part 1, 566 p.
  4. Khimushin F. F. Heat-Resistant Steels and Alloys, 2nd ed., rev. and add. Moscow: Metallurgiya, 1969, 750 p.
  5. Ryndenkov D. V., Smirnov M. O., Karyagin D. A., Galkin V. A. Reducing the Quenching Duration for Components Made of the Heat-Resistant Wrought Nickel Alloy EI698-VD. Tekhnologiya legkikh splavov, 2026, no. 1, pp. 60–65.
  6. Narsky A. R., Deynega G. I., Kuzmina I. G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: July 13, 2026). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  7. Lopatin N. V., Bubnov M. V., Rogalev A. M., Korobova N. V., Sidorov A. A. Isothermal forging of EP741-NP alloy disc billets produced by powder metallurgy methods. Aviacionnye materialy i tehnologii, 2014, no. S5, pp. 31–37. DOI: 10.18577/2071-9140-2014-0-s5-31-37.
  8. Kolyadov E. V., Visik E. M., Gerasimov V. V., Bityutskaya O. N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), pp. 15–24. Available at: http://www.journal.viam.ru (accessed: July 13, 2026). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  9. Kucheryaev V. V., Mironova N. A., Shishkov S. U. Research of technological features of Ni–Al–Co system ingots deformation. Trudy VIAM, 2016, no. 3 (39), pp. 3–9. Available at: http://www.viam-works.ru (accessed: July 13, 2026). DOI: 10.18577/2307-6046-2016-0-3-1-1.
  10. Doronin O. N., Gorlov D. S., Azarovsky E. N., Kochetkov A. S. Study of the structure and properties of a heat-resistant coating at high-temperature deformation of samples from titanium intermetallic alloy. Aviation materials and technology, 2021, no. 1 (62), pp. 61–70. Available at: http://www.journal.viam.ru (accessed: July 13, 2026). DOI: 10.18577/2713-0193-2021-0-1-61-70.
  11. Ospennikova O. G., Bubnov M. V., Kapitanenko D. V. Computer modeling of metal working processes by pressure. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 141–147.
  12. Tsepin M. A., Begnarsky V. V., Lisunets N. L., Sinitsyn M. V., Erokhov M. A. Use of specialized software in the development of metal forming processes. Tsvetnye metally, 2007, no. 5, pp. 98–101.
  13. Shpagin A. S., Kapitanenko D. V., Moiseev N. V., Bazhenov A. R. Development of the technology for manufacturing ring blanks made of EP648-VI alloy by isothermal air forging using low-power hydraulic presses. Aviation materials and technologies, 2024, no. 4 (77), pp. 17–26. Available at: http://www.journal.viam.ru (accessed: July 13, 2026). DOI: 10.18577/2713-0193-2024-0-4-17-26.
  14. Vlasov A. V., Stebunov S. A., Evsyukov S. A., Biba N. V., Shitikov A. A. Finite-Element Modeling of Forging and Bulk Forming Processes. Moscow: Bauman Moscow State Tech. Univ., 2019, 384 p.
  15. Sirotinsky A. A. Production Technology and Industrial Application of Silicate-Enamel Coatings. Ekspozitsiya Neft Gaz, 2007, no. 42, pp. 36–38.