The study of chemical assembly of macromolecules in hydrolytic polycondensation of 1,1,3,3-tetramethyl-1,3-diethoxydisiloxane

Butuzov A.V.
Butuzov A.V. The study of chemical assembly of macromolecules in hydrolytic polycondensation of 1,1,3,3-tetramethyl-1,3-diethoxydisiloxane // Proceedings of VIAM. 2026. No. 6. DOI: 10.18577/2307-6046-2026-0-6-74-85. URL: https://www.viam-works.ru/en/journal/2026/6/7
Keywords
partial hydrolysis, homofunctional condensation, heterofunctional condensation, chemical assembly, organoalkoxysilanes, organosilanols, organocyclosiloxanes
Abstract

The article describes the results of a research on polycondensation «in situ» in the processes of partial hydrolysis of C2H5O(CH3)2SiOSi(CH3)2OC2H5. The influence of the molar ratio of reagents on the oligomeric composition of the partial hydrolysis products and the dependence of the monomer conversion degree on conversion of functional groups are presented. A comparison of the patterns of macromolecules formation in the processes of partial hydrolysis of 1,1,3,3-tetramethyl-1,3-diethoxydisiloxane and homofunctional condensation of 1,1,3,3-tetramethyldisiloxane-1,3-diol is carried out.

Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. The Present and Future of Additive Technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  3. Kablov E.N. Additive Technologies – the Dominant Focus of the National Technological Initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  4. Turchenko M.V., Lebedeva Yu.E., Belyachenkov I.O., Prokofiev V.A. Obtaining of ceramic materials by stereolithography method. Trudy VIAM, 2023, no. 9 (127). pp. 79–89. Available at: http://www.viam-works.ru (accessed: August 28, 2025). DOI: 10.18577/2307-6046-2023-0-9-79-89.
  5. Butuzov A.V., Semina A.V. Preceramic polymers for the production of ceramic products by vat photopolymerization. Part 1. Methods of production and properties. Trudy VIAM, 2025, no. 3 (145), pp. 70–88. Available at: http://www.viam-works.ru (accessed: August 28, 2025). DOI: 10.18577/2307-6046-2025-0-3-70-88.
  6. Lacelle T., Sampson K.L., Sarvestani H.Y. et al. Additive manufacturing of polymer derived ceramics: Materials, methods, and applications. APL Materials, 2023, vol. 11, pp. 1–29. DOI: 10.1063/5.0151661.
  7. Rasaki S.A., Xiong D., Xiong S. et al. Photopolymerization-based additive manufacturing of ceramics: A systematic review. Journal of advanced ceramics, 2021, vol. 10, no. 3, pp. 442–471. DOI: 10.1007/s40145-021-0468-z.
  8. Shestakov A.M. Ceramics based on organosilicon polymers-precursors: methods of preparation and properties (review). Trudy VIAM, 2020, no. 11 (93), pp. 76–92. Available at: http://www.viam-works.ru (accessed: August 28, 2025). DOI: 10.18577/2307-6046-2020-0-11-76-92.
  9. Parashchenko N.M., Tupikov A.S., Lyzhenkov Z.A., Golovko D.S. Review of Polymer-Derived Ceramics (PDC). Part 1. Preceramic polymers and production of PDC materials. Trudy VIAM, 2025, no. 8 (150), pp. 134–151. Available at: http://www.viam-works.ru (accessed: September 23, 2025). DOI: 10.18577/2307-6046-2025-0-8-134-151.
  10. Tarasova E.M., Butuzov A.V., Cherkasova A.A., Ivanov P.V. Study of chemical assembly of macromolecules in polycondensation of difunctional dimethylsilanes. Tonkie khimicheskie tekhnologii, 2016, vol. 11, no. 1, pp. 59–66.
  11. Zhang Z., Sakka S. Hydrolysis and polymerization of dimetildiethoxysilane, methyltrimethoxysilane and tetramethoxysilane in presence of aluminum acetylacetonate. A complex catalyst for the formation of siloxanes. Journal of Sol-Gel Science and Technology, 1999, vol. 16, pp. 209–220.
  12. Rakhimov V.I., Rakhimova O.V., Semov M.P. Kinetics of the initial stages of the sol-gel process. III. Evolution of silica associates. Fizika i khimiya stekla, 2009, vol. 35, no. 2, pp. 163–169.
  13. Lebedeva Yu.E., Popovich N.V., Orlova L.A., Chaynikova A.S., Grachshencov D.V. Investigation of rheological properties at sol-gel synthesis of materials in Y2O3–SiO2 system. Aviacionnye materialy i tehnologii, 2014, no. S6, pp. 67–72. DOI: 10.18577/2071-9140-2014-0-s6-67-72.
  14. Zhai Q., Zhou C., Zhao S. et al. Kinetic study of alkoxysilane Hydrolysis under acidic conditions by fourier transform near infrared spectroscopy combined with partial least-squares model. Industrial and Engineering Chemistry Research, 2014, vol. 53, pp. 13598–13609. DOI: 10.1021/ie5012195.
  15. Sugahara Y., Okada S., Kuroda K., Kato C. 29Si NMR study of hydrolysis and initial polycondensation processes of organoalkoxysilanes. II. Methyltriethoxysilane. Journal of Non-Crystalline Solids, 1994, vol. 167, pp. 21–38. DOI: 10.1016/S0022-3093(05)80802-6.
  16. Dong H., Lee M., Zhang Z., Reidy R.F., Mueller D.W. Methyltrimethoxysilane sol-gel polymerization in acidic ethanol solutions studied by 29Si NMR spectroscopy. Journal of Sol-Gel Science and Technology, 2003, vol. 28, pp. 5–14. DOI: 10.1023/A:1025690300105.
  17. Hook R.J. A 29Si NMR study of the sol-gel polymerization rates of substituted ethoxysilanes. Journal of Non-Crystalline Solids, 1996, vol. 195, pp. 1–15.
  18. Parale V.G., Mahadik D.B., Kavale M.S., Mahadik S.A. Sol-gel preparation of PTMS modified hydrophobic and transparent silica coatings. Journal of Porous Materials, 2012, vol. 20 (4), pp. 733–739. DOI: 10.1007/s10934-012-9648-0.
  19. Sugahara Y., Okada S., Kuroda K., Kato C. 29Si NMR study of hydrolysis and initial polycondensation processes of organoalkoxysilanes. I. Dimethyldiethoxysilane. Journal of Non-Crystalline Solids, 1992, vol. 139, pp. 25–34.
  20. Butuzov A.V., Cherkasova A.A., Ivanov P.V. The study of dimethylcyclosiloxanes formation regularities in heterophase hydrolysis of a dimethyldialkoxysilane (abstract). XVI International Scientific Conference «High-Tech in Chemical Engineering–2016» (Moscow, October 10–15, 2016). Moscow, 2016, p. 26.
  21. Ivanov P.V. Features of polycondensation of organosilanols. Vestnik MITKhT, 2011, vol. 6, no. 3, pp. 3–22.
  22. Aggarwal E.H., Bauer S.H. The structure of hexamethylcyclotrisiloxane as determined by the diffraction of electrons on the vapor. The Journal of Chemical Physics, 1950, vol. 18, no. 1, pp. 42–50. DOI: 10.1063/1/1747454.