Polytype modifications of silicon carbide in coatings
Sidorov D.V., Shavnev A.A. Polytype modifications of silicon carbide in coatings // Proceedings of VIAM. 2026. No. 5. DOI: 10.18577/2307-6046-2026-0-5-113-122. URL: https://www.viam-works.ru/en/journal/2026/5/9
Keywords
silicon carbide, polytype modification, crystal, transformation, producing, application
Abstract
The article presents a review of scientific and technical literature in the field of crystalline coatings of silicon carbide of various polytype modifications and methods for their production. The paper examines promising areas of application for the most common crystalline polytypic modifications of silicon carbide, which include dark matter detectors and biosensors, in addition to power devices and microelectronics. Approaches to studying the preferential formation of one or another polytype of silicon carbide in crystalline coatings are described.
Reference list
- Park Y., Weber E. SiC materials and devices. Academic press, 1998, pp. 1–18.
- Sidorov D.V., Grunin A.A., Schavnev A.A. Implementation of technology for chemical vapor deposition of silicon carbide in electronics. Part 1. Trudy VIAM, 2024, no. 3 (133), pp. 101–116. Available at: http://www.viam-works.ru (accessed: September 19, 2025). DOI: 10.18577/2307-6046-2024-0-3-101-116.
- Avrov D.V., Lebedev A.O., Tairov Yu.M. Polytypic inclusions and polytypic stability of silicon carbide crystals. Fizika i tekhnologiya poluprovodnikov, 2016, vol. 50, pp. 501–507.
- Kukushkin S.A., Osipov A.V. Paths of polytypic transformations in silicon carbide. Fizika tverdogo tela, 2019, vol. 61, pp. 1443–1447.
- Pensl G., Clobanu F., Frank T. et al. SiC material properties. International Journal of high speed electronics and systems, 2005, vol. 4, pp. 705–745.
- ElMendili Y., Orberger B., Chateigner D. et al. Insight into the structural, elastic and electronic properties of a new orthorhombic 6O–SiC polytype. Nature, 2020, vol. 10, p. 7562.
- Powell A., Rowland L. SiC Materials – progress, status, and potential roadblocks. Proceedings of the IEEE, 2002, vol. 90, pp. 942–955.
- Elasser A., Chow T. Silicon carbide benefits and advantages for power electronics circuits and systems. Proceedings of the IEEE, 2002, vol. 90, p. 969–986.
- Friedrichs P. Silicon carbide power-device products – Status and upcoming challenges with a special attention to traditional, nonmilitary industrial applications. Physica status Solidi, 2008, vol. 245, pp. 1232–1238.
- Properties of silicon carbide (SiC). Available at: http://ioffe.ru/SVA/NSM/Semicond/SiC/ebasic.html (accessed: August 15, 2025).
- Grunin A.A., Sidorov D.V., Schavnev A.A. Implementation of technology for chemical vapor deposition of silicon carbide in electronics. Part 2. Trudy VIAM, 2025, no. 7 (149), pp. 92–104. Available at: http://www.viam-works.ru (accessed: September 19, 2025). DOI: 10.18577/2307-6046-2025-0-7-92-104.
- Choyke W., Matsunami H., Pensl G. Silicon carbide: recent major advances. Springer, 2004, 430 p.
- Griffin M., Hochberg Y., Inzani K. et al. Silicon carbide detectors for sub-GeV dark matter. Physical review D, 2021, vol. 103, p. 075002.
- Azar M., Ji Z., Jahanzamin J. Fluorescent Silicon Carbide Quantum Dots. Silicon carbide – materials, devices and emerging applications. IntechOpen, 2024, pp. 1–20. DOI: 10.5772/intechopen.1007535.
- Mamun A., McGarrity M., Kim J. et al. Silicon carbide-based DNA sensing technologies. Micromachines, 2023, vol. 14, pp. 1557–1562.
- Song Y., Lu Y., Zhang L. et al. Fabrication of silicon carbide quantum dots via chemical-etching approach and fluorescent imaging for living cells. Materials Sciences and Applications, 2014, vol. 5, pp. 177–182.
- Li X., Zhang Y., Liu Y. et al. Bacteria-targeting BSA-stabilized SiC nanoparticles as a fluorescent nanoprobe for forensic identification of saliva. Microchimica Acta, 2019, vol. 186, pp. 766–773.
- Yao W., Shi J., Ling J. et al. SiC-functionalized fluorescent aptasensor for determination of Рroteus mirabilis. Microchimica Acta, 2020, vol. 187, pp. 406–411.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Sidorov D.V., Schavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 2. Trudy VIAM, 2022, no. 2 (108), pp. 88–98. Available at: http://www.viam-works.ru (accessed: September 19, 2025). DOI: 10.18577/2307-6046-2022-0-2-88-98.
- Sidorov D.V., Schavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 1. Trudy VIAM, 2021, no. 6 (100), pp. 100–111. Available at: http://www.viam-works.ru (accessed: September 19.09.2025). DOI: 10.18577/2307-6046-2021-0-6-100-111.
- Chin J., Gantzel P., Hudson R. The structure of chemical vapor deposited silicon carbide. Thin Solid Films, 1977, vol. 40, pp. 57–72.
- Yang L., Chen Z., Wang B. Chemical vapor deposition of SiC at different molar ratios of hydrogen to methyltrichlorosilane. Journal of central south university of technology, 2009, vol. 16, pp. 0730–0737.
- Ivashchenko V., Turchi P., Shevchenko V. Simulations of the mechanical properties of crystalline, nanocrystalline, and amorphous SiC and Si. Physical Review B, 2007, vol. 75, p. 085209.
- Powell J., Will H. Low-temperature solid-state phase transformations in 2H silicon carbide. Journal of applied physics, 1972, vol. 43, pp. 1400–1408.
- Ito K., Kanno H., Kawahara T., Goto T. 2H–SiC films grown by laser chemical vapor deposition. Journal of the European ceramic society, 2015, vol. 35, pp. 4611–4615.
- Hagasawa H., Yagi K., Kawahara T. et al. Hetero- and homo-epitaxial growth of 3C–SiC for MOSFETs. Microelectronic Engineering, 2006, vol. 83, pp. 185–188.
- Fanton M., Snyder D., Weiland B. et al. Growth of nitrogen-doped SiC boules by halide chemical vapor deposition. Journal of crystal growth, 2006, vol. 287, pр. 359–362.
- Latha H., Udayakumar A., Prasad V. Microstructure and electrical properties of nitrogen doped 3C–SiC thin films deposited using methyltrichlorosilane. Materials science in semiconductor processing, 2015, vol. 29, pp. 117–123.
- Nigam S., Chung H., Polyakov F. Growth kinetics study in halide chemical vapor deposition of SiC. Journal of crystal growth, 2005, vol. 284, pp. 112–122.
- Fissel A. Thermodynamic consideration of the epitaxial growth of SiC polytypes. Journal of crystal growth, 2000, vol. 212, pp. 438–450.
- Maltsev A., Maksimov A., Yushin N. 4H–SiC single crystal ingots grown on 6H–SiC and 15R–SiC seeds. Institute physical conference series, 1996, vol. 142, pp. 41–44.
- Stein R., Lanig P. Control of polytype formation by surface anergy effects during the growth of SiC monocrystals by the sublimation method. Journal of crystal growth, 1993, vol. 131, pp. 71–74.
- Feng Z., Lin H., Xin B. et al. Structural characteristic of 3C–SiC thin films grown on Si-face and C-face 4H–SiC substrates by high temperature chemical vapor deposition. Vacuum, 2023, vol. 207, p. 111643.
- Kanaya M., Takanashi J., Fujiwara Y., Moritani A. Controlled sublimation growth of single crystalline 4HSiC and 6HSiC and identification of polytypes by xray diffraction. Applied physics letters, 1991, vol. 58, pp. 56–58.
- Tairov Y., Tsvetkov V. General principles of growing large-size single crystals of various silicon carbide polytypes. Journal of Crystal Growth, 1981, vol. 52, pр. 146–150.
- Luchinin V.V. Structure and formation of micro- and nanosystems based on wide-band-gap materials possessing polymorphism: thesis, Dr Sc. (Tech.). St. Petersburg, 1999, 503 p.
- Silicon Carbide. Ed. G. Henisz, R. Roy. Trans. from English. Moscow: Mir, 1972, 387 p.
- Shekhawat D., Sudhahar D., Doll J. et al. Phase formation of cubic silicon carbide from reactive silicon–carbon multilayers. MRS Advances, 2023, vol. 8, pp. 494–498.
- Grieseler R., Gallino I., Duboiskaya N. et al. Silicon carbide formation in reactive silicon-carbon multilayers. Materials science forum, 2022, vol. 1062, pp. 44–48.
- Omori M., Takei H., Fukuda T. Formation of cubic SiC crystals by gas-phase reaction. Japanese journal of Applied Physics, 1989, vol. 28, pp. 1217–1220.
- Kuebler L., Hershkovitz E., Kouzminov D. et al. 4H to 3C polytypic transformation in Al+ implanted SiC during high temperature annealing. Electronic materials letters, 2023, vol. 20, pp. 345–351.
- Heinz K., Bernhardt J., Schardt J., Starke U. et al. Functional surface reconstructions of hexagonal SiC. Journal of physics: Condensed matter, 2004, vol. 16, p. 1705.
- Seino K., Oshiyama A. Energetics of the surface step and its morphology on the 3C–SiC(111) surface clarified by the density-functional theory. Applied physics express, 2020, vol. 13, p. 012206.
- Kukushkin S.A., Osipov A.V. Microscopic description of the mechanism of transition between 2H and 4H polytypes of silicon carbide. Fizika tverdogo tela, 2019, vol. 61, pp. 422–425.
- Yoo S., Matsunami H. Solid-state phase transformation in cubic silicon carbide. Japanese Journal of Applied Physics, 1991, vol. 30, pp. 545–549.
- Jepps N., Page T. Polytypic transformation in silicon carbide. Progress in crystal growth and characterization, 1983, vol. 7, pp. 259–307.
- Jayakumari S., Tangstad M. Transformation of β-SiC from charcoal, coal, and petroleum coke to α-SiC at higher temperatures. Metallurgical and materials transaction B, 2020, vol. 51, pp. 2673–2688.
- Moberlychan W., Cao J., Gilbert C. et al. The cubic-to-hexagonal transformation to toughen SiC. Ceramic microstructure: control at the atomic level. New York: Plenum press, 1998, pр. 177–190.
- Soukiassian P., Enriquez H. Atomic scale control and understanding of cubic silicon carbide surface reconstructions, nanostructures and nanochemistry. Journal of Physics: Condensed Matter, 2004, vol. 16, pp. 1611–1658.