Modern technologies of new generation polymer composite materials processing

Timoshkov P.N., Kogan D.I.
Timoshkov P.N., Kogan D.I. Modern technologies of new generation polymer composite materials processing // Proceedings of VIAM. 2013. No. 4. URL: https://www.viam-works.ru/en/journal/2013/4/8
Abstract

Modern technologies of new generation polymer composite materials processing based on polymer resins development of VIAM Federal State Unitary Enterprise and carbon and glass reinforcement fillers is described. The main examples of processing and technological equipment, developed by VIAM Federal State Unitary Enterprise in comparison with foreign analogs, and its characteristics are provided. VIAM Federal State Unitary Enterprise is equipped now with modern research, test and production equipment which allow to develop and produce polymer composite materials by modern technologies, according to all requirements for aviation material of new generation.