Effect of isothermal annealing on the crystallinity degree of polyetherketoneketone containing discrete carbon fibers
Losev A.V., Gulyaev A.I., Juravleva P.L., Antyufeeva N.V. Effect of isothermal annealing on the crystallinity degree of polyetherketoneketone containing discrete carbon fibers // Proceedings of VIAM. 2026. No. 2. DOI: 10.18577/2307-6046-2026-0-2-58-72. URL: https://www.viam-works.ru/en/journal/2026/2/6
Keywords
polyetherketoneketone, additive manufacturing, semicrystalline thermoplastic, X-ray diffraction analysis, microstructure, annealing
Abstract
This study demonstrates the effect of annealing temperature on crystallite size, lattice parameters, and the degree of crystallinity of polyetherketoneketone (PEKK), containing carbon fibers. The particle sizes of the PEKK and carbon fibers were determined using optical and electron microscopy. Temperature dependences of the thermoplastic's degree of crystallinity, calculated using X-ray diffraction analysis, were plotted. The mechanism of isothermal crystallization of PEKK was studied, and the effect of polymer crystallinity on fracture microstructure was demonstrated.
Reference list
- Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polymer composite materials on a thermoplastic matrix. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2016, vol. 59, no. 10, pp. 61–71.
- Kablov E.N., Sagomonova V.A., Sorokin A.E., Tselikin V.V., Gulyaev A.I. Study of the structure and properties of a polymer composite material with an integrated vibration-absorbing layer. Vse materialy. Entsiklopedicheskiy spravochnik, 2020, no. 3, pp. 2–9.
- Kablov E.N., Kondrashov S.V., Melnikov A.A., Pavlenko S.A., Guseva M.A., Pykhtin A.A., Larionov S.A. Investigation of the influence of the thermal regime of FDM printing on the structuring and warping of polyethylene samples. Trudy VIAM, 2021, no. 7 (101), pp. 48–58. Available at: http://www.viam-works.ru (accessed: November 20, 2025). DOI: 10.18577/2307-6046-2021-0-7-48-58.
- Gurov D.A., Pavlyukovich N.G., Tsapenko A.N. 3D printing with composite organic filament based on liquid crystal polymers and polyetheretherketone. Aviation materials and technologies, 2024, no. 4 (77), pp. 62–81. Available at: http://www.journal.viam.ru (accessed: October 14, 2025). DOI: 10.18577/2713-0193-2024-0-4-62-81.
- Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), pp. 41–50. Available at: http://www.journal.viam.ru (accessed: October 14, 2025). DOI: 10.18577/2713-0193-2022-0-1-41-50.
- Pavlukovich N.G., Ivanov М.S., Morozova V.S., Donskih I.N. Investigation of the thermal stability of the melt polyetheretherketone PEEK-50P and carbon fiber based on it. Aviation materials and technologies, 2024, no. 2 (75), pp. 90–98. Available at: http://www.journal.viam.ru (accessed: October 14, 2025). DOI: 10.18577/2713-0193-2024-0-2-90-98.
- Ivanov М.S., Morozova V.S., Pavlukovich N.G. The influence of operational factors on the properties of carbon fiber based on polyetheretherketone. Aviation materials and technologies, 2024, no. 2 (75), pp. 99–108. Available at: http://www.journal.viam.ru (accessed: October 14, 2025). DOI: 10.18577/2713-0193-2024-0-2-99-108.
- Lyashenko E.Yu., Yakovleva K.A., Andreeva T.I. et al. Composite materials based on polyetheretherketone. Plasticheskie massy, 2023, no. 1-2, pp. 11–16. DOI: 10.35164/0554-2901-2023-1-2-11-13.
- Gurov D.A., Tsapenko A.N., Pavlukovich N.G. Effect of mutual stabilization of polyetherether-ketone and thermotropic liquid crystal polymers in polymer composites based on them for 3D printing. Trudy VIAM, 2024, no. 8 (138), pp. 3–18. Available at: http://www.viam-works.ru (accessed: November 20, 2025). DOI: 10.18577/2307-6046-2024-0-8-3-18.
- Gurov D.A., Tsapenko A.N., Pavlukovich N.G. Effect of mutual strengthening in polymer composites based on polyethereketone and thermotropic liquid crystal polymers obtained by 3D-printing. Trudy VIAM, 2024, no. 10 (140), pp. 45–62. Available at: http://www.viam-works.ru (accessed: November 20, 2025). DOI: 10.18577/2307-6046-2024-0-10-45-62.
- Musin I.N., Lisanevich M.S., Lutova D.A. et al. Application of 3D printing of superstructural plastics for medicine (review). Vestnik Tekhnologicheskogo universiteta, 2024, vol. 27, no. 12, pp. 23–33.
- Shakhmurzova K.T., Kurdanova Zh.I., Zhansitev A.A. et al. Synthesis and properties of polyether ketone ketone (review). Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Tekhnologiya tekstilnoy promyshlennosti, 2024, no. 6 (414), pp. 49–66. DOI: 10.47367/0021-3497_2024_6_49.
- Kurdanova Zh.I., Shakhmurzova K.T., Zhansitov A.A. et al. Polyetherketoneketone and composites based on it (review). Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Tekhnologiya tekstilnoy promyshlennosti, 2023, no. 5 (407), pp. 5–19. DOI: 10.47367/0021-3497_2023_5_5.
- Slonov A.L., Musov I.V., Zhansitov A.A. et al. Study of the properties of monofilament based on polyetherketoneketone. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Tekhnologiya tekstilnoy promyshlennosti, 2023, no. 6 (408), pp. 71–80. DOI: 10.47367/0021-3497_2023_6_71.
- Maloney A., Manaf E., Gately N. Annealing 3D printed PEKK: Investigating the impact of annealing on the mechanical, physical, and thermal properties in additively manufactured PEKK. Materials & Design, 2025, vol. 253, art. 113938. DOI: 10.1016/j.matdes.2025.113938.
- Method for producing polyether ketone ketone fibers based on a non-destructive wet dissolution process: pat. 114232109 CN; appl. 24.11.21; publ. 25.03.22.
- Perez-Martin H., Mackenzie P., Baidak A. Crystallisation behaviour and morphological studies of PEKK and carbon fibre/PEKK composites. Composites: Part A, 2022, vol. 159, art. 106992. DOI: 10.1016/j.compositesa.2022.106992.
- Hoang V.-T., Kwon B.-S., Sung J.-W. Postprocessing method-induced mechanical properties of carbon fiber in forced thermoplastic composites. Journal of Thermoplastic Composite Materials, 2020, vol. 36 (1), pp. 1–16. DOI: 10.1177/0892705720945376.
- Roland S., Moghaddam M., Tence-Girault S. et al. Evolution of Mechanical Properties of Aged Poly(ether ketoneketone) explained by a Microstructural Approach. Polymer Degradation and Stability, 2020, vol. 123, pp. 1–23. DOI: 10.1016/j.polymdegradstab.2020.109412.
- Cortes L.Q., Causse N., Dantras E. et al. Morphology and dynamical mechanical properties of poly ether ketoneketone (PEKK) with meta phenyl links. Applied Polymer Science, 2016, vol. 133, pp. 1–10. DOI: 10.1002/app.43396.
- Coulson M., Cortes L.E.Q., Dantras E. et al. Dynamic rheological behavior of poly(ether ketone ketone) from solid state to melt state. Journal of Applied Polymer Science, 2018, vol. 135 (27), Р. 1–7. DOI: 10.1002/APP.46456.
- Pomatto M.E., Crater E.R., Godshall G.F. et al. Blocky bromination of poly(ether ketone ketone) as a means to preserve crystallizability and rapid crystallization kinetics. Polymer Chemistry, 2024, vol. 15, рр. 609–621. DOI: 10.1039/d3py01338c.
- Tence-Girault S., Quibel J., Cherri A. et al. Quantitative Structural Study of Cold-Crystallized PEKK. ACS Applied Polymer Materials, 2021, vol. 3, рр. 1795−1808. DOI: 10.1021/acsapm.0c01380.
- Method for producing polyether ketone ketone: pat. 2791106 Rus. Federation; appl. 15.08.22; publ. 02.03.23.
- Gardner K.H., Hsiao B.S., Matheson Jr. R.R., Wood B.A. Structure, crystallization and morphology of poly (aryl ether ketone ketone). Polymer, 1992, vol. 33, pp. 2483–2495. DOI: 10.1016/0032-3861(92)91128-O.
- Marinosci V., Chen K., Helthuis G.J. et al. Direct observation of the fracture behavior of the polyether ketone ketone (PEKK) spherulites. Applied Polymer Science, 2024, vol. 141 (1), p. 11. DOI: 10.1002/app.54764.