Trends in the development of fire-resistant paintwork coatings for painting elements of aircraft passenger cabin interiors

Kozlova A.A., Shunina M.A., Kozlov I.A.
Kozlova A.A., Shunina M.A., Kozlov I.A. Trends in the development of fire-resistant paintwork coatings for painting elements of aircraft passenger cabin interiors // Proceedings of VIAM. 2026. No. 1. DOI: 10.18577/2307-6046-2026-0-1-186-196. URL: https://www.viam-works.ru/en/journal/2026/1/14
Keywords
paint and varnish materials, fire-resistant coatings, aircraft interior coatings, flammability, adhesion, protective-decorative painting, heat generation, smoke generation
Abstract

This article presents theresults of information search and discusses the main tendencies in the field of creation of fireproof paint and varnish materials and coverings on their basis for painting interior elements of aviation engineering. The research defines the main requirements for interior coatings, and for choice of components for obtaining fire-resistant interior paint and varnish materials and coverings. The most promising research and development for fire-resistant paint coatings are identified.

Reference list
  1. Veshkin E.A., Satdinov R.A., Barannikov A.A. Modern materials for the aircraft cabin. Trudy VIAM, 2021, no. 9 (103), pp. 33–42. Available at: http://www.viam-works.ru (accessed: March 28, 2025). DOI: 10.18577/2307-6046-2021-0-9-33-42.
  2. Garashchenko A.N., Kulkov A.A., Strakhov V.L. The effect of the service life on the flame-retardant efficiency of the bulging coatings and the fire resistance of structures. Aviation materials and technologies, 2022, no. 2 (67), pp. 97–110. Available at: http://www.journal.viam.ru (accessed: March 28, 2025). DOI: 10.18577/2713-0193-2022-0-2-97-110.
  3. Kan A.Ch., Zhelezina G.F., Kulagina G.S., Ayupov T.R. Fire safety of structural organic plastics reinforced with aramid fabrics. Aviation materials and technologies, 2022, no. 4 (69), pp. 51–60. Available at: http://www.journal.viam.ru (accessed: March 28, 2025). DOI: 10.18577/2713-0193-2022-0-4-51-60.
  4. Barbotko S.L. Requirements of aviation standards and methods for assessing the fire safety of aviation materials: history, current status, and development prospects. Vestnik Voronezhskogo instituta GPS MCHS Rossii, 2014, is. 3 (12), pp. 23–33.
  5. Konstantinova N.I., Tsarichenko S.G., Krivoshapkina O.V., Kolesnikov V.V. On the fire hazard of paints and varnishes. Lakokrasochnye materialy i ikh primenenie, 2014, no. 6, pp. 18–22.
  6. Nevzorov G.N., Drinberg A.S., Nedvedskiy G.R. et al. Development of special coatings for the interior spaces of ships and vessels with reduced flammability. Reports of the 5th All-Rus. sc. and pract. Conf. with the participation of young people «Innovative materials and technologies in design». St. Petersburg, 2019, pp. 115–117.
  7. Barbotko S.L., Volny O.S., Kiriyenko O.A., Shurkova E.N. Fire safety assessment of polymeric materials for aviation purposes. Ed. E.N. Kablov. Moscow: VIAM, 2018, 408 p.
  8. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Kondrashov E.K. Paints and Varnishes and Coatings Based on Them in Mechanical Engineering. Moscow: Paint-Media, 2021, p. 141.
  10. Water-Borne Paint and Varnish Coating Composition: pat. 2338766 Rus. Federation; appl. 27.08.07; publ. 20.11.08.
  11. Kablov E.N. The Role of Chemistry in Creating Next-Generation Materials for Complex Technical Systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: UB of RAS, 2016, pp. 25–26.
  12. State Standard R 52020–2003. Water-Dispersible Paints and Varnishes. General Specifications. Moscow: Publ. House of Standards, 2003, 15 p.
  13. Pavlikova S.M., Anisimov S.V., Shurygina Yu.N. Acrylic and styrene acrylic aqueous dispersions in paint and varnish compositions for metal painting. Lakokrasochnye materialy i ikh primenenie, 2017, no. 4, pp. 24–28.
  14. Karpov S.V., Dzhalmukhanova A.S., Badamshina E.R. Synthesis and study of the properties of water-dispersion polyurethanes modified with partial nitrate of B-cyclodextrin. Reports of the academic forum of young scientists from the countries of Greater Eurasia «Continent of Science». Moscow: Center for Scientific and Technical Solutions, 2023, pp. 217–218.
  15. Noble K.L. Waterborne polyurethanes. Progress in Organic Coatings, 1997, vol. 32, no. 1–4, pp. 131–136.
  16. Lee Y., Luo X., Hu S. et al. Corrosion protection studies of crude glycerol-based waterborne polyurethane coating on steel substrate. Journal of The Electrochemical Society, 2016, vol. 163, is. 3, pp. 54–61.
  17. Lei L., Zhong L., Lin X. et al. Synthesis and characterization of waterborne polyurethane dispersions with different chain extenders for potential application in waterborne ink. Chemical Engineering Journal, 2014, vol. 253, pp. 518–525.
  18. Kozlova A.A., Kondrashov E.K. Influence of molecular weight and elemental composition of isocyanates on the properties of fluoropolyurethane enamels. Aviation materials and technologies, 2023, no. 4 (73), pp. 92–100. Available at: http://www.journal.viam.ru (accessed: April 22, 2025). DOI: 10.18577/2713-0193-2023-0-4-92-100.
  19. Halogen-free, non-intumescent, fire retardant coating composition: pat. 3963012 EP; appl. 24.04.20; publ. 07.06.23.
  20. Solvent-soluble fluoropolymer resin for coatings that can be cured at room temperature or at elevated temperatures. Available at: http://www.agcchem.com (accessed: April 05, 2025).
  21. Aqueous coating composition for aircraft interior and aircraft interior: pat. 2016079265 JP; appl. 15.10.14; publ. 16.05.16.
  22. Modified halogenated and halogensulfonated (co)polymer of 4-methylpentene-1, binder, composition and articles based on it: pat. 2252227 Rus. Federation; appl. 04.10.02; publ. 20.05.05.
  23. Water-dispersion paint and varnish composition: pat. 2154078 Rus. Federation; appl. 12.01.99; publ. 10.08.00.
  24. Complex mixed nitrate esters of cellulose with phthalate groups as a polymer base for adhesives, varnishes, paints, coatings, solid rocket propellants and the method for producing them: pat. 2170235 Rus. Federation; appl. 19.04.96; publ. 10.07.01.
  25. Composite single-pack silicate paint: pat. 2645502 Rus. Federation; appl. 14.06.16; publ. 21.02.18.
  26. Water-based paint and varnish composition for coatings: pat. 2087505 Rus. Federation; appl. 11.01.95; publ. 20.08.97.
  27. Aqueous fluorocarbon coating for painting metal base materials: pat. 102408808 CN; appl. 16.09.11; publ. 24.07.13.
  28. Water-based primer coating composition for aluminum substrate: pat. 2016519141 JP; appl. 10.03.15; publ. 20.04.17.
  29. Domnichenko R.G., Vostrikova G.Yu., Nikulin S.S. Production of epoxy-acrylic water-dispersion coatings. Khimiya, fizika i mekhanika materialov, 2019, no. 3 (22), pp. 14–22.
  30. Shinkareva E.V. Composite paints and varnishes based on aqueous epoxy emulsions. Izvestiya Natsionalnoy akademii nauk Belarusi. Seriya khimicheskikh nauk, 2019, vol. 55, no. 3, pp. 329–337.
  31. Khalturinsky N.A. Combustion of polymers, mechanism of action of flame retardants. Uspekhi khimii, 1984, no. 2, pp. 334–339.
  32. Zaripov I.I., Vikhareva I.N., Buylova E.A., Berestova T.V., Mazitova A.K. Additives for reducing the flammability of polymers. Nanotekhnologii v stroitelstve, 2022, no. 14 (2), pp. 156–161.
  33. Water-dispersion paint: pat. 2209223 Rus. Federation; appl. 17.12.01; publ. 27.07.03.
  34. Aqueous flame retardant compositions and aqueous coating compositions comprising such flame retardant compositions: pat. 20220054346 KR; appl. 17.11.20; publ. 31.12.24.
  35. Flame-retardant, isocyanate-free coating composition: pat. 7189392 JP; appl. 23.11.20; publ. 21.12.22.
  36. Fadeev S.S., Bogdanova V.V., Safropenko E.D. Inhibition of polymer combustion. Study of the mechanism of action of synergistic mixtures of antimony oxide and halogen-containing compounds. Moscow: NIITEkhim, 1988, 39 p.
  37. Kablov V.F., Keibal N.A. Polymer materials with functionally active components. Research and technology (part 1). Volgograd: VPI (branch) of VolGTU, 2018, 406 p.
  38. Buravov B.A., Tuzhikov O.O., Al-Hamzavi A.Kh.D. et al. Modern trends in the development of flame retardants for polymer composites. Composition, properties, application. Izvestiya VolgGTU. Ser.: Khimiya i tekhnologiya elementoorganicheskikh monomerov i polimernykh materialov, 2020, no. 12 (247), pp. 7–24.
  39. Al-Hamzawi A.H.D. Phosphorus-Containing Oligoether Methacrylate Binders for Reinforced Plastics with Low Flammability: thesis, Cand. Sci. (Tech.). Volgograd, 2023, 137 p.
  40. Evtushenko Yu.M., Grigoriev Yu.A., Kuchkina I.O. et al. Effect of a Complex Flame Retardant on the Physicochemical Properties of Unsaturated Orthophthalic Resin. Plasticheskie massy, 2020, no. 1–2, pp. 26–29.
  41. Rodrigues J., Shimpi N.G. Nanostructured flame-retardants: An overview. Nano-Structures & Nano-Objects, 2024, vol. 39, p. 101253.
  42. Singh M.K., Rangappa S.M., Misra M. et al. Recent advancements in nanostructured flame-retardants: Types, mechanisms, and applications in polymer composites. Nano-Structures & Nano-Objects, 2025, vol. 42, p. 101468.
  43. Tu Z., Ou H., Ran Y. et al. Preparation and flame retardant properties of organic montmorillonite synergistic intumescent flame retardant polypropylene. Journal of loss prevention in the process industries, 2024, vol. 87, p. 105226
  44. Sankeshi S., Ganapathiraju J., Bajaj P. et al. 2D-nanostructures as flame retardant addives: Recent progress in hybrid polymeric coatings. Nano-Structures & Nano-Objects, 2024, vol. 40, p. 101346.
  45. Qiu X., Wu C., Lin J. et al. Construction of MOFs-based nanocomposites and their application in flame retardant polymers: A rewiew. Polymer degradation and stability, 2024, vol. 229, p. 110982.
  46. Liu C., Zhuang D., Zhou Y. et al. Mechanically reinforced and flame-retardant epoxy resin nanocomposite based on molecular engeneering of POSS. Polymer testing, 2025, vol. 143, p. 108719.
  47. Greiner L., Kukla P., Eibl S., Döring M. Phosphorylated salicylic acid as flame retardant in epoxy resins and composites. Journal of renewable materials, 2022, vol. 10, is. 7, p. 1931–1950.
  48. Greiner L., Kukla P., Eibl S., Döring M. Phosphorus containing polyacrylamides as flame retardants for epoxy-based composites in aviation. Polymers, 2019, vol. 11, is. 2, p. 284.
  49. Kondrashov E.K., Kozlova A.A. UV quantum technologies for the formation of protective, decorative and functional polymer coatings. Part I. Film-forming agents for UV-polymerizable coatings. Lakokrasochnye materialy i ikh primenenie, 2022, no. 10 (546), pp. 20–26.