Application of composite materials and polymer filler in a helicopter blade design

Gusev Y.A., Usacheva M.N., Parakhin I.V., Kovalenko A.V., Vasyukov A.N.
Gusev Y.A., Usacheva M.N., Parakhin I.V., Kovalenko A.V., Vasyukov A.N. Application of composite materials and polymer filler in a helicopter blade design // Proceedings of VIAM. 2025. No. 9. DOI: 10.18577/2307-6046-2025-0-9-50-62. URL: https://www.viam-works.ru/en/journal/2025/9/4
Keywords
polymer composite materials, polymer filler, helicopter blade, prepregs, aviation products, carbon fiber reinforced plastic, fiberglass reinforced plastic
Abstract

This article presents the overview of modern polymer composite materials and polymer fillers used in helicopter blades in Russia and worldwide, as well as the history and prospects for their development. The main requirements for helicopter blade materials, examples of blade elements using PCM and polymer filler, basic reinforcement schemes and manufacturing technologies are presented. The analysis of modern carbon fillers is carried out, and the main differences between medium-modulus and high-strength carbon fibers are considered.

Reference list
  1. Kablov E.N., Gunyaev G.M., Ilchenko S.I. et al. Structural carbon fiber reinforced plastics with increased conductivity. Aviatsionnye materialy i tekhnologii, 2004, no. 2, pp. 25–36.
  2. Postnov V.I., Veshkin E.A., Makrushin K.V., Sudin Yu.I. Technological features of manufacturing polymer composite materials of main rotor blades for a light helicopter. Aviation materials and technologies, 2023, no. 1 (70), paper no. 06. Available at: http://www.journal.viam.ru (accessed: July 23, 2025). DOI: 10.18577/2713-0193-2023-0-1-82-92.
  3. Veshkin E.A., Slavin A.V., Postnova M.V., Apalkova A.V. The role of temperature-time curing conditions in the formation of unidirectional and equally strong carbon fiber plastics properties. Aviation materials and technologies, 2025, no. 2 (79), paper no. 05. Available at: http://www.journal.viam.ru (accessed: July 24, 2025). DOI: 10.18577/2713-0193-2025-0-2-59-71.
  4. Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleinimide binders. Aviation materials and technologies, 2024, no. 4 (77), paper no. 04. Available at: http://www.journal.viam.ru (accessed: July 22, 2025). DOI: 10.18577/2713-0193-2024-0-4-43-61.
  5. Sparless helicopter blade made of polymer composite materials and its manufacturing method: pat. WO2015/102521 A1 Rus. Federation; appl. 30.12.14; publ. 09.07.15.
  6. Kovalenko A.V., Sidelnikov N.K., Sokolov I.I., Tundaykin K.O. Spheroplastic with adjustable viscosity for filling sections of honeycomb structures. Trudy VIAM, 2019, no. 11 (83), paper no. 04. Available at: http://www.viam-works.ru (accessed: July 30, 2025). DOI: 10.18577/2307-6046-2019-0-11-37-43.
  7. Moir I., Seabridge A.G. Aircraft systems. Harlow: Longman Scientific & Technical, 1992, 415 p.
  8. Case J., Chilver A.H., Ross C.T.F. Strength of materials and structures. London: Arnold, 1999, 346 p.
  9. Helicopters. Hexcel. Available at: https://www.hexcel.com/Markets/Space-and-Defense/Helicopters (accessed: July 22, 2025).
  10. SGL Carbon delivers composite materials for Airbus Helicopter rotor blades. CompositeWorld. Available at: https://www.compositesworld.com/news/sgl-carbon-delivers-composite-materials-for-airbus-helicopter-rotor-blades (accessed: July 22, 2025).
  11. Erickson S-64 Air Crane full composite main rotor blades. Jec. Available at: https://www.jeccomposites.com/news/spotted-by-jec/erickson-s-64-air-crane-full-composite-main-rotor-blades (accessed: July 22, 2025).
  12. What are Helicopter Blades Made of? Pilot Teacher. Available at: https://www.pilotteacher.com/what-is-a-helicopter-blade-made-of-it-used-to-be-wood/ (accessed: July 22, 2025).
  13. Edwards K.L., Davenport C. Materials for rotationally dynamic components: rationale for higher performance rotor-blade design. Materials and Design, 2006, vol. 27, pp. 31–35.
  14. Hancox N.L., Mayer R.M. Design data for reinforced plastics: a guide for engineers and designer. London: Chapman & Hall, 1994, 264 p.
  15. Strong A.B. Manufacturing. International encyclopedia of composites. Eds. S.M. Lee. New York: Van Nostrand-Reinhold, 1990, pp. 102–126.
  16. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: July 28, 2025). DOI: 10.18577/2713-0193-2021-0-2-51-61.
  17. Timoshkov P.N. Equipment and materials for the technology of automated calculations prepregs. Aviacionnye materialy i tehnologii, 2016, no. 2, pp. 35–39. DOI: 10.18577/2071-9140-2016-0-2-35-39.
  18. Doroshenko N.I., Chursova L.V. Evolution of materials for blades of helicopters. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 16–18.
  19. Slyusar B.N., Flek M.B., Goldberg E.S. et al. Helicopter engineering technology. Technology of production of helicopter blades and aircraft structures from polymer composite materials. Rostov-on-Don: Publ. house of the SSC of RAS, 2013, 230 p.
  20. Sidorina A.I., Safronov A.M., Kutsevich K.E., Klimenko O.N. Carbon fabrics for aircraft products. Trudy VIAM, 2020, no. 12 (94), paper no. 05. Available at: http://www.viam-works.ru (accessed: July 23, 2025). DOI: 10.18577/2307-6046-2020-0-12-47-58.
  21. Barannikov A.A., Postnova M.V., Krasheninnikova E.V., Vasyukov A.N. Application of new technologies in the production of helicopter main rotor blades. Trudy VIAM, 2021, no. 11 (105). paper no. 09. Available at: http://www.viam-works.ru (accessed: July 23, 2025). DOI: 10.18577/2307-6046-2021-0-11-91-102.
  22. Popov Yu.O., Kolokoltseva T.V., Khrulkov A.V. The new generation of materials and technologies for helicopter blade spars. Aviacionnye materialy i tehnologii, 2014, no. S2, pp. 5–9. DOI: 10.18577/2071-9140-2014-0-s2-5-9.
  23. Sokolov I.I. Spheroplastics based on thermosetting binders for aviation products: thesis, Cand. of Sc. (Tech.). Moscow, 2013, 127 p.
  24. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate. Aviacionnye materialy i tehnologii, 2012, no. 4, pp. 31–38.
  25. Sokolov I.I., Minakov V.T. Spheroplasts for aviation purposes based on epoxy adhesives and dispersed fillers. Klei. Germetiki. Tekhnologii, 2012, no. 5, pp. 22–26.
  26. Doroshenko N.I. Application of PCM in the design of helicopter propeller blades. Polymer composite materials for the aerospace industry: proc. All-Rus. sci. and tech. conf. Moscow: VIAM, 2019, pp. 23–41.
  27. Pascal F., Navarro P., Marguet S., Ferrero J.-F. Study of medium velocity impacts on the lower surface of helicopter blades. Procedia Engineering, 2014, vol. 88, pp. 93–100.
  28. Helicopter rotor blade and method of manufacturing a blade from a composite material: pat. RU 2541574 C1 Rus. Federation; appl. 25.12.13; publ. 20.02.15.
  29. Middleton D.H. Composite materials in aircraft structures. Harlow: Longman Scientific & Technical, 1990, 530 p.
  30. Aristova Е.Yu., Denisova V.А., Drozhzhin V.S. et al. Composite materials using hollow microspheres. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 52–57. DOI: 10.18577/2071-9140-2018-0-1-52-57.
  31. Kolokoltseva T.V., Popov Yu.O., Lantsov I.A., Gusev Yu.A. Prepregs and fiberglass based on VSR-3М resin and fiberglass fabrics for use in helicopter blades. Trudy VIAM, 2023, no. 11 (129), paper no. 06. Available at: http://www.viam-works.ru (accessed: July 23, 2025). DOI: 10.18577/2307-6046-2023-0-11-56-65.
  32. Popov Yu.O., Kolokoltseva T.V., Bespalova L.S., Khrulkov A.V., Kogan D.I. Fiberglass VPS-31 and hybrid composite material VKG-5 from unidirectional prepregs based on melt binder and rope carbon, glass fillers. Aviatsionnye materialy i tekhnologii, 2006, no 1, pp. 10–20.
  33. Composite rotor blade and method of manufacture: pat. US 6659722 B2 USA; appl. 07.11.02; publ. 09.12.03.
  34. Montagnier O. Optimisation of hybrid high-modulus/high-strength carbon fiber reinforced plastic composite drive shafts. Materials & Design, 2013, vol. 46, pp. 88–100.
  35. Morgan P. Carbon Fibers and Their Composites. Boca Raton: CRC Press, 2005, 1200 p.
  36. High Modulus Carbon Fiber: Modulus And Composite Explained. Baetro Machining Blog. Available at: https://baetro-machining.com/blog/high-modulus-carbon-fiber (accessed: July 24, 2025).
  37. Gupta M.K., Srivastava R.K. Mechanical Properties of Hybrid Fibres Reinforced Polymer Composite: A Review. Polymer-Plastics Technology and Engineering, 2015, vol. 55 (6), pp. 1–66.
  38. Ikbal M.H., Ahmed A., Qingtao W. et al. Hybrid composites made of unidirectional T600S carbon and E-glass fabrics under quasi-static loading. Journal of Industrial Textiles, 2017, vol. 46 (7), pp. 1–25.