Fixation of the amorphous state in alloys Co–Cr–W system under the influence of high cooling rates

Valeev R.A., Serov M.M., Leschev N.E., Yaroshenko A.S.
Valeev R.A., Serov M.M., Leschev N.E., Yaroshenko A.S. Fixation of the amorphous state in alloys Co–Cr–W system under the influence of high cooling rates // Proceedings of VIAM. 2025. No. 5. DOI: 10.18577/2307-6046-2025-0-5-51-60. URL: https://www.viam-works.ru/en/journal/2025/5/4
Keywords
metal fiber, high-speed solidification of the melt, amorphous state, method of extraction of a hanging drop of melt
Abstract

The article presents the results of the work carried out at the NRC «Kurchatov Institute» – VIAM Research Center on the application of the hanging melt droplet extraction method to obtain fibers from cobalt alloys of the Co–Cr–W system. The conducted studies have shown that during the quenching of the melt in alloys of the Co–Cr–W system, the amorphous state is fixed, while most of the structure of the obtained fibers is replaced by an amorphous phase. The justified modes of heat treatment providing crystallization of the amorphous phase are given. It is shown that after heat treatment, an increase in the amount of solid solutions based on Co occurs in the obtained samples.

Reference list
  1. Farafonov D.P., Degovec M.L., Rogalev A.M. Research of experimental compositions of wear-resistant alloys on the basis of cobalt for repair and hardening of working blades of high-pressure turbines by method of laser welding. Trudy VIAM, 2017, no. 8 (56), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 15, 2024). DOI: 10.18577/2307-6046-2017-0-8-5-5.
  2. Johns Hopkins University. Metallic Glass: Material Of The Future? Science Daily. Available at: https://www.sciencedaily.com/releases/1998/03/980331074950.htm (accessed: October 18, 2024).
  3. Kablov E.N., Petrakov A.F., Piskorsky V.P., Valeev R.A., Nazarova N.V. Influence of dysprosium and cobalt on the temperature dependence of magnetization and phase composition of the material of the Nd–Dy–Fe–Co–B system. Metallovedenie i termicheskaya obrabotka metallov, 2007, no. 4, pp. 3–10.
  4. Zhang T., Inoue A. Bulk Glassy Alloys in (Fe, Co, Ni)–Si–B System. Materials Transactions (Japan), 2001, vol. 42, no. 6, pp. 1015–1018.
  5. Miller M.K. Microstructure. Bulk Metallic Glasses. Eds. M. Miller, P. Liaw. Boston: Springer, 2008. DOI: 10.1007/978-0-387-48921-6-5.
  6. Аntsiferov V.N., Nechaev A.S. Obtaining rapidly cooled fibers by extraction from the melt. Metallurg, 2013, no. 4, pp. 85–87.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Buzenkov A.V., Burkanov M.V., Valeev R.A., Piskorsky V.P. Properties of sintered magnets Pr–Dy–Fe–Co–B depending on the composition and technological parameters of manufacture. Trudy VIAM, 2024, no. 5 (135), paper no. 09. Available at: http://www.viam-works.ru (accessed: November 17, 2024). DOI: 10.18577/2307-6046-2024- 0-5-91-100.
  9. Evgenov A.G., Shurtakov S.V., Chumanov I.R., Leshchev N.E. New wear-resistant cobalt-based alloy: effect of silicon and carbon on structure and tribotechnical characteristics. Part 1. Aviation materials and technologies, 2021, no. 4 (65), paper no. 07. Available at: http://www.journal.viam.ru (accessed: November 17, 2024). DOI: 10.18577/2713-0193-2021-0-4-59-69.
  10. Serov M.M., Borisov B.V. Production of metal fibers and porous materials from them by the method of extraction of a hanging drop of the melt. Tekhnologiya legkikh splavov, 2007, no. 3, pp. 62–65.
  11. Betzofen S.Ya., Ashmarin A.A., Terentyev V.F. et al. Phase composition and residual stresses in the surface layers of VNS9-Sh tripsteel. Deformatsiya i razrushenie materialov, 2020, no. 6, pp. 12–20.
  12. Metallic glasses. Trans. from Engl. Eds. J.J. Gilmar and H.J. Leamy. Moscow: Metallurgiya, 1984, 264 p.
  13. Davis J.R. ASM Specialty Handbook: Tool Materials. ASM International, 1995, 501 p.
  14. Kurlov A.S., Gusev A.I. Tungsten carbides and the phase diagram of the W–C system. Neorganicheskiye materialy, 2006, vol. 42, no. 2, pp. 156–163.
  15. Fedorchenko I.M. Properties of metal powders, refractory compounds and sintered materials: handbook. Kyiv: Naukova Dumka, 1978, 184 p.
  16. Sinnecker E.H.C.P., Páramo D., Larin V. et al. Glass coated microwires with enhanced coercivity. The Journal of Magnetism and Magnetic Materials, 1999, vol. 203, pp. 54–56.
  17. Popova N., Nikonenko E., Erbolatova G. et al. Impact of thermochemical treatment on structure and phase state of austenitic alloy. AIP Conference Proceedings, 2019, vol. 2167, p. 020287.
  18. Ayache J., Beaunier L., Boumendil J. et al. Sample Preparation Handbook for Transmission Electron Microscopy. Springer Science+Business Media LLC, 2010, 233 p.
  19. Sevalnev G.S., Vostrikov A.V., Nefedkin D.Yu., Moiseenkov V.V., Volkov R.B., Ulyanov E.I. Study of the structure, distribution of carbide phase, hardness and tribotechnical characteristics of high-chromium bearing steels of the martensitic class. Trudy VIAM, 2023, no. 10 (128), paper no. 02. Available at: http://www.viam-works.ru (accessed: November 05, 2024). DOI: 10.18577/2307-6046-2023-0-10-13-23.
  20. Zolotukhin I.V. Physical properties of amorphous metallic materials. Moscow: Metallurgiya, 1986, 176 p.
  21. Zaitsev A.I., Mogutnov B.M., Shakhpazov E.Kh. Amorphization of metallic melts. Moscow: Interkontakt Nauka, 2011, 292 p.