Influence of homogenization modes of ingots and heat treatment of sheets from alloy V95osch-T2 on their structure and properties
Astashkin A.I., Babanov V.V., Selivanov A.A., Tkachenko E.A. Influence of homogenization modes of ingots and heat treatment of sheets from alloy V95osch-T2 on their structure and properties // Proceedings of VIAM. 2025. No. 3. DOI: 10.18577/2307-6046-2025-0-3-12-22. URL: https://www.viam-works.ru/en/journal/2025/3/2
Keywords
aluminum alloy V95och, Al–Zn–Mg–Cu system, homogenization annealing, technological plasticity of ingots, microstructure, mechanical and corrosion properties of sheets, artificial aging
Abstract
The article presents the results of a study of the relationship between the microstructure of V95och alloy ingots after homogenization annealing in single- and two-stage modes with the parameters of technological plasticity in the temperature range of 350–450 °C. There has been stablished the dependence from the homogenization mode of the structure and properties of sheets with a thickness of more than 6 mm made of V95och alloy, aged in a new experimental mode and a serial aging mode T2. We selected the modes of homogenization annealing and aging that ensure achievement of the highest level of service characteristics of sheets.
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
- Antipov V.V. Prospects for development of aluminium, magnesium and titanium alloys for aerospace engineering. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 186–194. DOI: 10.18577/2071-9140-2017-0-S-186-194.
- Tarasov Yu.M., Antipov V.V. The VIAM new materials – for perspective aviation engineering of production of JSC «OAK». Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 5–6.
- Duyunova V.A., Nechaikina T.A., Oglodkov M.S., Yakovlev A.L., Leonov A.A. Promising developments in the field of lightweight materials for modern aerospace technology. Tekhnologiya legkikh splavov, 2018, no. 4, pp. 28–43.
- Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
- Senatorova O.G., Antipov V.V., Bronz A.V. et al. High-strength and super-strong alloys of the traditional Al–Zn–Mg–Cu system, their role in technology and development possibilities. Tekhnologiya legkikh splavov, 2016, no. 2, pp. 43–49.
- Oglodkov M.S., Romanenko V.A., Benarieb I., Rudchenko A.S., Grigoryev M.V. Study of industrial semi-finished products from advanced aluminum-lithium alloys for aircraft products. Aviation materials and technologies, 2023, no. 3 (72), paper no. 05. Available at: http://www.journal.viam.ru (accessed: September 20, 2024). DOI: 10.18577/2713-0193-2023-0-3-62-77.
- Senatorova O.G., Uksusnikov A.N., Legoshina S.F., Ivanov A.L., Sidelnikov V.V. Effect of various small additives on the structure and properties of sheets made of high-strength alloys of the Al–Zn–Mg–Cu system. Aviacionnye materialy i tehnologii, 2002, is.: Promising aluminum, magnesium and titanium alloys for aerospace engineering, pp. 91–95.
- Nikitin V.I. Genetic engineering technologies – a new direction in the production of aluminum alloys. Proc. scientific-technical. conf. «New directions of development of production and consumption of aluminum and its alloys». Samara, 2000, pp. 158–165.
- Aviation materials: handbook in 13 vols. Ed. E.N. Kablov. 7th ed., rev. and add. Moscow: VIAM, 2008, vol. 4: Aluminum and Beryllium Alloys, Part 1: Wrought Aluminum Alloys, book 2, pp. 35–66.
- Fridlyander I.N. Metallurgy of Aluminum Alloys. Moscow: Nauka, 1985, 238 p.
- Kolobnev N.I., Ber L.B., Tsukanov S.L. Heat Treatment of Wrought Aluminum Alloys. Moscow: NP «APRAL», 2020, 552 p.
- Wei Wang, Ralph T. Shuey. Homogenization Model for 7xxx Aluminum Alloy. Proceedings of the 12th International Conference on Aluminium Alloys. Yokohama, 2010, pp. 264–269.
- Nechaykina T.A., Oglodkov M.S., Ivanov A.L., Kozlova O.Yu., Yakovlev S.I., Shlyapnikov M.A. Features of hardening of wide cladding sheets from V95p.ch. aluminum alloy on a continuous heat treatment line. Trudy VIAM, 2021, no. 11 (105), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 20, 2024). DOI: 10.18577/2307-6046-2021-0-11-25-33.
- Astashkin A.I., Zaitsev D.V., Selivanov A.A., Tkachenko E.A. The influence of homogenization annealing оn the structural phase evolution and technological plasticity of aluminum alloy 1163 ingots. Trudy VIAM, 2024, no. 7 (137), paper no. 02. Available at: http://www.viam-works.ru (accessed: September 20, 2024). DOI: 10.18577/2307-6046-2024-0-7-12-23.
- Fridlyander I.N., Berstenev V.V., Tkachenko E.A. et al. Effect of heat treatment and deformation on grain size and mechanical properties of duralumin alloys. Metallovedenie i termicheskaya obrabotka metallov, 2003, no. 7, pp. 3–6.
- Nechaikina T.A., Blinova N.E., Ivanov A.L., Kozlova O.Yu., Kozhekin A.E. Research of the effect of homogenization and quench hardening modes on the structure and mechanical properties of retail rings from alloy В95o.ch.-T2. Trudy VIAM, 2018, no. 10 (70), paper no. 04. Available at: http://www.viam-works.ru (accessed: September 20, 2024). DOI: 10.18577/2307-6046-2018-0-10-27-36.
- Yu-lin Zheng, Cheng-bo Li, Shengdan Liu et al. Effect of homogenization time on quench sensitivity of 7085 aluminum alloy. Transactions of Nonferrous Metals Society of China, 2014, vol. 24, pp. 2275−2281.
- Aryshenskiy V.Yu., Grechnikova A.F., Drits A.M., Sosedkov S.M. Selection of technological parameters for reducing the grain size in the base and cladding of cladding sheets made of aluminum alloys. Tekhnologiya legkikh splavov, 2010, no. 3, pp. 21–30.
- Tkachenko E.A., Senatorova O.G., Milevskaya T.V., Ivanov A.L. Influence of grain size on the complex of properties of clad cladding cold-rolled sheets made of base alloys 1163 and B95pch. Tsvetnye metally, 2014, no. 13, pp. 57–63.