Materials for applying ceramic layers of heat-protective coatings

Artemenko N.I., Benklyan A.S., Stekhov P.A., Aleksandrov D.A.
Artemenko N.I., Benklyan A.S., Stekhov P.A., Aleksandrov D.A. Materials for applying ceramic layers of heat-protective coatings // Proceedings of VIAM. 2025. No. 2. DOI: 10.18577/2307-6046-2025-0-2-75-88. URL: https://www.viam-works.ru/en/journal/2025/2/6
Keywords
thermal protective coating, electron beam deposition, magnetron sputtering, atmospheric plasma sputtering
Abstract

The main methods and materials for applying ceramic layers of heat-protective coatings are considered. The main methods (electron beam method, magnetron sputtering method and atmospheric plasma spraying method) of manufacturing materials for applying ceramic layers of heat-protective coatings for various applications are considered. There are shown methods to increase sphericity and strength of particles for powder materials, which increase stability and reproducibility of the plasma spraying process. 

Reference list
  1. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  2. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Denisova V.S., Malinina G.A., Vlasova O.V., Vinogradova A.Yu. The influence of silicon tetraboride additives on properties of heat-resistant coatings for nickel alloys protection. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 68–73. DOI: 10.18577/2071-9140-2019-0-2-68-73.
  4. Doronin O.N., Gorlov D.S., Azarovsky E.N., Kochetkov A.S. Study of the structure and properties of a heat-resistant coating at high-temperature deformation of samples from titanium intermetallic alloy. Aviation materials and technology, 2021, no. 1 (62), paper no. 06. Available at: http://www.journal.viam.ru (accessed: August 30, 2024). DOI: 10.18577/2713-0193-2021-0-1-61-70.
  5. Kablov E.N., Muboyadzhyan S.A. Heat-resistant and heat-protective coatings for high-pressure turbine blades of advanced gas turbine engines. Metally, 2012, no. 1, pp. 5–13.
  6. Loshchinin Yu.V., Budinovskiy S.A., Razmakhov M.G. Heat conductivity of heat-protective coatings ZrO2–Y2O3 alloyed by REM oxides obtained by magnetronny application. Aviaсionnye materialy i tehnologii, 2018, no. 3, pp. 42–49. DOI: 10.18577/2071-9140-2018-0-3-42-49.
  7. Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), paper no. 10. Available at: http://www.journal.viam.ru (accessed: August 30, 2024). DOI: 10.18577/2713-0193-2022-0-3-108-119.
  8. Liu Q., Huang S., He A. Composite ceramics thermal barrier coatings of yttria stabilized zirconia for aero-engines. Journal of materials science & technology, 2019, vol. 35, no. 12, pp. 2814–2823. DOI: 10.1016/j.jmst.2019.08.003.
  9. Zhang B., Chen K., Baddour N., Patnaik P. Failure and life evaluation of EB-PVD thermal barrier coatings using temperature-process-dependent model parameters. Corrosion Science, 2019, vol. 156, pp. 1–9. DOI: 10.1016/j.corsci.2019.04.020.
  10. Ma X., Rivellini K., Ruggiero P., Wildridge G. Toward durable thermal barrier coating with composite phases and low thermal conductivity. Journal of Thermal Spray Technology, 2020, vol. 29, pp. 423–432. DOI: 10.1007/s11666-020-00979-x.
  11. Shi L., Sun Z., Lu Y. The combined influences of film cooling and thermal barrier coatings on the cooling performances of a film and internal cooled vane. Coatings, 2020, vol. 10, no. 9, p. 861. DOI: 10.3390/coatings10090861.
  12. Herman H. Powders for thermal spray technology. KONA Powder and Particle Journal, 1991, vol. 9, pp. 187–199. DOI: 10.14356/kona.1991024.
  13. Evaporated material condensation in vacuum (arc, magnetronny, electron beam methods). Available at: http://www.helpiks.org (accessed: September 23, 2024).
  14. Amaya C., Prias-Baragan J.J., Aperador W. Thermal conductivity of yttria-stabilized zirconia thin films with a zigzag microstructure. Journal of Applied Physics, 2017, vol. 121, p. 245110.
  15. Saint-gobain coating solutions. Available at: http://www.coatingsolutions.saint-gobain.com (accessed: September 23, 2024).
  16. Chevallier J., Chalk C. Modelling evaporation in electron-beam physical vapour deposition of thermal barrier coatings. Emergent Materials, 2021, vol. 4, no. 6, pp. 1499–1513. DOI: 10.1007/s42247-021-00284-5.
  17. Budinovskiy S.A., Doronin O.N., Kosmin A.A., Benklyan A.S. Influence of the state of the YSZ target on its sputtering rate during deposition of a TBC ceramic layer by the UOKS-3 unit. Aviation materials and technologies, 2021, no. 2 (63), paper no. 09. Available at: http://www.journal.viam.ru (accessed: August 30, 2024). DOI: 10.18577/2713-0193-2021-0-2-85-92.
  18. Mehta A., Vasudev H., Singh S. et al. Processing and advancements in the development of thermal barrier coatings: a review. Coatings, 2022, vol. 12, no. 9, p. 1318. DOI: 10.3390/coatings12091318.
  19. Gaedike B., Guth S., Kern F. et al. Deposition of 3YSZ-TiC PVD coatings with high-power impulse magnetron sputtering (HiPIMS). Applied Sciences, 2021, vol. 11, no. 6, p. 2753. DOI: 10.3390/app11062753.
  20. Kaziev A., Kolodko V., Lisenkov V., Tumarkin A. Cu Metallization of Al2O3 Ceramic by Coating Deposition from Cooled-and Hot-Target Magnetrons. Coatings, 2023, vol. 13, no. 2, p. 238. DOI: 10.3390/coatings13020238.
  21. Heydari P. A review on functionally graded-thermal barrier coatings (FG-TBC) fabrication methods in gas turbines. American Journal of Mechanical and Materials Engineering, 2022, vol. 6, no. 2, pp. 18–26. DOI: 10.11648/j.ajmme.20220602.12.
  22. Li R. High-Temperature oxidation resistance and molten salt corrosion study of YSZ, CeYSZ, and YSZ/CeYSZ thermal barrier coatings by atmospheric plasma spraying. Coatings, 2024, vol. 14, no. 1, р. 102. DOI: 10.3390/coatings14010102.
  23. Artemenko N.I. Research of the operation modes of the Metco F4 serial plasma-gun using plasma-forming gases argon and nitrogen. Trudy VIAM, 2018, no. 5 (65), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 25, 2024). DOI: 10.18577/2307-6046-2018-0-5-76-89.
  24. Artemenko N.I., Tatarnikov S.V., Doronin O.N. Investigation of the influence of the parameters of applying the ceramic layer of the ZrO2–7 % Y2O3 heat-shielding coating by plasma spraying on the productivity of the technological process. Trudy VIAM, 2023, no. 4 (122), paper no. 07. Available at: http://www.viam-works.ru (accessed: August 30, 2024). DOI: 10.18577/2307-6046-2023-0-4-69-80.
  25. Druzhnova Ya.S. Development of methods for thermal spraying of hardening tires based on tungsten and chromium carbides (review). Trudy VIAM, 2022, no. 10 (116), paper no. 09. Available at: http://www.viam-works.ru (accessed: September 30, 2024). DOI: 10.18577/2307-6046-2022-0-10-100-115.
  26. Stunda-Zujeva A., Irbe Z., Berzina-Cimdina L. Controlling the morphology of ceramic and composite powders obtained via spray drying – A review. Ceramics International, 2017, vol. 43, pp. 11543–11551.