Development of a test program for aircraft anticorrosive protection systems of with account of operational factors

Kutyrev A.E., Krivushina A.A., Vdovin A.I.
Kutyrev A.E., Krivushina A.A., Vdovin A.I. Development of a test program for aircraft anticorrosive protection systems of with account of operational factors // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-135-146. URL: https://www.viam-works.ru/en/journal/2025/11/12
Keywords
anticorrosive protection, accelerated tests, galvanic corrosion, fungal resistance, microbiological damage, alternating operational loads
Abstract

The article demonstrates the necessity of developing a methodology for complex testing of aircraft anticorrosive protection systems, which considers the impact of the climatic factors, alongside with the microbiological and operational ones. The latter negatively affect the anticorrosive protection system, which can lead to its destruction, and, consequently to, the development of corrosion damage. The framework of this methodology has been determined, as well as test program required for its development has been created.

Reference list
  1. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  2. Antipov V.V., Klochkova Yu.Yu., Romanenko V.A. Modern aluminum and aluminum-lithium alloys. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 195–211. DOI: 10.18577/2071-9140-2017-0-S-195-211.
  3. Karimova S.A. Corrosion is the main enemy of aviation. Nauka i zhizn, 2007, no. 6, pp. 63–65.
  4. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: April 12, 2024). DOI: 10.18577/2713-0193-2021-0-4-70-80.
  5. Kablov E.N., Karimova S.A., Semenova L.V. Corrosion activity of carbon fiber reinforced plastics and protection of metal load-bearing structures in contact with carbon fiber reinforced plastic. Korroziya: materialy, zashchita, 2011, no. 12, pp. 1–7.
  6. Feigenbaum Yu.M., Dubinsky S.V. Influence of random operational damage on the strength and service life of aircraft structures. Nauchny vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta grazhdanskoy aviatsii, 2013, no. 187, pp. 83–91.
  7. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), paper no. 12. Available at: http://www.viam-works.ru (accessed: April 12, 2024). DOI: 10.18577/2307-6046-2021-0-1-114-122.
  8. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climatic factors (review). Part 2. Main trends. Trudy VIAM, 2021, no. 2 (96), paper no. 11. Available at: http://www.viam-works.ru (accessed: April 12, 2024). DOI: 10.18577/2307-6046-2021-0-2-99-108.
  9. Jenkins M.G., Lara-Curzio E., Gonczy S.T. Mechanical, Thermal and Environmental Testing and Performance of Ceramic Composites and Components. Philadelphia, 2000, 53 р.
  10. Kutyrev А.E., Vdovin A.I., Antipov V.V., Duyunova V.A. Methodological issues of studying the effectiveness of anticorrosion protection used in aviation equipment products. Trudy VIAM, 2024, no. 1 (131), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 12, 2024). DOI: 10.18577/2307-6046-2024-0-1-78-91.
  11. Grossman D.M. More realistic tests for atmospheric corrosion. ASTM Standartization news, 1996, no. 4, pp. 32–39.
  12. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (SSC). Aviacionnye materialy i tehnologii, 2012, no. 4, pp. 18‒22.
  13. LeBozec N., Blandin N., Thierry D. Accelerated corrosion tests in the automotive industry: A comparison of the performance towards cosmetic corrosion. Materials and Corrosion, 2008, vol. 59, no. 11, pp. 889–894.
  14. Kutyrev A.E., Fomina M.A., Chesnokov D.V. Development of a method for cyclic corrosion tests simulating the full-scale exposure of aluminum alloys to a coastal atmosphere. Part 1. Basic principles. Korroziya: materialy, zashchita, 2019, no. 10, pp. 35–42.
  15. Belov D.V., Sokolova T.N., Kartashov V.R. et al. Corrosion of aluminum and aluminum alloys under the influence of microorganisms. Izvestiya vysshikh uchebnykh zavedeniy. Khimiya i khimicheskaya tekhnologiya, 2007, vol. 50, no. 6, pp. 60–61.
  16. Krivushina A.A., Bobyreva T.V., Smirnov D.N. Fungal resistance of Thiokol sealants to tropical microorganisms and test cultures. Part 1. Polymer Science, Series D, 2022, vol. 15, no. 2, pp. 177–182. DOI: 10.1134/S1995421222020149.
  17. Melchers R.E. Modelling of marine immersion corrosion for mild and lowalloy steels – Part 1: Phenomenological model. Corrosion (NACE), 2003, vol. 59 (4), pp. 319–334.
  18. Glikman L.A. Corrosion-mechanical strength of metals. Moscow-Leningrad: Mashgiz, 1955, 175 p.
  19. Vasiliev B.Yu., Shapkin V.S., Barulenkova N.V. et al. Effect of aftereffects of cyclic loads on the corrosion of aluminum alloys. Zashchita metallov, 2006, vol. 42, no. 3, pp. 227–232.
  20. Antonova E.N., Vasiliev B.Yu., Shapkin V.S. Electrochemical diagnostics of Tu-154 aircraft panels after different periods of operation. Nauchnyy vestnik MGTU GA: Aeromekhanika i prochnost, 2002, vol. 53, pp. 110–118.