Influence of the coefficient of asymmetry of the loading cycle on the features of destruction of titanium alloy VT6

Naprienko S.A., Medvedev P.N., Levchenko A.A.
Naprienko S.A., Medvedev P.N., Levchenko A.A. Influence of the coefficient of asymmetry of the loading cycle on the features of destruction of titanium alloy VT6 // Proceedings of VIAM. 2025. No. 11. DOI: 10.18577/2307-6046-2025-0-11-112-123. URL: https://www.viam-works.ru/en/journal/2025/11/10
Keywords
cycle asymmetry coefficient, titanium alloys, alloy VT6, fractography, plastic deformation
Abstract

The influence of various values of the asymmetry coefficient of the loading cycle R (–1 to 0,9) in determining the minimum and maximum values of the bending moment during loading based on N = 106 cycles at which fracture occurs has been studied. It was revealed that the change in R values from –1 to 0,7 do not lead to a change in the fracture structure in the zone of fatigue crack development. At R equal to 0,8 and 0,9, fatigue failure occurs with the formation of chip facets. In the α- and β-phases, the residual macro- and micro-deformations of the crystal lattice increase with increasing values of R and maximum stresses.

Reference list
  1. Kablov E.N. Structural and functional materials ‒ the basis of economic and scientific-technical development of Russia. Voprosy materialovedeniya, 2006, no. 1, pp. 64–67.
  2. Kablov E.N. Heat-resistant structural materials. Liteynoe proizvodstvo, 2005, no. 7, pp. 2–7.
  3. Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. VIAM experience in the field of development and research of economically alloyed titanium alloys of new generation. Trudy VIAM, 2016, no. 9 (45), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 14, 2024). DOI: 10.18577/2307-6046-2016-0-9-5-5.
  4. Kablov E.N. Quality control of materials – a guarantee of safety of operation of aviation equipment. Aviatsionnye materialy i tekhnologii, 2001, no. 1, pp. 3–8.
  5. Prohodceva L.V., Erasov V.S., Lavrova O.Ju., Lavrov A.V. Influence of form of cycle on fatigue properties and microstructure of breaks of VT3-1 titanium alloy. Aviacionnye materialy i tehnologii, 2012, no. 2, pp. 54–58.
  6. Bannikov M.V., Oborin V.A., Naimark O.B. Study of the stages of fracture of titanium alloys in the mode of high- and hygocycle fatigue based on the morphology of the fracture surface. Vestnik Permskogo natsionalnogo issledovatelskogo politekhnicheskogo universiteta. Mekhanika, 2015, no. 3, pp. 15–24.
  7. Ospennikova O.G., Napriyenko S.A., Avtayev V.V. Boundary between single-crystal substrate and received by selective laser melting alloy ZhS32-VI structural and phase changes after high temperatures and tension influence investigation. Trudy VIAM, 2019, no. 1 (73), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 14, 2024). DOI: 10.18577/2307-6046-2019-0-1-115-124.
  8. Shakirtov M.M. On the influence of the external load cycle asymmetry coefficient on the characteristics of the material loading cycle at the tip of a crack-like defect. Trudy MAI, 2016, no. 89, p. 5.
  9. Klevtsov G.V., Botvina L.R., Klevtsova N.A., Limar L.V. Fractal diagnostics of fracture of metallic materials and structures. Moscow: MISiS, 2007, 264 p.
  10. Abalkhan D.Yu., Chigvintsev R.A. Influence of loading cycle asymmetry on the kinetics of fatigue crack growth in titanium alloys. XXVII Regional Conf. of Young Scientists and Researchers of the Volgograd Region: Collection of Conf. Proc. Volgograd, 2022, pp. 78–80.
  11. Gorbovets M.A., Belyaev M.S., Khodynev I.A., Lukyanova M.I. Study of low-cycle fatigue of heat-resistant alloys under a «hard» loading cycle. Tsvetnye metally, 2017, no. 2, pp. 91–95. DOI: 10.17580/tsm.2017.02.15.
  12. Erasov V.S., Oreshko E.I. Fatigue tests of metal materials (review). Part 1. Main definitions, loading parameters, representation of results of tests. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 59–70. DOI: 10.18577/2071-9140-2020-0-4-59-70.
  13. Kapustin V.I., Zakharchenko K.V., Cherepanova V.K., Shayapov V.R. Investigation of dissipative processes of VT6 alloy under fatigue. Aviation materials and technologies, 2022, no. 4 (69), paper no. 09. Available at: http://www.journal.viam.ru (accessed: November 14, 2024). DOI: 10.18577/2713-0193-2022-0-4-96-111.
  14. Duyunova V.A., Pavlova T.V., Kashapov O.S., Chuchman O.V. Fatigue strength of forgings from VT6 alloy for parts of gas turbine engines and aircrafts. Aviation materials and technologies, 2023, no. 2 (71), paper no. 02. Available at: http://www.journal.viam.ru (accessed: November 11, 2024). DOI: 10.18577/2713-0193-2023-0-2-23-35.
  15. Yakovlev A.L., Arislanov A.A., Putyrsky S.V., Nochovnaya N.A. Study of mechanical properties and structure of large-sized semi-finished products made of VT6ch titanium alloy. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 12–18. DOI: 10.18577/2071-9140-2020-0-4-12-18.
  16. Gorelik S.S., Skakov Yu.A., Rastorguev L.N. X-ray and electron-optical analysis: textbook for universities; 4th ed., add. and rev. Moscow: MISiS, 2002, 360 p.
  17. Umansky Ya.S., Skakov Yu.A., Ivanov A.N., Rastorguev L.N. Crystallography, X-ray diffraction and electron microscopy. Moscow: Metallurigya, 1982, 632 p.
  18. Naprienko S.A., Medvedev P.N., Raevskikh A.N., Popov M.A. Diffraction research methods in the analysis of the plastic deformation zone under the fracture surface. Vestnik moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Mechanical Engineering, 2019, no. 4 (127), pp. 97–110.
  19. Bache M.R. A review of dwell sensitive fatigue in titanium alloys: the role of microstructure, texture and operating conditions. International Journal of Fatigue, 2003, vol. 25, pp. 1079–1087.
  20. Mills M., Ghosh S., Rokhlin S. et al. The Evaluation of Cold Dwell Fatigue in Ti-6242. New Jersey, 2018, 198 p.
  21. Naprienko S.A., Kashapov O.S., Zaitsev D.V., Medvedev P.N. Features of fracture of titanium alloy VT8-1 under cold creep conditions. Deformatsiya i razrushenie materialov, 2024, no. 6, pp. 30–38.
  22. Zhihong W., Hongchao K., Nana C. et al. Recent developments in cold dwell fatigue of titanium alloys for aero-engine applications: a review. Journal of Materials Research and Technology, 2022, vol. 20, pp. 469–484.
  23. Dunne F.P.E., Rugg D. On the mechanisms of fatigue facet nucleation in titanium alloys. Fatigue & Fracture of Engineering Materials & Structures, 2008, no. 31, рр. 949–958. DOI: 10.1111/j.1460-2695.2008.01284.x.
  24. Stroh A.N. The Formation of Cracks as a Result of Plastic Flow. Proceedings of the Royal Society a Mathematical, Physical and Engineering Sciences, 1954, no. 223, pp. 404–414. DOI: 10.1098/rspa.1954.0124.