Fundamental and applied projects on titanium alloys and perspective areas of their development

Khorev А.I.
Khorev А.I. Fundamental and applied projects on titanium alloys and perspective areas of their development // Proceedings of VIAM. 2013. No. 2. URL: https://www.viam-works.ru/en/journal/2013/2/4
Abstract

A complex of fundamental and applied research projects aimed at titanium alloys development as well as their process engineering and technologies of aviation, rocket and space parts production have been carried out. There were designed theories of complex alloying, microalloying, thermal and thermomechanical treatments, textural strengthening, composite materials with outer and inside reinforcement by high-strength fibers, multilayered and plated composite materials.