Study of salt desposition rate on the surface of various fibre-reinforced plastic materials during exposure to a seaside atmosphere

Kornienko G.V., Startsev O.V., Alexandrova T.V., Dvirnaya E.V.
Kornienko G.V., Startsev O.V., Alexandrova T.V., Dvirnaya E.V. Study of salt desposition rate on the surface of various fibre-reinforced plastic materials during exposure to a seaside atmosphere // Proceedings of VIAM. 2025. No. 10. DOI: 10.18577/2307-6046-2025-0-10-156-176. URL: https://www.viam-works.ru/en/journal/2025/10/12
Keywords
salt disposition rate, fibre-reinforced plastics, the capillary electrophoresis method, wet candles, dry plates
Abstract

The salt deposition rate on the surface of different fibre-reinforced plastics and standard samples of «wet candles» and «dry plates» during the exposure in a seaside atmosphere in various distances from the sea has been studied. During one year of the exposure, the content of different ions on the surface of the samples was determined by the capillary electrophoresis method. The dependence of the salt content on the surface of various samples on the duration of winds, blowing from the sea, and surface roughness profile of materials, was established.

Reference list
  1. Irving P., Soutis C. Polymer composites in the aerospace industry. 2nd ed. Woodhead Publishing, 2019, 688 p. DOI: 10.1017/aer.2020.118.
  2. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Herald of the Russian Academy of Sciences, 2023, vol. 93, no. 10, pp. 907–916. DOI: 10.31857/S0869587323100055.
  3. Xu X., Peng G., Zhang B. et al. Material performance, manufacturing methods, and engineering applications in aviation of Carbon fiber reinforced polymers: A comprehensive review. Thin-Walled Structures, 2024, vol. 209, art. 112899. DOI: 10.1016/j.tws.2024.112899.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: April 05, 2024). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Gulyev I.N., Zelenina I.V., Valevin E.O., Khaskov M.A. Influence of climatic ageing on the properties of high-temperature carbon fiber reinforced plastics. Trudy VIAM, 2021, no. 2 (96), paper no. 05. Available at: http://www.viam-works.ru (accessed: April 05, 2024). DOI: 10.18577/2307-6046-2021-0-2-39-51.
  6. Qin G., Fan Q., Mi P. et al. Review of aging mechanisms, mechanical properties, and prediction models of fiber-reinforced composites in natural environments. Polymer Composites, 2024, vol. 45, no. 16, pp. 14448–14474. DOI: 10.1002/pc.28799.
  7. Kablov E.N., Kirillov V.N., Startsev O.V., Krotov A.S. Climatic aging of composite aviation materials: III. Significant aging factors. Russian Metallurgy (Metally), 2012, vol. 2012, no. 4, рр. 323–329. DOI: 10.1134/S0036029512040040.
  8. Startsev V.O., Valevin E.O., Vardanyan A.M., Nechaev A.A. Evaluation of the stability of aircraft carbon fiber reinforced plastics to atmospheric precipitation. New generation materials and technologies for advanced products of aviation and space technology. Moscow, 2021, аrt. 05.
  9. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials. Moscow: NRC «Kurchatov Institute» – VIAM, 2023, 520 p.
  10. Kablov E.N., Lebedev M.P., Startsev O.V., Golikov N.I. Climatic tests of materials, structural elements, machinery and equipment under conditions of extremely low temperatures. Proc. VI Eurasian Symposium on the Problems of Strength of Materials and Machines for Cold Climate Regions EURASTRENCOLD–2013. Yakutsk, 2013, pp. 5–7.
  11. Startsev O.V., Lebedev M.P., Kychkin A.K. Aging of polymer composite materials in extremely cold climates. Izvestiya Altayskogo gosudarstvennogo universiteta, 2020, no. 1 (111), pp. 41–51. DOI: 10.14258/izvasu(2020)1-06.
  12. Vidinha H., Branco R., Amaro A.M., Neto M.A. Monotonic and fatigue behavior of notched glass fibre-reinforced polymer laminates immersed in seawater. Theoretical and Applied Fracture Mechanics, 2023, vol. 126, art. 103977. DOI: 10.1016/j.tafmec.2023.103977.
  13. Ghabezi P., Harrison N.M. Multi-scale modelling and life prediction of aged composite materials in salt water. Journal of Reinforced Plastics and Composites, 2024, vol. 43, no. 3–4, pp. 205–219. DOI: 10.1177/07316844231160189.
  14. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Corrosive aggressiveness of the coastal atmosphere. Part 1. Influencing factors (review). Korroziya: materialy, zashchita, 2013, no. 12, pp. 6–18.
  15. Kablov E.N., Startsev O.V., Medvedev I.M. Corrosive aggressiveness of the coastal atmosphere. Part 2. New approaches to assessing the corrosivity of coastal atmospheres. Korroziya: materialy, zashchita, 2016, no. 1, pp.1–15.
  16. Raman R.K.S., Guo F., Al-Saadi S., Zhao X.L. Understanding fibre-matrix degradation of FRP composites for advanced civil engineering applications: an overview. Corrosion and Materials Degradation, 2018, vol. 1, no. 1, pp. 27–41. DOI: 10.3390/cmd1010003.
  17. Startsev V.O. Effect of aggressive liquids on properties of polymer composite materials (review). Trudy VIAM, 2022, no. 8 (114), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 05, 2025). DOI: 10.18577/2307-6046-2022-0-8-98-112.
  18. Cao Y., Gao G., Wang W. et al. Deterioration behaviors of phenolic amine/epoxy-based GFRP laminates exposed to aggressive environments. Composites Part A: Applied Science and Manufacturing, 2025, vol. 192, art. 108788. DOI: 10.1016/j.compositesa.2025.108788.
  19. Startsev V.O. The degradation of polymer composite materials in seawater (review). Aviation materials and technologies, 2023, no. 1 (70), paper no. 12. URL: http://www.journal.viam.ru (accessed: April 05, 2024). DOI: 10.18577/2713-0193-2023-0-1-148-170.
  20. Yang Y., Silva M.A.G., Silva R.J.C. Material degradation of CFRP-to-steel joints subjected to salt fog. Composites Part B: Engineering, 2019, vol. 173, art. 106884. DOI: 10.1016/j.compositesb.2019.05.095.
  21. Deng K., Luo B., Suo H. et al. Characterization of material degradation mechanism of carbon fiber reinforced epoxy resin composites under ultraviolet radiation and salt-fog synergistic environment. Polymer Composites, 2024, vol. 45, no. 1, pp. 805–824. DOI: 10.1002/pc.27816.
  22. Fiore V., Calabrese L., Miranda R., Badagliacco D. An experimental investigation on performances recovery of glass fiber reinforced composites exposed to a salt-fog/dry cycle. Composites Part B: Engineering, 2023, vol. 257, art. 110693. DOI: 10.1016/j.compositesb.2023.110693.
  23. da Silva G.A.S., d’Almeida J.R.M., Cardoso D.C.T. Investigation on moisture absorption behavior on GFRP and neat epoxy systems in hygrothermal salt fog aging. Composites Part B: Engineering, 2024, vol. 272, art. 111214. DOI: 10.1016/j.compositesb.2024.111214.
  24. Anderson E., Gunawan B., Nicholas J. A multicontinuum-theory-based approach to the analysis of fiber-reinforced polymer composites with degraded stiffness and strength properties due to moisture absorption. Journal of Marine Science and Engineering, 2023, vol. 11, no. 2, art. 421. DOI: 10.3390/jmse11020421.
  25. Wang D., Gong Q., Yuan Q., Luo S. Review of the properties of fiber-reinforced polymer-reinforced seawater–sea sand concrete. Journal of Materials in Civil Engineering, 2021, vol. 33, no. 10, art. 04021285. DOI: 10.1061/(ASCE)MT.1943-5533.0003894.
  26. Zhao Y., Liu W., Seah L.K., Chai G.B. Delamination growth behavior of a woven E-glass/bismaleimide composite in seawater environment. Composites Part B: Engineering, 2016, vol. 106, pp. 332–343. DOI: 10.1016/j.compositesb.2016.09.045.
  27. Gellert E.P., Turley D.M. Seawater immersion ageing of glass-fibre reinforced polymer laminates for marine applications. Composites Part A: Applied Science and Manufacturing, 1999, vol. 30, no. 11, pp. 1259–1265. DOI: 10.1016/S1359-835X(99)00037-8.
  28. Nan J., Zhi C., Meng J., Miao M. Seawater aging effect on fiber-reinforced polymer composites: Mechanical properties, aging mechanism, and life prediction. Textile Research Journal, 2023, vol. 93, no. 13–14, pp. 3393–3413. DOI: 10.1177/00405175231152666.
  29. Kini M.V., Pai D. The ageing effect on static and dynamic mechanical properties of fibre reinforced polymer composites under marine environment – a review. Materials Today: Proceedings, 2022, vol. 52, no. 3, pp. 689–696. DOI: 10.1016/j.matpr.2021.10.084.30.26.
  30. Ghabezi P., Harrison N.M. Indentation characterization of glass/epoxy and carbon/epoxy composite samples aged in artificial salt water at elevated temperature. Polymer Testing, 2022, vol. 110, art. 107588. DOI: 10.1016/j.polymertesting.2022.107588.
  31. Shetty K., Bojja R., Srihari S. Effect of hygrothermal aging on the mechanical properties of IMA/M21E aircraft-grade CFRP composite. Advanced Composites Letters, 2020, vol. 29, art. 2633366X2092652. DOI: 10.1177/2633366X20926520.
  32. Yang S., Chu M., Chen F. et al. Effect of different environmental conditions on durabilities of polyester and vinylester-based glass-fiber-reinforced polymer pultruded profiles. Frontiers in Materials, 2022, vol. 9, art. 862872. DOI: 10.3389/fmats.2022.862872.
  33. Srihari S., Revathi A., Rao R. Hygrothermal effects on RT-cured glass-epoxy composites in immersion environments. Part B: Degradation studies. Journal of Reinforced Plastics and Composites, 2002, vol. 21, no. 11, pp. 993–1002. DOI: 10.1177/073168402128987653.
  34. Wang J., GangaRao H., Liang R. Durability of glass fiber-reinforced polymer composites under the combined effects of moisture and sustained loads. Journal of Reinforced Plastics and Composites, 2015, vol. 34, no. 21, pp. 1739–1754. DOI: 10.1177/0731684415596846.
  35. Kafodya I., Xian G., Li H. Durability study of pultruded CFRP plates immersed in water and seawater under sustained bending: Water uptake and effects on the mechanical properties. Composites Part B: Engineering, 2015, vol. 70, pp. 138–148. DOI: 10.1016/j.compositesb.2014.10.034.
  36. Hong B., Xian G., Li H. Comparative study of the durability behaviors of epoxy and polyurethane-based CFRP plates subjected to the combined effects of sustained bending and water/seawater immersion. Polymers, 2017, vol. 9, no. 11, art. 603. DOI: 10.3390/polym9110603.
  37. Fakhrul T., Islam M.A. Degradation behavior of natural fiber reinforced polymer matrix composites. Procedia Engineering, 2013, vol. 56, pp. 795–800. DOI: 10.1016/j.proeng.2013.03.198.
  38. Chen Y., Davalos J.F., Ray I., Kim H.Y. Accelerated aging tests for evaluations of durability performance of FRP reinforcing bars for concrete structures. Composite structures, 2007, vol. 78, no. 1, pp. 101–111. DOI: 10.1016/j.compstruct.2005.08.015.
  39. Wu G., Wang X., Wu Z. Durability of basalt fibers and composites in corrosive environments. Journal of Composite Materials, 2015, vol. 49, no. 7, pp. 873–887. DOI: 10.1177/0021998314526628.
  40. Startsev V.O., Startsev O.V., Zeleneva T.O., Vardanyan A.M. Influence of precipitation on changes in the mass of samples of polymeric composite materials in open climatic conditions. Aviation materials and technologies, 2024, no. 1 (74), paper no. 11. Available at: http://www.journal.viam.ru (accessed: April 05, 2024). DOI: 10.18577/2713-0193-2024-0-1-136-154.
  41. Lu Z., Xie J., Zhang H., Li J. Long-term durability of basalt fiber-reinforced polymer (BFRP) sheets and the epoxy resin matrix under a wet–dry cyclic condition in a chloride-containing environment. Polymers, 2017, vol. 9, no. 12, art. 652. DOI: 10.3390/polym9120652.
  42. Bhat R., Mohan N., Sharma S. Influence of seawater absorption on the hardness of glass fiber/polyester composite. Journal of Computer Mechanical Management, 2022, vol. 1, no. 1, pp. 1–11. DOI: 10.57159/gadl.jcmm.1.1.23003.
  43. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. II. Development of methods for studying the early stages of aging. Deformatsiya i razrusheniye materialov, 2020, no. 1, pp. 15–21. DOI: 10.31044/1814-4632-2020-1-15-21.
  44. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  45. Kablov E.N., Startsev V.O. Climatic aging of polymer composite materials for aviation purposes. I. Assessment of the influence of significant impact factors. Deformatsiya i razrusheniye materialov, 2019, no. 12, pp. 7–16. DOI: 10.31044/1814-4632-2019-12-7-16.
  46. Pershina N.A., Ionin V.A., Polischuk A.I. The influence of the proximity of the sea and corrosive agents of the atmosphere on the corrosion rate in different climatic regions. Climate–2018: Issues of forecasting corrosion, aging and biodeterioration of materials. Moscow, 2018, pp. 227–238.
  47. Vetrova E.Yu., Shchekin V.K., Kurs M.G. Comparative evaluation of methods for the determination of corrosion aggressivity of the atmosphere. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 74–81. DOI: 10.18577/2071-9140-2019-0-1-74-81.
  48. Zhirnov A.D., Strekalov P.V., Karimova S.A., Zhilikov V.P. Seasonal dynamics of the metal corrosion process in the coastal zone of the Black Sea. Korroziya: materialy, zashchita, 2007, no. 8, pp. 23–29.
  49. State Standard 9.039–74. ESZKS. Corrosive aggressiveness of the atmosphere. Moscow: Publ. house of standards, 1974. 39 p.
  50. Panin S.V., Startsev O.V., Krotov A.S., Medvedev I.M., Frolov A.S. Corrosion and aging of structural materials surface studied by 3D microscopy. Trudy VIAM, 2014, no. 12, paper no. 12. Available at: http://www.viam-works.ru (accessed: April 05, 2025). DOI: 10.18577/2307-6046-2014-0-12-12-12.
  51. Startsev V.O., Kutsevich K.E., Khrulev K.A., Molokov M.V. Predicting the surface temperature of composite material samples based on adhesive prepregs when exposed to climatic conditions. Klei. Germetiki. Tekhnologii, 2017, no. 9, pp. 24–31.
  52. Nikolaev E.V., Barbotko S.L., Andreeva N.P., Pavlov M.R., Grashchenkov D.V. Complex research of influence of climatic and operational factors on new generation epoxy binding and polymeric composite materials on its basis. Part 4. Natural climatic tests of polymeric composite materials on the basis of epoxy matrix. Trudy VIAM, 2016, no. 6, paper no. 11. Available at: http://www.viam-works.ru (accessed: April 05, 2025). DOI: 10.18577/2307-6046-2016-0-6-11-11.
  53. Kutsevich K.E., Dementeva L.A., Lukina N.F. Properties and application of polymer composite materials based on glue prepregs. Trudy VIAM, 2016, no. 8, paper no. 7. Available at: http://www.viam-works.ru (accessed: April 05, 2025). DOI: 10.18577/2307-6046-2016-0-8-7-7.
  54. Tolkachev A.P. Features of the chemical composition of sea water. Shag v nauku, 2019, no. 3, pp. 115–117.
  55. Andrulionis N.Yu., Zavyalov I.B., Rozhdestvensky S.A. The main ionic composition of the waters of the Kerch Strait and adjacent waters. Morskoy gidrofizicheskiy zhurnal, 2024, vol. 40, no. 1 (235), pp. 87–107.
  56. Panchenko Yu.M., Marshakov A.I., Nenasheva T.A. et al. Corrosion resistance of structural metals with different orientation of samples at different distances from the seashore. Korroziya: zashchita materialov i metody issledovaniy, 2024, no. 2, pp. 29–44. DOI: 10.61852/2949-3412-2024-2-2-29-44.