Thermal diffusion coatings and their applications

Knyazev A.V., Dyomin S.A., Fomina M.A., Batrakov E.N.
Knyazev A.V., Dyomin S.A., Fomina M.A., Batrakov E.N. Thermal diffusion coatings and their applications // Proceedings of VIAM. 2024. No. 9. DOI: 10.18577/2307-6046-2024-0-9-54-70. URL: https://www.viam-works.ru/en/journal/2024/9/6
Keywords
structural steels, thermal diffusion coatings, corrosion, sulfide-oxide corrosion, corrosion protection, anti-corrosion coatings, diffusion
Abstract

The paper is dedicated to a review of scientific advances in the application of thermal diffusion coatings to protect materials from aggressive environments. Diffusion saturation allows the formation of the desired phase structure in the surface layers of parts by doping with aluminum, boron, chromium, or silicon. Thermal diffusion protective coatings can serve as a replacement for traditionally applied coatings to protect against atmospheric corrosion of steel parts, improve the hardness, wear resistance, and heat resistance of nickel-alloy parts or protect stainless steels from exposure to corrosive media.

Reference list
  1. Kablov E.N. Marketing of materials science, aircraft engineering and industry: present and future. Direktor po marketingu i sbytu, 2017, no. 5–6, pp. 40–44.
  2. Kablov E.N., Startsev V.O. Measurement and forecasting of materials samples’ temperature during weathering in different climatic zones. Aviacionnye materialy i tehnologii, 2020, no. 4 (61), pp. 47–58. DOI: 10.18577/2071-9140-2020-0-4-47-58.
  3. Kablov E.N., Khmeleva K.M., Zavarzin S.V., Kozlov I.A., Lonskii S.L. The effect of heat treatment on the characteristics of aluminium-zinc coatings obtained by the cold spray method. Aviation materials and technologies, 2022, no. 1 (66), paper no. 07. Available at: http://www.journal.viam.ru (ассеssed: August 05, 2024). DOI: 10.18577/2713-0193-2022-0-1-78-91.
  4. Zhabin A.N., Nyafkin A.N., Serpova V.M., Krasnov E.I. Methods of physical vapor deposition for the manufacture of metal matrix composites (review). Trudy VIAM, 2020, no. 11 (93), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 05, 2024). DOI: 10.18577/2307-6046-2020-0-11-68-75.
  5. Kablov E.N., Akinina M.V., Volkova E.F., Mostyaev I.V., Leonov A.A. The research of aspects of phase composition and fine structure of magnesium alloy ML9 in the as-cast and heat-treated conditions. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 17–24. DOI: 10.18577/2071-9140-2020-0-2-17-24.
  6. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  7. Кablov E.N. VIAM: new generation materials for PD-14. Krylya Rodiny, 2019, no. 7–8, pp. 54–58.
  8. Kablov E.N. Materials and chemical technologies for aviation equipment. Vestnik Rossiyskoy akademii nauk, 2012, vol. 82, no. 6, pp. 520–530.
  9. Wang P., He W., Mauer G. et al. Monte Carlo simulation of column growth in plasma spray physical vapor deposition process. Surface and Coatings Technology, 2018, vol. 335, pp. 188–197.
  10. Öchsner A., Murch G.E., Delgado J.M.P.Q. Microstructure and properties of CBN diffusion coating on high-speed steel. Defect and Diffusion Forum, 2011, vol. 312–315, pp. 542–547.
  11. Zhang H., Pan Y., He Y.Z. Grain refinement and boundary misorientation transition by annealing in the laser rapid solidified 6FeNiCoCrAlTiSi multicomponent ferrous alloy coating. Surface and Coatings Technology, 2011, vol. 205, pp. 4068–4072.
  12. Qi K., Yang Y., Hu G.F. et al. Thermal expansion control of composite coatings on 42CrMo by laser cladding. Surface and Coatings Technology, 2020, vol. 397, p. 125983.
  13. Kuo Y.L., Chang K.H. Atmospheric pressure plasma enhanced chemical vapor deposition of SiOx films for improved corrosion resistant properties of AZ31 magnesium alloys. Surface and Coatings Technology, 2015, vol. 283, pp. 194–200.
  14. García J.R., Fernández J.E., Cuetos J.M., Costales F.G. Fatigue effect of WC coatings thermal sprayed by HVOF and laser treated, on medium carbon steel. Engineering Failure Analysis, 2011, vol. 18, pp. 1750–1760.
  15. Yu O., Goncharov I.V., Sapegina R.R. et al. Tantalum chemical vapour deposition on steel and tungsten substrates in the TaBr5-cd-He system. Surface and Coatings Technology, 2019, vol. 377, p. 124893.
  16. Wang W., Wang D., Han F.S. Improvement of corrosion resistance of twinning-induced plasticity steel by hot-dipping aluminum with subsequent thermal diffusion treatment. Materials Letters, 2019, vol. 248, pp. 60–64.
  17. Kurt B., Özdoğan L., Güney B. et al. Characterization and wear behavior of TiBC coatings formed by thermo-reactive diffusion technique on AISI D6 steel. Surface and Coatings Technology, 2020, vol. 385, p. 125332.
  18. Fan X.S., Yang Z.G., Xia Z.X. et al. The microstructure evolution of VC coatings on AISI H13 and 9Cr18 steel by thermo-reactive deposition process. Journal of Alloys and Compounds, 2010, vol. 505, pp. L15–L18.
  19. Kong D.J., Wang J.C., Guo H.Y. XPS and EDS analysis of VC coatings prepared by TD process. Rare Metal Materials and Engineering, 2016, vol. 45, pp. 297–302.
  20. Sun C.Y., Xue Q., Zhang J. et al. Growth behavior and mechanical properties of Cr–V composite surface layer on AISI D3 steel by thermal reactive deposition. Vacuum, 2018, vol. 148, pp. 158–167.
  21. Tong L., Dengzun Y., Chungen Z. Low-temperature formation of aluminide coatings on Ni-base superalloys by pack cementation process. Chinese Journal of Aeronautics, 2010, vol. 23, pp. 381–385.
  22. Qiao M., Zhou C. Hot corrosion behavior of Co modified NiAl coating on nickel base superalloys. Corrosion Science, 2012, vol. 63, pp. 239–245.
  23. He H., Liu Z., Wang W., Zhou C. Microstructure and hot corrosion behavior of Co–Si modified aluminide coating on nickel based superalloys. Corrosion Science, 2015, vol. 100, pp. 466–473.
  24. Mohammadi K., Haghi A.K. A study on characterization of pack-cemented aluminide coating on metals. Journal of Materials Processing Technology, 2008, vol. 201, pp. 669–672.
  25. Xiang Z.D., Datta P.K. Relationship between pack chemistry and aluminide coating formation for low-temperature aluminisation of alloy steels. Acta Materialia, 2006, vol. 54, pp. 4453–4463.
  26. Fähsing D., Oskay C., Meibner T.M., Galetz M.C. Corrosion testing of diffusion-coated steel in molten salt for concentrated solar power tower systems. Surface and Coatings Technology, 2018, vol. 354, pp. 46–55.
  27. Vourlias G., Pistofidis N., Chaliampalias D. et al. Zinc deposition with pack cementation on low carbon steel substrates. Journal of Alloys and Compounds, 2006, vol. 416, pp. 125–130.
  28. Xue Q., Sun C., Yu J.Y. et al. Microstructure evolution of a Zn–Al coating co-deposited on low-carbon steel by pack cementation. Journal of Alloys and Compounds, 2017, vol. 699, pp. 1012–1021.
  29. Cheng J., Yi S., Park J.S. Simultaneous coating of Si and B on Nb–Si–B alloys by a halide activated pack cementation method and oxidation behaviors of the alloys with coatings at 1100 °C. Journal of Alloys and Compounds, 2015, vol. 644, pp. 975–981.
  30. Pourasad J., Ehsani N. In-situ synthesis of SiC–ZrB2 coating by a novel pack cementation technique to protect graphite against oxidation. Journal of Alloys and Compounds, 2017, vol. 690, pp. 692–698.
  31. Zhao Y.G., Zhou W., Qin Q.D. et al. Effect of pre-oxidation on the properties of aluminide coating layers formed on Ti alloys. Journal of Alloys and Compounds, 2005, vol. 391, pp. 136–140.
  32. Chaliampalias D., Papazoglou M., Tsipas S. et al. The effect of Al and Cr additions on pack cementation zinc coatings. Applied Surface Science, 2010, vol. 256, pp. 3618–3623.
  33. Qiao Y.Q., Guo X.P. Formation of Cr-modified silicide coatings on a Ti–Nb–Si based ultrahigh-temperature alloy by pack cementation process. Applied Surface Science, 2010, vol. 256, pp. 7462–7471.
  34. Stathokostopoulos D., Chaliampalias D., Stefanaki E.C. et al. Structure, morphology and electrical properties of Mg2Si layers deposited by pack cementation. Applied Surface Science, 2013, vol. 285, pp. 417–424.
  35. Thermochemical Surface Engineering of Steels. Eds. E.J. Mittemeijer, M.A.J. Somers. Cambridge: Elsevier, Woodhead Publishing, 2014, 792 p.
  36. Handbook of Hard Coatings: Deposition Technologies, Properties and Applications. Ed. R.F. Bunshah. New York: Noyes Publ., Park Ridge, 2001, 560 p.
  37. Budinski K.G. Overview of Surface Engineering and Wear. Ohaio: ASTM International Publishing, 1996, 21 p.
  38. Surface Hardening of Steels: Understanding the Basics. Ed. J.R. Davis. Ohaio: ASM International, 2002, 364 p.
  39. Surface Engineering for Corrosion and Wear Resistance. Ed. J.R. Davis. Ohaio: ASM International, 2001, 288 p.
  40. Natrup F., Graf W. Sherardizing: corrosion protection of steels by zinc diffusion coatings. Thermochemical Surface Engineering of Steels. Kopenhagen: DTU Library, 2015, pp. 737–750.
  41. Pistofidis N., Vourlias G., Chaliampalias D. et al. On the mechanism of formation of zinc pack coatings. Journal of Alloys and Compounds, 2006, vol. 407, pp. 221–225.
  42. Kania H., Sipa J. Microstructure Characterization and Corrosion Resistance of Zinc Coating Obtained on High-Strength Grade 10.9 Bolts Using a New Thermal Diffusion Process. Materials, 2019, vol. 12, p. 1400.
  43. Kania H., Sipa J. Thermal diffusion zinc coating technology with reactive atmosphere recirculation. Part 1: General description of technology and structure of coatings. Ochrona Przed Korozja, 2018, vol. 11, pp. 338–345.
  44. Kania H., Sipa J. Zinc coating deposition with new thermal diffusion process on low carbon steel substrates. Wiadomosci Hutnicze, 2019, vol. 1, pp. 2–8.
  45. Kania H., Sipa J., Skupińska A. Thermal diffusion zinc coating technology with reactive atmosphere recirculation. Part 2: Corrosion resistance of coatings. Ochrona Przed Korozja, 2018, vol. 12, pp. 375–382.
  46. Lin Z., Xu L., Li X. et al. Corrosion resistance of composite coating used for fastener protection. Anti-Corrosion Methods and Materials, 2019, vol. 66, pp. 595–602.
  47. Schubert E., Klassen M., Zerner I. et al. Light-weight structures produced by laser beam joining for future applications in automobile and aerospace industry. Journal of Materials Processing Technology, 2001, vol. 115, pp. 2–8.