Application trends of high temperature refractory oxides for solid oxides fuel cells

Balinova Yu.A., Lugovoy A.A., Butakov V.V.
Balinova Yu.A., Lugovoy A.A., Butakov V.V. Application trends of high temperature refractory oxides for solid oxides fuel cells // Proceedings of VIAM. 2024. No. 8. DOI: 10.18577/2307-6046-2024-0-8-48-63. URL: https://www.viam-works.ru/en/journal/2024/8/5
Keywords
solid oxide fuel cells, conductivity, power density, oxide, cathode, anode, electrolyte, structure
Abstract

Solid oxide fuel cells attract the attention of developers due to their high energy efficiency, environmental friendliness and a wide variety of types of fuel used. The publication is devoted to the current state of the issue in the field of materials development for solid oxide fuel cells (SOFC). Ceramic oxide materials used for the anode, cathode and electrode of fuel cells are considered. It is shown that interest in solid oxide fuel cells will steadily grow, while small-sized SOFC up to nanoelements will have a special perspective.

Reference list
  1. Kuterbekov K.A., Nikonov A.V., Bekmyrza K.Zh. et al. Classification of Solid Oxide Fuel Cells Nanomaterials, 2022, no. 12, р. 1059. DOI: 10.3390/nano12071059.
  2. Jaiswal N., Tanwar K., Suman R. et al. A brief review on ceria based solid electrolytes for solid oxide fuel cells Journal of Alloys and Compounds, 2019, vol. 781, pp. 984–1005. DOI: 10.1016/j.jallcom.2018.12.015.
  3. Zhang W., Hu Y.H. Progress in proton-conducting oxides as electrolytes for low-temperature solid oxide fuel cells: From materials to devices Energy Science and Engineering, 2021. DOI: 10.1002/ese3.886.
  4. Dwivedi S. Solid oxide fuel cell: Materials for anode, cathode and electrolyte International Journal of Hydrogen Energy, 2020, vol. 45, no. 44, pp. 23988–24013. DOI: 10.1016/j.ijhydene.2019.11.234.
  5. Zavorotnaya U.M., Ponomarev I.I., Volkov Yu.A., Sinitsyn V.V. Development of high-performance hydrogen-air fuel cell with flourine-free sulfonated co-polynaphthoyleneimide membrane Membranes, 2023, vol. 13, p. 485. DOI: 10.3390/ membranes13050485.
  6. Hussain S., Yangping L. Review of solid oxide fuel cell materials: cathode, anode, and electrolyte Energy Transitions, 2020, vol. 4, pp. 113–126. DOI: 10.1007/s41825-020-00029-8.
  7. Kim J., Kim J., Yoon K.J. et al. Solid oxide fuel cells with zirconia/ceria bilayer electrolytes via roll calendering process Journal of Alloys and Compounds. 2020, vol. 846, art. 156318. DOI: 10.1016/j.jallcom.2020.156318.
  8. Fan L., Zhu B., Su P.-Ch., He Ch. Nanomaterials and technologies for low temperature solid oxide fuel cells: Recent advances, challenges and opportunities Nano Energy, 2018, vol. 45, pp. 148–176. DOI: 10.1016/j.nanoen.2017.12.044.
  9. Li J., Lu Y., Mushtaq N. et al. Analyzing the composite heterostructure as an efficient electrolyte for low-temperature ceramic fuel cells Journal of Alloys and Compounds, 2024, vol. 980, art. 173597. DOI: 10.1016/j.jallcom.2024.173597.
  10. Sun Ch., Hui R., Roller J. Cathode materials for solid oxide fuel cells: a review Journal of Solid State Electrochemistry, 2010, vol. 14, pp. 1125–1144. DOI: 10.1007/s10008-009-0932-0.
  11. Trofimenko N.E., Ullmann H. Oxygen stoichiometry and mixed ionic-electronic conductivity of Sr1‒aCeaFe1‒bCobO3‒x perovskite-type oxides Journal of the European Ceramic Society, 2000, vol. 20, pp. 1241–1250.
  12. Zhi M., Lee S., Miller N. et al. An intermediate-temperature solid oxide fuel cell with electrospun nanofber cathode Energy and Environmental Science, 2012, no. 5, pp. 7066–7071. DOI: 10.1039/C2EE02619H.
  13. Agarkov D.A., Bredikhin S.I. Solid oxide fuel cells (SOFC) and power plants based on them Energoekspert, 2021, no. 3, pp. 6–8.
  14. Lyskov N.V., Kotova A.I., Petukhov D.I. et al. A new electrochemically active and stable electrode based on praseodymium molybdate for symmetric SOFCs Elektrokhimiya, 2022, vol. 58, no. 11, pp. 746–755. DOI: 10.31857/S0424857022110093.
  15. Composite electrode material for electrochemical devices: pat. 2523550 Rus. Federation; appl. 22.03.13; publ. 20.07.14.
  16. Gallyamov A.N., Kazantsev A.L., Skovorodnikov P.V., Poilov V.Z. Review of modern functional materials used in solid oxide fuel cells operating on hydrogen fuel Vestnik PNI PU. Ser.: Khimicheskaya tekhnologiya i biotekhnologiya, 2022, no. 4, pp. 38–61. DOI: 10.15593/2224-9400/2022.4.04.
  17. Lomonova E.E., Kulebyakin A.V., Tabachkova N.Yu. Solid electrolytes for solid oxide fuel cells (SOFC). Available at: https://econobninsk.ru/images/prezentatsii/ИОФ_РАН_МИСИС_Ломонова_Табачкова_Твёрдые_электролиты_для_ТОТЭ_Обнинск_09-09-2021.pdf (accessed: April 19, 2024).
  18. Kolchina L.M. Synthesis and high-temperature properties of multicomponent cuprates – promising cathode materials for solid oxide fuel cells: thesis, Cand. Sc. (Chem.). Moscow, 2017, 134 p.
  19. Morales M., Segarra M. Materials Issues for Solid Oxide Fuel Cells Design Handbook of Clean Energy Systems. John Wiley & Sons, Ltd., 2015, pp. 1–17. DOI: 10.1002/9781118991978.hces190.
  20. Method for producing anode substrates with a developed microstructure used in multichannel SOFCs: pat. 2777101 Rus. Federation; appl. 29.12.21; publ. 01.08.22.
  21. Soloviev A.A., Sochugov N.S., Ionov I.V., Shipilova A.V., Kovalchuk A.N. Magnetron formation of Ni‒YSZ anodes of solid oxide fuel cells Elektrokhimiya, 2014, vol. 50, no. 7, pp. 724–732. DOI: 10.7868/S0424857014070160.
  22. Agarkova E.A., Zadorozhnaya O.Yu., Burmistrov I.N. et al. Fabrication and electrochemical characteristics of SOFCs based on supporting two-layer anode substrates obtained by casting on a moving belt Elektrokhimiya, 2022, vol. 58, no. 2, pp. 76–84. DOI: 10.31857/S0424857022020037.
  23. Simonenko T.L. Synthesis and study of solid electrolytes based on ZrO2, CeO2 and BaCe(Zr)O3 doped with magnesium, yttrium and gadolinium oxides: thesis, Cand. Sc. (Thech.). St. Petersburg, 2018, 160 p.
  24. Affandi N.S.M., Osman N. Short review on global trends in SOFC scenario and future perspective Materials Today: Proceedings, 2022, vol. 66 (10), pp. 3981–3984. DOI: 10.1016/j.matpr.2022.04.824.
  25. Global Solid Oxide Fuel Cell Market Share, Size, Growth, Trends, Analysis, Forecast: By Type: Planar, Tubular; By Application: Portable, Stationary, Transport; By End User: Residential, Commercial and Industrial, Data Centres, Military and Defence; Regional Analysis; Competitive Landscape; Key Trends and Developments in the Market; 2024–2032. Available at: https://markwideresearch.com/solid-oxide-fuel-cell-market/ (accessed: March 26, 2024).
  26. Batista R.M., Ferreira A.M.D.C., Muccillo E.N.S. Sintering and electrical conductivity of gadolinia-doped ceria Ionics, 2016, vol. 22, pp. 1159–1166. DOI: 10.1007/s11581-016-1648-7.
  27. Solovyev A.A., Rabotkin S.V., Shipilova A.V., Ionov I.V. Magnetron Sputtering of Gadolinium-doped Ceria Electrolyte for Intermediate Temperature Solid Oxide Fuel Cells International Journal of Electrochemical Science, 2019, vol. 14, pp. 575–584. DOI: 10.20964/2019.01.03.
  28. Agarkov D.A. Study of the relationship between microstructure and charge transfer processes in composite electrodes of SOFCs of planar geometry: Thesis, Cand. Sc. (Phys. & Math.). Chernogolovka, 2016, 171 p.
  29. Agarkov D., Borik M., Komarov B. et al. Long-Term Conductivity Stability of Electrolytic Membranes of Scandia Stabilized Zirconia Co-Doped with Ytterbia Membranes, 2023, vol. 13, p. 586. DOI: 10.3390/membranes13060586.
  30. Kablov E.N., Antipov V.V. The Role of New Generation Materials in Ensuring the Technological Sovereignty of the Russian Federation Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  31. Sokolov A.V., Deynega G.I., Kuzmina N.A. Influence of Sc2O3 additive on sintering temperature and properties of ZrO2–Y2O3 system oxide ceramics. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 64–69. DOI: 10.18577/2071-9140-2020-0-1-64-69.
  32. Doronin O.N., Artemenko N.I., Stekhov P.A., Voronov V.A. Deposition of ceramic layers of heat protection coatings based on the system Gd2O3–ZrO2–HfO2 and Sm2O3–Y2O3–HfO2. Aviation materials and technologies, 2022, no. 3 (68), paper no. 10. Available at: http://www.journal.viam.ru (accessed: March 26, 2024). DOI: 10.18577/2713-0193-2022-0-3-108-119.
  33. Lebedeva Yu.E., Shchegoleva N.E., Voronov V.A., Solntcev S.S. Al2O3 and ZrO2 ceramic materials obtained by sol-gel method. Trudy VIAM, 2021, no. 4 (98), paper no. 05. Available at: http://www.viam-works.ru (accessed: March 26, 2024). DOI: 10.18577/2307-6046-2021-0-4-61-73.
  34. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.