Investigation of the effect of components on the properties of sealing harness material for autoclave molding of polymer composite materials

Evdokimov A.A., Gerasimov D.M., Vakhrusheva Ja.A., Venediktova M.A., Bogdan L.M.
Evdokimov A.A., Gerasimov D.M., Vakhrusheva Ja.A., Venediktova M.A., Bogdan L.M. Investigation of the effect of components on the properties of sealing harness material for autoclave molding of polymer composite materials // Proceedings of VIAM. 2024. No. 8. DOI: 10.18577/2307-6046-2024-0-8-19-27. URL: https://www.viam-works.ru/en/journal/2024/8/2
Keywords
sealing harness, elastomeric material, ingredients, dimethylvinylsiloxane rubber, autoclave forming
Abstract

The results of studies of the optimal component composition of the sealing  harness material and the assessment of the effect of each component on the physico-mechanical characteristics of the resulting mixtures are described. Compositions based on dimethylvinylsiloxane rubber with ingredients such as covelos, carbon black and diatomite,chalk, BMK-5 copolymer and TMFT product, dicumyl peroxide are considered. Based on the conducted studies of experimental compositions, the ingredients most applicable for further  development of the optimal formulation of the sealing material used in autoclave molding have been determined.

Reference list
  1. Mikhailin Yu.A. Heat-resistant polymers and polymeric materials based on them. Polimernye materialy, 2005, no. 8, pp. 23–26.
  2. Evdokimov A.A. Polymer composite material manufactured using vacuum infusion technology with shaping at temperatures up to 40 °C: thesis, Cand. Sc. (Tech.). Moscow, 2020, 116 p.
  3. Valueva M.I., Zelenina I.V., Nacharkina A.V., Ahmadieva K.R. Technological features of obtaining high temperature polyimide carbons. Foreign experience (review). Trudy VIAM, 2022, no. 6 (112), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 16, 2024). DOI: 10.18577/2307-6046-2022-0-6-80-95.
  4. CYCOM 2237 Polyimide Resin System. Technical Data Sheet. Available at: https://www.solvay.com/en/product/cycom-2237 (accessed: February 15, 2024).
  5. Valueva M.I., Zelenina I.V., Zharinov M.A., Akhmadieva K.R. World market of high temperature polyimide carbon plastic (review). Trudy VIAM, 2019, no. 12 (84), paper no. 08. Available at: http://www.viam-works.ru (accessed: February 16, 2024). DOI: 10.18577/2307-6046-2019-0-12-67-69.
  6. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  7. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), paper no. 03. Available at: https://journal.viam.ru (accessed: February 15, 2024). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  8. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  9. Kablov E.N. The role of chemistry in the creation of new generation materials for complex technical systems. Reports of the XX Mendeleev Congress on General and Applied Chemistry. Ekaterinburg: Ural Branch of the Russian Academy of Sciences, 2016, pp. 25–26.
  10. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916.
  11. Chaykun A.M., Bobrova I.I., Gerasimov D.M., Sergeyev A.V. Elastomers for sealing harness materials: properties, methods of receiving and feature of manufacturing. Trudy VIAM, 2023, no. 7 (125), paper no. 05. Available at: http://www.viam-works.ru (accessed: February 16, 2024). DOI: 10.18577/2307-6046-2023-0-7-56-68.
  12. Schetz M. Silicone rubber. Moscow: Khimiya, 1975, 400 p.
  13. Dolgov O. N., Voronkov M.G., Grinblat M.P. Organosilicon liquid rubbers and materials based on them. Leningrad: Khimiya, 1975, 112 p.
  14. The big handbook of the rubber manufacturer: in 2 parts. Edы. S.V. Reznicenko, Yu.L. Morozov. Moscow: Tekhinform, 2012, part 1, 2, 1385 p.
  15. Rubber and resin. Science and technology: trans. from Engl. Eds. A.A. Berlin and Yu.L. Morozov. Dolgoprudny: Intellect, 2011, 768 p.
  16. Kornev A.E., Bukanov A.M., Sheverdyaev O.N. Technology of elastomer materials. Moscow: Istek, 2009, 502 p.
  17. Hoffman V. Vulcanization and vulcanizing agents. Leningrad: Khimiya, 1968, 464 p.
  18. Rubber technology: formulation and testing: trans. from Engl. Ed. J.S. Dik. St. Petersburg: Scientific foundations and technologies, 2010, 620 p.
  19. Agayants I.M. Five centuries of rubber and rubber. Moscow: Modern-A, 2002, 432 p.