Properties and purpose of film adhesives (constructional and foaming) with lowered combustibility

Isaev A.Yu., Rubtsova E.V., Lukina N.F.
Isaev A.Yu., Rubtsova E.V., Lukina N.F. Properties and purpose of film adhesives (constructional and foaming) with lowered combustibility // Proceedings of VIAM. 2024. No. 6. DOI: 10.18577/2307-6046-2024-0-6-42-50. URL: https://www.viam-works.ru/en/journal/2024/6/4
Keywords
constructional film adhesive, foaming film adhesive, adhesive joints, lap shear strength, honeycomb sandwich strength, heat resistance, curing mode, adhesive with lowered combustibility
Abstract

Theresults of research of the properties of epoxy film adhesiveswith lowered combustibility and heat resistance up to 120 °C – VK-108 and VKV-28 are presented. VK-108 structural adhesive is intended for gluing parts and units from metal materials and polymeric composite materials, including honeycomb sandwich constructions.  VKV-28 foaming adhesive is designed to connect the cellular fillers with each other and with the frame elements in honeycomb sandwich  made from aluminum alloys and polymeric composite materials. Аdhesivesare self-extinguishing and meet the requirements of AP-25 (Appendix F, Рart I).

Reference list
  1. Kablov E.N. The main directions of the development of materials for the Authoric technique of the XXI century. Perspektivnyye materialy, 2000, no. 3, pp. 27–36.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N. The role of fundamental research in the creation of materials of the new generation. XXI Mendeleevsky Congress for General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  4. Kablov E.N., Minakov V.T., Anikhovskaya L.I. Glues and materials based on them for repairing structures of aviation equipment. Aviatsionnye materialy i tekhnologii, 2002, no. 1, pp. 61–65.
  5. Grashhenkov D.V., Chursova L.V. Strategy of development of composite and functional materials. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 231–242.
  6. Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
  7. Petrova A.P. The main stages of gluing technology. Klei. Germetiki. Tekhnologii, 2014, no. 2, pp. 24–30.
  8. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: March 21, 2024). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  9. Aviation materials: a guide of 13 vols. Ed. E.N. Kablov. 7th ed., add. and rev. Moscow: VIAM, 2019, vol. 10: Adhesives, sealants, rubber, hydraulic fluidity, part 1: Adhesives, glue prepares, 276 p.
  10. Petrova A.P., Malysheva G.V. Adhesives, adhesive binding and adhesive prepares: textbook. Ed. E.N. Kablov. Moscow: VIAM, 2017, 472 p.
  11. Petrova A.P., Donskoy A.A. Adhesive materials. Sealants. St. Petersburg: Professional, 2008, 589 p.
  12. Shershak P.V., Yakovlev N.O., Shokin G.I., Kutsevich K.E., Popkova E.A. Evaluation method and factors influencing the bonding quality between face and honey-comb cores in floor and interior aircraft panels. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 81–88. DOI: 10.18577/2071-9140-2020-0-2-81-88.
  13. Petrova A.P. Foaming adhesives and their use in aircraft construction. Klei. Germetiki. Tekhnologii, 2015, no. 1, pp. 2–5.
  14. Kutsevich K.E., Tyumeneva T.Yu., Petrova A.P. Influence of fillers on properties of adhesive prepregs and PCM on their basis. Aviacionnye materialy i tehnologii, 2017, no. 4 (49), pp. 51–55. DOI: 10.18577/2071-9140-2017-0-4-51-55.
  15. Dementyeva L.A., Tyumeneva T.Yu., Sharova I.A. Adhesives with reduced flammability for aircraft. Tr. VI Int. conf. Vologda, 2011, pp. 127–128.
  16. Zastrogina O.B., Shvets N.I., Serkova U.A., Veshkin E.A. Fireproof materials based on phenol-formaldehyde binders. Klei. Germetiki. Tekhnologii, 2017, no. 7, pp. 22–27.
  17. Zastrogina O.B., Serkova E.А., Sarychev I.A., Vavilova M.I. Influence of Russian and Chinese vinyflex on the properties of the VFT binder and fiberglass based on it. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 3–9. DOI: 10.18577/2071-9140-2020-0-3-3-9.
  18. Donskoy A.A., Baritko N.V. Self-extinguishing low-density sealants. Klei. Germetiki. Tekhnologii, 2006, no. 9, pp. 10–12.
  19. Kurshubadze I.V., Petrova A.P. Performance of adhesive joints in marine subtropical conditions. Klei. Germetiki. Tekhnologii, 2005, no. 12, pp. 14–17.
  20. Lukina N.F., Isaev A.Yu., Starodubtseva О.А., Balabanovа О.S. Approaches to creation of conducting glue from the lowered curing temperature. Trudy VIAM, 2023, no. 5 (123), paper no. 05. Available at: http://www.viam-works.ru (accessed: May 01, 2024). DOI: 10.18577/2307-6046-2023-0-5-54-63.
  21. Petrova A.P., Lukina N.F., Isaev A.Yu., Smirnov O.I. The effect of the adhesive primer EP-0234 on the properties of adhesive compounds obtained using adhesive VK-36. Trudy VIAM, 2022, no. 6 (112), paper no. 04. Available at: http://www.viam-works.ru (accessed: March 21, 2024). DOI: 10.18577/2307-6046-2022-0-6-39-48.
  22. Lukina N.F., Kotova Е.V., Petrova A.P., Isaev A.Yu. Improvement of properties of fenolformaldegidny adhesives when updating by their polyvinylacetals. Trudy VIAM, 2022, no. 6 (112), paper no. 03. Available at: http://www.viam-works.ru (accessed: March 21, 2024). DOI: 10.18577/2307-6046-2022-0-7-27-36.