Light sources for simulating the aging of polymer materials under the influence of solar radiation

Laptev A.B., Pavlov M.R., Zeleneva T.O.
Laptev A.B., Pavlov M.R., Zeleneva T.O. Light sources for simulating the aging of polymer materials under the influence of solar radiation // Proceedings of VIAM. 2024. No. 5. DOI: 10.18577/2307-6046-2024-0-5-71-82. URL: https://www.viam-works.ru/en/journal/2024/5/7
Keywords
ultraviolet radiation, polymer aging, ultraviolet frequency, source of ultraviolet, photolysis
Abstract

A step-by-step analysis of the ultraviolet spectrum was carried out. It is shown that UV-B and UV-C light are present on the Earth's surface in small doses. UV-A light on the Earth's surface has significant doses leading to photolysis and destruction of heteroorganic polymers. In order to conduct research by simulating light aging, it is necessary to simulate solar radiation in the range from 290 nm (UV-B) with a set of LED radiation sources that fully correspond to the spectral composition and power of Sunlight on the Earth's surface.

Reference list
  1. Kablov E.N., Laptev A.B., Prokopenko A.N., Gulyaev A.I. Relaxation of polymeric composite materials under the prolonged action of static load and climate (review). Part 1. Binders. Aviation materials and technologies, 2021, no. 4 (65), paper no. 08. Available at: http://www.journal.viam.ru (accessed: November 20, 2023). DOI: 10.18577/2071-9140-2021-0-4-70-80.
  2. Kablov E.N. New generation materials and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  3. Kablov E.N., Kondrashov S.V., Melnikov A.A., Schur P.A. Application of functional and adaptive materials obtained by 3D printing (review). Trudy VIAM, 2022, no. 2 (108), paper no. 03. Available at: http://www.viam-works.ru (accessed: November 20, 2023). DOI: 10.18577/2307-6046-2022-0-2-32-51.
  4. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climate factors (review). Part 1. Testing of new materials. Trudy VIAM, 2021, no. 1 (95), paper no. 12. Available at: http://www.viam-works.ru (accessed: November 20, 2023). DOI: 10.18577/2307-6046-2021-0-1-114-122.
  5. Laptev A.B., Pavlov M.R., Novikov A.A., Slavin A.V. Current trends in the development of testing materials for resistance to climatic factors (review). Part 2. Main trends. Trudy VIAM, 2021, no. 2 (96), paper no. 11. Available at: http://www.viam-works.ru (accessed: November 20, 2023). DOI: 10.18577/2307-6046-2021-0-2-99-108.
  6. Vitale V., Petkov B.H., Goutail F. Variations of UV irradiance at Antarctic station Concordia during the springs of 2008 and 2009. Antarctic Science, 2011, vol. 23 (04), pp. 389–398. DOI: 10.1017/S0954102011000228.
  7. Hoisington R.D., Whiteside M., Herndon J.M. Unequivocal Detection of Solar Ultraviolet Radiation 250–300 nm (UV-C) at Earth’s Surface. European Journal of Applied Sciences, 2023, vol. 11 (2), pp. 455–472.
  8. Herndon J.M., Hoisington R.D., Whiteside M. Deadly Ultraviolet UV-C and UV-B Penetration to Earth’s Surface: Human and Environmental Health Implications. Journal of Geography, Environment and Earth Science International, 2018, vol. 14 (2), pp. 1–11.
  9. Chesnokova T.Yu., Voronina Yu.V., Chentsov A.V. et al. Calculation of solar radiation fluxes in the UV range with different absorption cross sections of ozone and nitrogen dioxide. Matematicheskaya fizika i kompyuternoe modelirovanie, 2017, vol. 20, no. 5, pp. 76–88.
  10. Cárcer I.A., Dantoni H.L., Barboza-Flores M. KCl: Eu2+ as a solar UV-C radiation dosimeter. Optically stimulated luminescence and thermoluminescence analyses. Journal of Rare Earths, 2009, vol. 27 (4), pp. 579–583.
  11. D'Antoni H. Extreme environments in the forests of Ushuaia, Argentina. Geophysical Research Letters, 2007, vol. 34 (22), pp. 95–120.
  12. D'Antoni H.L., Rothschild L.J., Skiles J. Reply to comment by Stephan D. Flint et al. on «Extreme environments in the forests of Ushuaia, Argentina». Geophysical Research Letters, 2008, vol. 35 (13), pp. 574–581.
  13. Ceballos G., Ehrlich P.R., Dirzo R. Biological annihilation via the ongoing sixth mass extinction signaled by vertebrate population losses and declines. Proceedings of the National Academy of Sciences, 2017, vol. 114 (30), pp. 6089–6096.
  14. Living Planet Report 2020: Bending the Curve of Biodiversity Loss. Gland: WWF, 2020, 25 p.
  15. Dirzo R. Defaunation in the Anthropocene. Science, 2014, vol. 345 (6195), pp. 401–406.
  16. Herndon J.M., Williams D.D., Whiteside M. Previously unrecognized primary factors in the demise of endangered torrey pines: A microcosm of global forest die-offs. Journal of Geography, Environmental and Earth Science International, 2018, vol. 16 (4), pp. 1–14.
  17. Zong Y. Simple spectral stray light correction method for array spectroradiometers. Applied optics, 2006, vol. 45 (6), pp. 1111–1119.
  18. Ravanat J.-L., Douki T. UV and ionizing radiations induced DNA damage, differences and similarities. Radiation Physics and Chemistry, 2016, vol. 128, pp. 92–102.
  19. Meftah M., Damé L., Bolsée D. SOLAR-ISS: A new reference spectrum based on SOLAR/SOLSPEC observations? Astronomy Astrophysics, 2018, vol. 611, pp. 33–38. DOI: 10.1051/0004-6361/201731316.
  20. Herndon J.M., Whiteside M. Aerosolized coal fly ash particles, the main cause of stratospheric ozone depletion, not chlorofluorocarbon gases. European Journal of Applied Sciences, 2022, vol. 10 (3), pp. 586–603.
  21. Whiteside M., Herndon J.M. Destruction of stratospheric ozone: Role of aerosolized coal fly ash iron. European Journal of Applied Sciences, 2022, vol. 10 (4), pp. 143–153.
  22. Newman P.A., Oman L.D., Douglass A.R. et al. What would have happened to the ozone layer if chlorofluorocarbons (CFCs) had not been regulated? Atmosphere Chemical Physic, 2009, no. 9, pp. 2113–2128.
  23. Whiteside M., Herndon J.M. Humic like substances (HULIS): Contribution to global warming and stratospheric ozone depletion. European Journal of Applied Sciences, 2023, vol. 11 (2), pp. 325–346.
  24. Herndon J.M. Obtaining evidence of coal fly ash content in weather modification (geoengineering) through analyses of postaerosol spraying rainwater and solid substances. Indian Journal Science, Research and Technology, 2016, vol. 4(1), аrt. 30-6.
  25. Vechkanov E.M., Vnukov V.V. Thermodynamics and kinetics of biological processes: textbook for universities. Rostov-on-Don: Copy-Center, 2011, 53 p.
  26. Kablov E.N., Startsev V.O., Laptev A.B. Aging of polymer composite materials: textbook. Moscow: National Research Center «Kurchatov Institute» – VIAM, 2023, 520 p.
  27. Istamov F., Dadomatov X., Boboev T. Influence of tensile load on the kinetics of photodestruction of polymethyl methacrylate. Doklady Akademii nauk Respubliki Tadzhikistan, 2002, vol. 45, no. 10, pp. 76–80.
  28. Berlin A.A., Korolev G.V., Kefeli T.Ya., Severgin Yu.M. Acrylic oligomers and materials based on them. Moscow: Nauka, 1983, 320 p.
  29. UV-curing electrical insulating composition: pat. SU 1483495 A1; appl. 21.07.87; publ. 30.05.89.
  30. Semyannikov V.A. Study of light scattering of the process of formation of microheterogeneous structure of network polymers based on oligoester acrylates: thesis, Cand. Sc. (Chem.). Yaroslavl: Yaroslavl Polytech Institute, 1988, 134 p.
  31. Vasiliev D.K. Changes in UV spectra during photoinitiated polymerization of methacrylates: thesis, Cand. Sc. (Chem.). Yaroslavl: Yaroslavl Polytech Institute, 1990, 125 p.
  32. Tofa M., Djafar Z., Piarah W.H. A New Hybrid of Photovoltaic-thermoelectric Generator with Hot Mirror as Spectrum Splitter. Journal of Physical Science, 2018, vol. 29 (Supp. 2), pp. 63–75. DOI: 10.21315/jps2018.29.s2.6.
  33. Magdalena V., Linyu G., Feng J. LED-based solar simulator to study photochemistry over a wide temperature range in the large simulation chamber AIDA. Atmospheric measurement technology, 2022, vol. 15, pp. 1795–1810.