Application of epoxy compositions in the development of asphalt concrete coatings
Zagora A.G., Tkachuk A.I., Mukhametov R.R., Eldjaeva G.B. Application of epoxy compositions in the development of asphalt concrete coatings // Proceedings of VIAM. 2024. No. 2. DOI: 10.18577/2307-6046-2024-0-2-34-48. URL: https://www.viam-works.ru/en/journal/2024/2/4
Keywords
epoxy asphalt, polymer bitumen binders, epoxy asphalt concrete coatings, epoxy resins
Abstract
This work is devoted to a review of researches and developments related to the modification of asphalt concrete mixtures with various types of epoxy resins and hardeners. The development of the world economy is impossible without the use of new technologies in the construction of roads and bridges. One of the most effective options for modifying traditional asphalt concrete road pavements is the introduction of epoxy compositions into the bitumen composition. The main result of using epoxy asphalt is a noticeable increase in physical and mechanical characteristics and moisture resistance compared to a conventional asphalt.
Reference list
- Zakieva R.R., Gussamov I.I., Gadelshin R.M. et al. The influence of modification with a copolymer of ethylene with vinyl acetate on the performance properties of binders and asphalt concrete based on it. Khimiya i tekhnologiya topliv i masel, 2015, no. 5 (591), pp. 36–39.
- Fang C., Zhou S., Zhang M. et al. Optimization of the modification technologies of asphalt by using waste EVA from packaging. Journal of Vinyl and Additive Technology, 2009, no. 15, pp. 199–203. DOI: 10.1002/vnl.20189.
- Upadhyay S., Mallikarjunan V., Subbaraj V., Varughese S. Swelling and diffusion characteristics of polar and nonpolar polymers in asphalt. Journal of Applied Polymer Science, 2008, no. 109, pp. 135–143. DOI: 10.1002/app.27764.
- Khakimullin Yu.N., Ayupov D.A., Sundukov V.I. et al. Non-separating three-component polymer-bitumen binders. Stroitelnye materialy, 2017, no. 10, pp. 51–55.
- Belyaev P.S., Polushkin D.L., Makeev P.V., Frolov V.A. Modification of petroleum road bitumen with polymer materials to obtain asphalt concrete pavements with increased performance characteristics. Vestnik Tambovskogo gosudarstvennogo tekhnicheskogo universiteta, 2016, no. 22. pp. 264–271.
- Yang F., Gong H., Cong L. et al. Investigating on polymerization process and interaction mechanism of thermosetting polyurethane modified asphalt. Construction and Building Materials, 2022, no. 335. DOI: 10.2139/ssrn.4008099.
- Kuznetcova P.A., Tkachuk A.I., Lyubimova A.S., Eldjaeva G.B. Characteristics of the molten epoxy resin system VSE-62, processed by the injection methods, for the manufacture of highly loaded structural polymer composite materials. Trudy VIAM, 2023, no. 5 (123), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2023-0-5-43-53.
- Mukhametov R.R., Petrova A.P. Properties of epoxy polymer binders and their processing into polymer composite materials. Novosti materialovedeniya. Nauka i tekhnika, 2018, no. 3–4 (30), art. 06. Available at: http://www.materialsnews.ru (accessed: November 08, 2023).
- Zagora A.G., Tkachuk A.I., Terekhov I.V., Mukhametov R.R. Methods of chemical modification of epoxy oligomers (review). Trudy VIAM, 2021, no. 7 (101), paper no. 08. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2021-0-7-73-85.
- Inorganic cement-epoxy resin composition containing animal glue: рat. 3198758 US; appl. 05.12.1961; publ. 03.08.1965.
- Luo S., Qian Z., Wang H. Condition survey and analysis of epoxy asphalt concrete pavement on Second Nanjing Yangtze River Bridge: A ten-year review. Journal of Southeast University (English Edition), 2011, no. 27 (4), pp. 417–422. DOI: 10.3969/j.issn.1003 7985.2011.04.014.
- Han Y., Zhang Z., Tian J., Ni F. Long-Term In Situ Performance Evaluation of Epoxy Asphalt Concrete for Long-Span Steel Bridge Deck Pavement. Coatings, 2023, no. 13 (3), pp. 545. DOI: 10.3390/coatings13030545.
- Ma B., Zhou X., Wei K. Preparation and properties evaluation of shape memory epoxy asphalt composites with high toughness and damping. Applied Sciences, 2017, no. 7, p. 523.
- Pokrovsky A.V. Cast asphalt concrete and bridge systems in China. Dorogi. Innovatsii v stroitelstve, 2019, no. 77, pp. 84–89.
- Yao B., Chen C., Loh K. Performance characteristics of diluted epoxy asphalt binders and their potential application in chip seal. Journal of Materials in Civil Engineering, 2019, no. 31 (12). DOI: 10.1061/(ASCE)MT.1943-5533.0002943.
- Liu Y., Wang S. Research Progress of Epoxy Asphalt Material for Roads. Journal of World Architecture, 2023, no. 7. DOI: 10.26689/jwa.v7i3.4854.
- Chen Y., Hossiney N., Yang X. et al. Application of Epoxy-Asphalt Composite in Asphalt Paving Industry: A Review with Emphasis on Physicochemical Properties and Pavement Performances. Advances in Materials Science and Engineering, 2021, no. 1, pp. 1–35. DOI: 10.1155/2021/3454029.
- Kang Y., Wu Q., Jin R. et al. Rubber-like quasi-thermosetting polyetheramine-cured epoxy asphalt composites capable of being opened to traffic immediately. Scientific Reports, 2016, no. 6. DOI: 10.1038/srep18882.
- Song M., Liang R., Deng J., Kang Y. Sealed accelerants facilitate epoxy asphalt concretes opening to traffic quickly. Construction and Building Materials, 2017, no. 147, pp. 1–8.
- Turonchik S.A. Modification of asphalt concrete using epoxy resin. Road construction and its engineering support: III Int. conf. Minsk, 2022, pp. 358–362.
- Ayupov D.A., Potapova L.I., Murafa A.V., Fakhrutdinova V.Kh., Khakimullin Yu.N., Khozin V.G. Study of the features of the interaction of bitumen with polymers. Izvestia KGASU, 2011, no. 1 (15), pp. 140–146.
- Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2020-0-1-68-77.
- Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
- Kablov E.N. New Generation Materials and Technologies for Their Digital Processing. Herald of the Russian Academy of Sciences, 2020, no. 90, pp. 225–228.
- Kolobkov A.S. Polymer composite materials for various aircraft structures (review). Trudy VIAM, 2020, no. 6–7 (89), paper no. 05. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2020-0-67-38-44.
- Su W., Han X., Gong J. et al. Toughening epoxy asphalt binder using core-shell rubber nanoparticles. Construction and Building Materials, 2020, no. 258 (12). DOI: 10.1016/j.conbuildmat.2020.119716.
- Tkachuk A.I., Lyubimova A.S., Kuznetcova P.A. Opportunities of the development of plant-based epoxy resins (review). Trudy VIAM, 2022, no. 8 (114), paper no. 04. Available at: http://www.viam-works.ru (accessed: November 08, 2023). DOI: 10.18577/2307-6046-2022-0-8-49-64.
- Si J., Li Y., Wang J. et al. Improving the compatibility of cold-mixed epoxy asphalt based on the epoxidized soybean oil. Construction and Building Materials, 2020, no. 243. DOI: 10.1016/j.conbuildmat.2020.118235.
- Al Fuhaid A.F. Biobased Epoxy Asphalt Binder (BEAB) for Pavement Asphalt Mixtures Mixtures // USF Tampa Graduate Theses and Dissertations. 2018. Available at: https://digitalcommons.usf.edu/etd/7599 (accessed: November 08, 2023).
- Huang M., Wen X., Wang L. Influence of foaming effect, operation time and health preserving properties of foam epoxy asphalt mixtures. Construction and Building Materials, 2017, no. 151, pp. 931–938. DOI: 10.1016/j.conbuildmat.2017.06.083.
- Yu X., Dong F., Ding G. et al. Rheological and microstructural properties of foamed epoxy asphalt. Construction and Building Materials, 2016, no. 114, pp. 215–222. DOI: 10.1016/j.conbuildmat.2016.03.179.
- Cong P., Liu N., Shang H., Zhao H. Rheological and fatigue properties of epoxy asphalt binder. International Journal of Pavement Research and Technology, 2015, no. 8 (5), pp. 370–376. DOI: 10.6135/ijprt.org.tw/2015.8(5).370.
- Moraes R. Evaluation of Epoxy Asphalt Binders for Open-Graded Friction Course (OGFC) Application. RILEM. Bituminous Materials: Proceedings of the International Symposium, 2022, pp. 787–794. DOI: 10.1007/978-3-030-46455-4_100.
- Sun Y., Han X., Su W., Gong J. Mechanical and bonding properties of pristine montmorillonite reinforced epoxy asphalt bond coats. Polymer Composites, 2020, no. 41 (8). DOI: 10.1002/pc.25595.
- Bahmani H., Sanij K.H., Peiravian F. Estimating moisture resistance of asphalt mixture containing epoxy resin using surface free energy method and modified Lottman test. International Journal of Pavement Engineering, 2021, no. 23 (2), pp. 1–13. DOI: 10.1080/10298436.2021.1904236.
- Sun Y., Gong J., Liu Y. et al. Viscous, damping, and mechanical properties of epoxy asphalt adhesives containing different penetration-grade asphalts. Journal of Applied Polymer Science, 2019, no. 136 (5). DOI: 10.1002/app.47027.
- Jamshidi A., White G., Kurumisawa K. Rheological Characteristics of Epoxy Asphalt Binders and Engineering Properties of Epoxy Asphalt Mixtures-State-of-the-Art. Road Materials and Pavement Design, 2022, no. 23 (9), pp. 1957–1980. DOI: 10.1080/14680629.2021.1963814.
- Cai X., Huang W., Liang J., Wu K. Study of Pavement Performance of Thin-Coat Waterborne Epoxy Emulsified Asphalt Mixture. Frontiers in materials, 2020, no. 7, p. 88. DOI: 10.3389/fmats.2020.00088.
- Yu D. Study on Waterborne Epoxy Resin Modified Emulsified Asphalt and the Performance of Mixture: Master’s thesis. Chongqing Jiaotong University, 2018, pp. 215–222.
- Yang G., Wang C., Fu H. et al. Waterborne epoxy resin–polyurethane–emulsified asphalt: preparation and properties. Journal of Materials in Civil Engineering, 2019, no. 31. DOI: 10.1061/(ASCE)MT.1943-5533.0002904.
- Chen R., Gong J., Jiang Y. et al. Halogen-free flame retarded cold-mix epoxy asphalt binders: rheological, thermal and mechanical characterization. Construction and Building Materials, 2018, no. 186, pp. 863–870. DOI: 10.1016/j. conbuildmat.2018.08.018.
- Hu C., Zhao J., Leng Z. et al. Laboratory evaluation of waterborne epoxy bitumen emulsion for pavement preventative maintenance application. Construction and Building Materials, 2019, no. 197, pp. 220–207. DOI: 10.1016/j.conbuildmat.2018.11.223.
- Liang H., Wang D., Wang G. et al. Numerical simulation and laboratory testing verification on the performance of an asphalt pavement seal coat with superficially permeating and solidifying properties. Journal of Testing and Evaluation, 2019, no. 47, pp. 4427–4451. DOI: 10.1520/JTE20170625.
- Gu Y., Tang B., He L. et al. Compatibility of cured phase-inversion waterborne epoxy resin emulsified asphalt. Construction and Building Materials, 2019, no. 229. DOI: 10.1016/j.conbuildmat.2019.116942.
- Thermoset modified additive for asphalt mixture, preparation method thereof and asphalt mixture: pat. 10030146B2 US; аppl. 23.05.14; рubl. 24.07.18.
- Asphalt composition comprising thermosetting reactive compounds: рat. 11059749B2 US; аppl. 04.06.18; рubl. 13.07.21.
- Waterborn polymer-modified emulsified asphalt mixture and process for producing the same: рat. 9982136B2 US, аppl. 11.08.15; рubl. 29.05.18.
- Jiang L., Hu K., Liu Z. et al. Aliphatic diamide as novel asphalt-modified epoxy curing agent for enhanced performance. Advances in Polymer Technology, 2018, no. 37, pp. 830–836. DOI: 10.1002/adv.21726.
- Wang X., Wu R., Zhang L. Development and performance evaluation of epoxy asphalt concrete modified with glass fibre. Road Materials and Pavement Design, 2019, no. 20, pp. 715–726. DOI: 10.1080/14680629.2017.1413006.