Determination of the causes of the formation of surface cracks in stamped parts made of low-carbon steels

Morozova L.V.
Morozova L.V. Determination of the causes of the formation of surface cracks in stamped parts made of low-carbon steels // Proceedings of VIAM. 2024. No. 11. DOI: 10.18577/2307-6046-2024-0-11-14-21. URL: https://www.viam-works.ru/en/journal/2024/11/2
Keywords
fractography, crack, steel, low-carbon steel, destruction
Abstract

A comprehensive study of parts made of low-carbon steel grades DC04 and DX54D was carried out in order to establish the causes of the formation of surface cracks using optical and electron microscopy, chemical analysis and metallography, the structure was assessed, the chemical composition, the structure of surface cracks and artificially obtained fractures of parts were studied. An X-ray spectral microanalysis of the surface of the opened cracks was carried out. A decrease in ductility due to contamination of the parts material with non-metallic inclusions has been established.

Reference list
  1. Steel and Alloy Brand Book. 4th ed., rev. and add. Ed. Yu.G. Dragunov, A.S. Zubchenko. Moscow: Mashinostroenie, 2014, 491 p.
  2. Novikov I.I., Zolotorevsky V.S., Portnoy K.K. et al. Metallurgy: textbook in 2 vols. Ed. V.S. Zolotorevsky. Moscow: Publ. House MISIS, 2009, vol. 1, 496 p.
  3. Novikov I.I., Zolotorevsky V.S., Portnoy K.K. et al. Metallurgy: textbook. in 2 vols. Ed. V.S. Zolotorevsky. Moscow: Publ. House MISIS, 2009, vol. 2, 528 p.
  4. Erasov V.S., Oreshko E.I., Lutsenko A.N. Multilevel large-scale complex research of deformation of metal materials. Aviation materials and technologies, 2022, no. 1 (66), paper no. 11. Available at: http://www.journal.viam.ru (accessed: June 07, 2024). DOI: 10.18577/2713-0193-2022-0-1-129-142.
  5. Gulyaev A.P. Metal Science: textbook for universities. 6th ed., rev. and add. Moscow: Metallurgiya, 1986, 544 p.
  6. Kablov E.N. Key Problem – Materials. Trends and Guidelines for Innovative Development of Russia. Moscow: VIAM, 2015, pp. 458–464.
  7. Kablov E.N., Bakradze M.M., Gromov V.I., Voznesenskaya N.M., Yakusheva N.A. New high strength structural and corrosion-resistant steels for aerospace equipment developed by FSUE «VIAM» (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 3–11. DOI: 10.18577/2071-9140-2020-0-1-3-11.
  8. Sevalnev G.S., Antsyferova M.V., Dulnev K.V., Sevalneva T.G., Vlasov I.I. Influence of nitrogen concentration on the structure and properties of sparingly alloyed structural steel. Aviacionnye materialy i tehnologii, 2020, no. 2 (59), pp. 10–16. DOI: 10.18577/2071-9140-2020-0-2-10-16.
  9. Bernstein M.L. Thermomechanical processing of metals and alloys: in 2 vols. Moscow: Metallurgiya, 1968, vol. 1, 596 p.
  10. Lednev I.S. Magnetic methods of non-destructive testing of aircraft parts. Aviation materials and technologies, 2024, no. 1 (74), paper no. 09. Available at: http://www.journal.viam.ru (accessed: June 07, 2024). DOI: 10.18577/2713-0193-2024-0-1-111-120.
  11. Oreshko E.I., Erasov V.S., Yakovlev N.O., Utkin D.A. Methods for determining the mechanical characteristics of materials using indentation (review). Aviation materials and technology, 2021, no. 1 (62), paper no. 10. Available at: http://www.journal.viam.ru (accessed: June 07, 2024). DOI: 10.18577/2713-0193-2021-0-1-104-118.
  12. Gordeeva T.A., Zhegina I.P. Analysis of fractures in assessing the reliability of materials. Moscow: Mashinostroenie, 1978, 200 p.
  13. Klevtsov G.V., Botvina L.R., Klevtsova N.A., Limar L.V. Fractal diagnostics of destruction of metal materials and structures. Moscow: MISIS, 2007, 259 p.
  14. Grigorenko V.B., Morozova L.V. Application of the scanning electron microscopy for studying of initial destruction stages. Aviacionnye materialy i tehnologii, 2018, no. 1 (50), pp. 77–87. DOI: 10.18577/2071-9140-2018-0-1-77-87.
  15. State Standard 5639–82. Steels and alloys. Methods of detection and determination of grain size. Moscow: Publ. House of Standards, 2003, 21 p.