The influence of the melt flow of polyetheretherketone on the characteristics of carbon fiber plastic based on it

Morozova V.S., Ivanov M.S., Shestakov A.M., Pavlukovich N.G.
Morozova V.S., Ivanov M.S., Shestakov A.M., Pavlukovich N.G. The influence of the melt flow of polyetheretherketone on the characteristics of carbon fiber plastic based on it // Proceedings of VIAM. 2024. No. 1. DOI: 10.18577/2307-6046-2024-0-1-44-51. URL: https://www.viam-works.ru/en/journal/2024/1/5
Keywords
polyetheretherketone, carbon fiber, melt flow rate, strength, tension, compression, bending, interlayer shear
Abstract

The properties of carbon fiber based on polyetheretherketone with different melt flow rate (from 52 to 1590 g/10 min) synthesized at the Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute» have been studied. The dependences of the values of the deformation and strength characteristics of carbon fiber on the MFR of the polymer binder have been revealed. The maximum values of the MFR of polyetheretherketone for production of carbon fiber with physical and mechanical properties that are not inferior to the characteristics of sheet carbon fiber VCU-65, developed by NRC «Kurchatov Institute» – VIAM.

Reference list
  1. Slavin A.V., Donetskiy K.I., Khrulkov A.V. Prospects for the use of polymer composite materials in aircraft structures in 2025–2035 (review). Trudy VIAM, 2022, no. 11 (117), paper no. 08. Available at: http://www.viam-works.ru (accessed: October 02, 2023). DOI: 10.1877/2307-6046-2022-0-11-81-92.
  2. Erasov V.S., Sibayev I.G. Scheme for the development and evaluation of properties of structural aviation composite materials. Aviation materials and technologies, 2023, no. 1 (70), paper no. 05. Available at: http://www.journal.viam.ru (accessed: October 02, 2023). DOI: 10.18577/2071-9140-2023-0-1-61-81.
  3. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), paper no. 10. Available at: http://www.journal.viam.ru (accessed: October 02, 2023). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  4. Gunyaev G.M., Kablov E.N. Structural carbon fiber reinforced plastics at the turn of the century. Aviation materials. Selected works of «VIAM» 1932–2002. Moscow: VIAM, 2002, pp. 242–247.
  5. Sorokin A.E., Ivanov M.S., Sagomonova V.A. Thermoplastic polymer composite materials based on polyetheretherketones of various manufacturers. Aviation materials and technologies, 2022, no. 1 (66), paper no. 04. Available at: http://www.journal.viam.ru (accessed: October 02, 2023). DOI: 10.18577/2071-9140-2022-0-1-41-50.
  6. Ivanov M.S., Sagomonova V.A., Morozova V.S. Domestic thermoplastic carbon plastic based on polyetheretherketone. Trudy VIAM, 2022, no. 12 (118), paper no. 05. Available at: http://www.viam-works.ru (accessed: October 02, 2023). DOI: 10.18577/2307-6046-2022-0-12-49-62.
  7. Beev A.A., Khashirova S.Yu., Beeva D.A., Shokumova M.U. Powdered aromatic polyetheretherketones and copolyetheretherketones. Plasticheskiye massy, 2022, no. 7–8, pp. 6–9. DOI: 10.35164/0554-2901-2022-7-8-6-9.
  8. Mikitaev A.K., Salamov A.Kh., Beev A.A., Beeva D.A. Filling with polyetheretherketones (PEEK) as a method for producing composites with high performance properties. Plasticheskiye massy, 2017, no. 5–6, pp. 6–9. DOI: 10.35164/0554-2901-2017-5-6-6-9.
  9. Lyashenko E.Yu., Yakovleva K.A., Andreeva T.I., Prudskova T.N., Kravchenko T.P., Gorbunova I.Yu., Davidyants N.G. Composite materials based on polyetheretherketone. Plasticheskiye massy, 2023, no. 1–2, pp. 11–13. DOI: 10.35164/0554-2901-2023-1-2-11-13.
  10. Kharaev A.M., Bazheva R.Ch. Polyetheretherketones: synthesis, properties, application (review). Plasticheskiye massy, 2018, no. 7–8, pp. 15–23. DOI: 10.35164/0554-2901-2018-7-8-15-23.
  11. May R. Polyetheretherketones. Encyclopedia of Polymer Science and Technology. Wiley, 2008, pp. 1–9. DOI:10.1002/0471440264.pst266.
  12. Method for producing polyetheretherketone: pat. 2673242 Rus. Federation; appl. 27.06.18; publ. 23.11.18.
  13. Gurenkov V.M., Gorshkov V.О., Chebotarev V.P., Prudskova Т.N., Andreeva Т.I. Comparative analysis of properties of polyetheretherketone of domestic and foreign production. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 41–47. DOI: 10.18577/2071-9140-2019-0-3-41-47.
  14. Gurenkov V.M., Molotkova N.N., Shelonina I.M., Petrova M.A., Gorshkova M.Yu., Prudskova T.N. Molecular mass characteristics of polyetheretherketone (PEEK): analysis of determination conditions. Plasticheskiye massy, 2021, no. 11–12, pp. 3–6. DOI: 10.35164/0554-2901-2021-11-12-3-6.
  15. Bogutsky V.B., Shron L.B. On the issue of using the melt flow index in polymer processing. Vestnik nauki i obrazovaniya Severo-Zapada Rossii, 2021, vol. 7, no. 2, pp. 1–8.
  16. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.