Fire safety of injection molding of thermoplastics and tpe material

Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V.
Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Fire safety of injection molding of thermoplastics and tpe material // Proceedings of VIAM. 2013. No. 11. URL: https://www.viam-works.ru/en/journal/2013/11/2
Abstract

The article describes the operational and technological properties of thermoplastic molding compositions, including high heat resistance, and thermoplastic elastomers – a new class of polymers that combine the power of plastic deformation and rubber processing thermoplastics. Polymers designed to meet requirements of АП-25 for the production of flammability and smoke.

Reference list
  1. Gudimov M.M. Osnovnye svoystva termoplastov [Basic properties of thermoplastics] //Aviatsionnaya promyshlennost'. 1990. №1. S. 2–8.
  2. Perov B.V., Surnin E.G. Termoplastichnye polimernye materialy mnogofunktsional'nogo naznacheniya [Multifunctional thermoplastic polymer materials] /V sb. Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2002. Yubileynyj nauchno-tehnicheskiy sbornik. M.: VIAM. 2002. S. 281–290.
  3. Ekardt G. Sostoyanie i perspektivy lit'ya pod davleniem izdeliy iz PM [Current state and trends of polymer products molding] //Polimernye materialy. 2007. №7. S. 16–24.
  4. Romashin A.G., Vikulin V.V., Muhin N.V. Progressivnye tehnologii i polimernye kompozitsionnye materialy dlya aviatsionnoy i raketno-kosmicheskoy tehniki HHΙ veka [Advanced technologies and polymer composite materials for aviation and aerospace engineering of XXI century] /V sb. Teoriya i praktika tehnologiy proizvodstva izdeliy iz kompozitsionnyh materialov i novyh metallicheskih splavov (TPKMM): Trudy Mezhdunarodnoy konf. M.: Znanie. 2004. S. 531–543.
  5. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  6. Petrova G.N., Abakumova N.M., Rumyantseva T.V. i dr. Pozharobezopasnye lit'evye termoplasty [Fire-safe molding thermoplastics] //Plasticheskie massy. 2005. №1. S. 45–46.
  7. Yuldashev A.H. Kompozitsionnye polimernye materialy konstruktsionnogo naznacheniya v mashinostroenii [Structural polymer composite materials in the mechanical engineering] //Kompozitsionnye materialy. 2010. №4. S. 71–73.
  8. Geoff G. Plastics in defense and safety //Plast. Eng. 2011. V. 6. №9. R. 28–31.
  9. Xiong Huawei, Zhao Dongbo. Shihua jishu yu yingong //Petrochem. Technol and Appl. 2011. V. 29. №5. Р. 435–438.
  10. Patent 8026309 SShA; opubl. 27.09.2011.
  11. Petrova G.N., Beider E.Ya. Molding thermoplastic materials for aerospace industry – Chemistry and Materials Science //Russian Journal of General Chemistry. 2011. V. 81. №5. Р. 1008–1013.
  12. Petrova G.N., Beyder E.Ya. Pozharobezopasnye lit'evye termoplasty dlya aviakosmicheskoy tehniki [Fire-safe molding thermoplastics for the aerospace engineering] //Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №8. S. 47–49.
  13. Mihaylin Yu.A. Termoustoychivye polimery i polimernye materialy [Thermally stable polymers and polymer materials]. SPb.: Professiya. 2006. S. 183–240.
  14. Hazova T.N. Sostoyanie rynka v proizvodstve polikarbonata [Market conditions in production of polycarbonate] //Mezhdunarodnye novosti mira plastmass. 2005. №1–2. S. 35, 36, 39.
  15. «Makrolon» kak faktor rosta Bayer v industrii polikarbonatov [Makrolon as the Bayer's growth factor in the industry of polycarbonates] //Chem. J. 2007. №2. S. 38–39.
  16. Petrova G.N. Napravlennaya modifikatsiya polisul'fonov i sozdanie na ih osnove lit'evyh i kompozitsionnyh materialov [Directional modification of polysulfones and formation of molding and composite materials on their basis]: Avtoref. dis. k.t.n. M.: VIAM. 2011. 27 s.
  17. Kravchenko T.P., Ermakov S.N., Kerber M.L., Kostyagina V.A. Nauchno-tehnicheskie problemy polucheniya kompozitsionnyh materialov na osnove konstruktsionnyh termoplastov [Scientific and technical problems of producing composite materials based on structural thermoplastics] //Plasticheskie massy. 2010. №10. S. 32–34.
  18. Bolduev V. Sovmeschaya nesovmestimoe [Combining the incompatible] //Plastiks. 2010. №4. S. 44–48.
  19. Petrova G.N., Rumyantseva T.V., Beyder E.Ya. Vliyanie modifitsiruyuschih dobavok na pozharobezopasnye svoystva i tehnologichnost' polikarbonata [Effect of modifying additives on fire-safe properties and processability of polycarbonate] //Trudy VIAM. 2013. №6. (elektronnyj zhurnal).
  20. Ermakov S.N., Kerber M.L., Kravchenko T.P. Himicheskaya modifikatsiya i smeshenie polimerov pri reaktsionnoy ekstruzii [Chemical modification and polymer blending in the process of reactive extrusion] //Plasticheskie massy. 2007. №10. S. 32–41.
  21. Petrova G.N., Beyder E.Ya., Chebotarev V.P. i dr. Regulirovanie svoystv polisul'fonov za schet modifikatsii [Polysulfones properties control through modification] //Plasticheskie massy. 2010. №12. S. 23–27.
  22. Mihaylin Yu.A. Pokazateli ognestoykosti PM i metody ih opredeleniya [Fire resistance criteria of polymer materials and methods for their determination] //Polimernye materialy. 2011. №8. S. 32–34.
  23. Shurkova E.N., Vol'nyj O.S., Izotova T.F., Barbot'ko S.L. Issledovanie vozmozhnosti snizheniya teplovydeleniya pri gorenii kompozitsionnogo materiala putem izmeneniya ego struktury [Study of the possibility for reducing the heat release by changing the composite structure during the burning process] //Aviatsionnye materialy i tehnologii. 2012. №1. S. 27–30.
  24. Kryzhanovskiy V.K., Burlov V.V. i dr. Tehnicheskie svoystva polimernyh materialov [Engineering properties of polymer materials] //Professiya. SPb. 2007. S. 35–37, 51–91, 174–182.
  25. Sudarushkin Yu.K., Gudimov M.M., Romanov D.S., Sokolov M.Yu. Primenenie lit'evyh polikarbonatov v aviapriborostroenii [Applications of molding polycarbonates for aircraft instrument engineering] //Aviatsionnaya promyshlennost'. 2003. №2. S. 48–52.
  26. Petrova G.N., Beyder E.Ya. Lit'evye termoplastichnye materialy [Molding thermoplastic materials] /V sb. 75 let. Aviatsionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM. 2007. S. 281–284.
  27. Petrova G.N., Barbot,ko S.L., Beider E.Ya., Bolotina L.M., Chebotarev V.P. Fire resistance properties of Polysulphones //International Polymer science and Technology. 2005. V. 32. №9. Р. 55–59.
  28. Dzheffri Holden, Hans R. Krihel'dorf, Roderik P. Kuirk. Termoelastoplasty [Thermoelastoplastics]: Per. s angl. SPb.: Professiya. 2011. S. 661–712.
  29. Evropeyskiy rynok termoplastichnyh elastomerov i sovremennye tendentsii [The European market of thermoplastic elastomers and current trends] //Promyshlennoe proizvodstvo i ispol'zovanie elastomerov. 2010. №3. S. 29–34.
  30. Polyurethane fiber containing poly (vinylidene fluoride): pat. TW470792 – TORAY DU PONT KK [JP] 01.01.2002.
  31. Halturinskiy N.A., Novikov D.D., Zhorina L.A. i dr. Vliyanie bromsoderzhaschih antipirenov na svoystva termoelastoplastov na osnove polipropilena i etilenpropilendienovogo kauchka [An effect of Br-bearing fire retardants on the properties of thermoplastic elastomers on the basis of polypropylene and ethylene-propylene rubber resin] //Perspektivnye materialy. 2010. №6. S. 68–71.
  32. Novokshonov V.V., Musin I.N., Kimel'blat V.I. Optimizatsiya svoystv maslostoykih termoplastichnyh elastomernyh kompozitsiy [Optimization of properties of oil resistant thermoplastic elastomeric compositions] //Plasticheskie massy. 2009. №3. S. 24–27.
  33. Nudel'man Z.N. Ftorkauchuki. Osnovy. Pererabotka. Primenenie. Reklama–Master [Fluoroelastomers. Fundamentals. Processing. Applications. Reklama-Master]. 2006. S. 40, 41, 170, 209, 210, 235, 237, 239.
  34. Petrova G.N., Perfilova D.N. i dr. Termoplastichnye elastomery dlya zameny rezin [Thermoplastic elastomer for the substitution of rubbers] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 302–308.
  35. Petrova G.N., Perfilova D.N., Rumyantseva T.V., Beyder E.Ya. Samozatuhayuschie termoelastoplasty [Self-extinguishing thermoelastoplastics] //Plasticheskie massy. 2013. №2. S. 5–7.
  36. Dushin M.I., Hrul'kov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detaley iz polimernyh kompozitsionnyh materialov [Selected technological parameters for the autoclave molding of polymer composites materials] //Aviatsionnye materialy i tehnologii. 2011. №3. S. 20–26.