Tendencies in the development of powder materials for the application of protective and functional coatings by the CGN method

Kozlov I.A., Fomina M.A., Dyomin S.A., Vasiliev A.S.
Kozlov I.A., Fomina M.A., Dyomin S.A., Vasiliev A.S. Tendencies in the development of powder materials for the application of protective and functional coatings by the CGN method // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-100-112. URL: https://www.viam-works.ru/en/journal/2023/8/9
Keywords
powder materials, repair technologies, protective coatings, increase in wear resistance, composite materials, coating morpholog, mechanical alloying
Abstract

The method of cold gas-dynamic spraying (CGS) of coatings has certain advantages, such as simplicity of the technological process, environmental friendliness, as well as the possibility of obtaining coatings with a wide range of functional properties (corrosion resistance, fire resistance, electrical insulating properties, etc.) through the use of various powder materials and ways to make them. The article presents the results of research in the field of application of powder materials for coating, describes composite powder materials with a complex structure obtained as a result of mechanical alloying, including those containing ceramic particles and particles of intermetallides.

Reference list
  1. Kosarev V.F., Alkhimov A.P. Technology, equipment, tools. Obrabotka metallov, 2003, no. 3, pp. 28–30.
  2. Alkhimov A.P., Gulidov A.I., Kosarev V.F., Nesterovich N.I. Peculiarities of deformation of microparticles upon impact with a solid barrier. Prikladnaya mekhanika i tekhnicheskaya fizika, 2000, vol. 41, no. 1, pp. 204–209.
  3. Alkhimov A.P., Klinkov S.V., Kosarev V.F., Fomin V.M. Cold gas-dynamic spraying. Theory and practice. Moscow: Fizmatlit, 2010, 536 p.
  4. Alkhimov A.P., Kosarev V.F., Papyrin A.N. The method of "cold" gas-dynamic spraying. DAN SSSR, 1990, vol. 315, no. 5, pp. 1062–1065.
  5. Peskova A.V., Bakradze M.M., Tikhonov M.M., Kuko I.S. Investigation of the influence of the oxide layer on the surface of particles metal-powder compositions of copper-chromium alloys on their technological properties. Trudy VIAM, 2023, no. 1 (119), paper no. 03. Available at: http://www.viam-works.ru (accessed: May, 18 2023). DOI: 10.18577/2307-6046-2023-0-1-28-38.
  6. Kozlov I.A., Fomina M.A., Demin S.A., Benarieb I., Khmeleva K.M. Use of metal powder compositions to remove defects of parts from VAS-1 alloy by cold gas-dynamic spraying method. Trudy VIAM, 2022, no. 12 (118), paper no. 09. Available at: http://www.viam-works.ru (accessed: May 17, 2023). DOI: 10.18577/2307-6046-2022-0-12-96-106.
  7. Khodykin L.G., Nyafkin A.N., Kosolapov D.V., Zhabin A.N. Laser welding of metal com-posite materials based on aluminium alloy reinforced with refractory particles SiC (review). Trudy VIAM, 2022, no. 12 (118), paper no. 06. Available at: http://www.viam-works.ru (accessed: April 05, 2023). DOI: 10.18577/2307-6046-2022-0-12-63-75.
  8. Druzhnova Ya.S. Development of methods for thermal spraying of hardening tires based on tungsten and chromium carbides (review). Trudy VIAM, 2022, no. 10 (116), paper no. 09. Available at: http://www.viam-works.ru (accessed: April 05, 2023). DOI: 10.18577/2307-6046-2022-0-10-100-115.
  9. Dykhuizen R.C., Smith M.F. Gas dynamic principles of cold spray. Journal of Thermal Spray Technology, 1998, vol. 7, no. 2, pp. 205–212.
  10. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  11. Kablov E.N., Startsev O.V. The basic and applied research in the field of corrosion and ageing of materials in natural environments (review). Aviacionnye materialy i tehnologii, 2015, no. 4 (37), pp. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  12. Kablov E.N., Startsev O.V., Medvedev I.M. Review of international experience on corrosion and corrosion protection. Aviacionnye materialy i tehnologii, 2015, no. 2 (35), pp. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  13. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 12, 2023). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  14. Konovalov V.V., Dubinskiy S.V., Makarov A.D., Dotsenko A.M. Research of correlation dependencies between mechanical properties of aviation materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 40–46. DOI: 10.18577/2071-9140-2018-0-2-40-46.
  15. Zamaletdinov I.I. Corrosion and protection of metals. Corrosion of powder materials: textbook. Perm: Perm State Tech. Univ, 2007, pp. 18–19.
  16. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  17. Zakirova L.I., Laptev A.B. Properties of protective electroplating coatings for replacement of cadmium on steel fixing parts (review). Part 1. Morphology and corrosion resistance. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 37–46. DOI: 10.18577/2071-9140-2020-0-3-37-46.
  18. Kozlov I.A., Leshchev K.A., Nikiforov A.A., Demin S.A. Cold spray coatings (review). Trudy VIAM, 2020, no. 8 (90), paper no. 08. Available at: http://www.viam-works.ru (accessed: May 04, 2023). DOI: 10.18577/2307-6046-2020-0-8-77-93.
  19. Abiev R.Sh., Bibik E.E., Vlasov E.A. et al. New reference book of a chemist and technologist. Electrode processes. Chemical kinetics and diffusion. colloidal chemistry. St. Petersburg: Professional, 2004, 838 p.
  20. Moridi A., Azadi M., Farrahi G.H. Thermo-mechanical stress analysis of thermal barrier coating system considering thickness and roughness effects. Surface and Coatings Technology, 2014, vol. 243, pp. 91–99.
  21. Richer P., Zúñiga A., Yandouzi M., Jodoin B. CoNiCrAlY microstructural changes induced during cold gas dynamic spraying. Surface and Coatings Technology, 2008, vol. 203, pp. 364–371.
  22. Inoue A., Kato A., Zhang T.G.K.S., Masumoto T. Mg–Cu–Y amorphous alloys with high mechanical strengths produced by ametallic mold casting method. Materials Transactions JIM, 1991, vol. 32, pp. 609–616.
  23. Сold gas dynamic spraying of high strength copper: рat. US7553385 В2; appl. 23.11.04; publ. 30.01.09.
  24. Wang C.-C., Mao Y.-W., Shan Z.-W. et al. Real-time, high-resolution study of nanocrystallization and fatigue cracking in a cyclically strained metallic glass. Proceedings of the National Academy of Sciences of the USA. 2013, pp. 1–6. DOI: 10.1073/pnas.1320235110.
  25. List A., Gärtner F., Schmidt T., Klassen T. Impact conditions for cold spraying of hard metallic glasses. Journal of Thermal Spray Technology, 2012, vol. 21, pp. 531–540.
  26. Zhang Y.Y., Wu X.K., Cui H., Zhang J.S. Cold-sprayprocessing of a high density nanocrystalline aluminum alloy 2009 coating using a mixture of as-atomized and as-cryomilled powders. Journal of Thermal Spray Technology, 2011, vol. 20, pp. 1125–1132.
  27. Novoselova T., Fox P., Morgan R., O’Neill W. Experimental study of titanium/aluminium deposits produced by cold gas dynamic spray. Surface and Coatings Technology, 2006, vol. 200, pp. 2775–2783.
  28. Kong L.Y., Shen L., Lu B. et al. Preparation of TiAl3–Al composite coating by cold spray and its high temperature oxidation behavior. Journal of Thermal Spray Technology, 2010, vol. 19, pp. 1206–1210.
  29. Lee H., Shin H., Ko K. Effects of gas pressure of cold spray on the formation of Al-based intermetallic compound. Journal of Thermal Spray Technology, 2010, vol. 19, pp. 102–109.
  30. Obtaining a single-phase intermetallic alloy based on the aluminum-titanium system: pat. RU 2561952; appl. 27.02.14, publ. 10.09.15.
  31. Liang Y., Shi B., Yang X. et al. Microstructure and nano-mechanical property of cold spray Co-base refractory alloy coating. Acta Metall. Sin. (English Letters), 2011, vol. 24, pp. 190–194.
  32. King P.C., Zahiri S.H., Jahedi M.Z. Rare earth/metal composite formation by cold spray. Journal of Thermal Spray Technology, 2008, vol. 17, pp. 221–227.
  33. Method for obtaining nanostructured functionally graded wear-resistant coatings: pat. 2354749 Rus. Federation; appl. 12.04.07; publ. 10.05.09.
  34. Method for producing composite reinforced powder material: pat. RU 2573309; appl. 08.07.14, publ. 20.01.16.
  35. Lee H., Shin H., Ko K. Effects of gas pressure of cold spray on the formation of Al-based intermetallic compound. Journal of Thermal Spray Technology, 2010, vol. 19, pp. 102–109.
  36. Liang Y., Shi B., Yang X., Zhang J., Meng X. Microstructure and nano-mechanical property of cold spray Co-base refractory alloy coating. Acta Metallurgica Sinica (English Letters), 2011, vol. 24, pp. 190–194.
  37. Al-Mangour B., Mongrain R., Irissou E., Yue S. Improving the strength and corrosion resistance of 316L stainless steel for biomedical applications using cold spray. Surface and Coatings Technology, 2013, vol. 216, pp. 297–307.
  38. Kang H.-K., Kang S.B. Tungsten/copper composite deposits produced by a cold spray. Scripta Materialia, 2003, vol. 49, pp. 1169–1174.
  39. King P.C., Zahiri S.H., Jahedi M.Z. Rare earth/metal composite formation by cold spray. Journal of Thermal Spray Technology, 2008, vol. 17, pp. 221–227.
  40. Yang G.-J., Li C.-J., Han F. et al. Low temperature deposition and characterization of TiO2 photocatalytic film through cold spray. Applied Surface Science, 2008, vol. 254, pp. 3979–3982.
  41. Bu H., Yandouzi M., Lu C. et al. Cold spray blended Al+Mg 17Al 12 coating for corrosion protection of AZ91D magnesium alloy. Surface and Coatings Technology, 2012, vol. 207, pp. 155–162.
  42. Kozlov I.A., Nikiforov A.A., Demin S.A., Vdovin A.I. Use of metal powder composition of the zinc–aluminum system for application of a protective coating by the method of cold gas-dynamic spraying. Trudy VIAM, 2022, no. 6 (112), paper no. 08. Available at: http://www.viam-works.ru (accessed: April 03, 2023). DOI: 10.18577/2307-6046-2022-0-7-89-98.