New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys

Echin A.B., Deynega G.I., Narskiy A.R.
Echin A.B., Deynega G.I., Narskiy A.R. New developments of NRC «Kurchatov Institute» – VIAM in the field of materials for casting processes of superalloys // Proceedings of VIAM. 2023. No. 8. DOI: 10.18577/2307-6046-2023-0-8-13-24. URL: https://www.viam-works.ru/en/journal/2023/8/2
Keywords
blades of gas turbine engines, cobalt aluminate, surface modification, aviation materials science, superalloys, equiaxial casting, directional crystallization
Abstract

The main results of the research work carried out at the NRC "Kurchatov Institute" – VIAM in the period from 2015 to the present in the field of creating new materials for casting processes of nickel superalloys are considered. Serial production and supply of a number of materials to machine-building enterprises has been established. A promising task is the organization of low-tonnage production of blades for power turbine installations in order to solve the problem of import substitution and expansion of domestic production.

Reference list
  1. History of aviation materials science. VIAM – 80 years: years and people. Ed. E.N. Kablov. Moscow: VIAM, 2012, 520 p.
  2. Kablov E.N. Improving the performance of cast blades of gas turbine engines from heat-resistant nickel alloys by controlling the process of structure formation during crystallization: thesis, Dr. Sc. (Tech.). Moscow: MGATU im. K.E. Tsiolkovsky, 1995, 60 p
  3. Cast blades of gas turbine engines: alloys, technologies, coatings. Ed. E.N. Kablov. 2nd ed. Moscow: Nauka, 2006, 632 p.
  4. Narsky A.R., Deinega G.I., Kuzmina I.G. The use of a modifier - cobalt aluminate in the casting of blades of gas turbine engines. Part 1. Liteynoye proizvodstvo, 2022, no. 3, pp. 15–19.
  5. Narsky A.R., Deinega G.I., Kuzmina I.G. Obtaining a fine–grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), paper no. 01. Available at: http://www.journal.viam.ru. DOI: 10.18577/2713-0193-2023-0-3-3-14.
  6. Lost wax casting. Eds. Ya.I. Shklennik, V.A. Ozerov. 3Rd ed. Moscow: Mashinostroenie, 1984, 408 p.
  7. Ospennikova O.G., Kablov E.N., Shunkin V.N. Development and research of a plasticizer for model compositions based on natural waxes. Aviation materials and technologies, 2002, no. 3, pp. 68–70.
  8. Ospennikova O.G. Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  9. Aslanyan I.R., Rassokhina L.I., Ospennikova O.G. Definition of quantitative factors, significantly influencing on technological characteristics of model compositions). Trudy VIAM, 2018, no. 12 (72), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 14, 2023). DOI: 10.18577/2307-6046-2018-0-12-3-13.
  10. Ospennikova O.G. Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures. Aviacionnye materialy i tehnologii, 2014, no. 3, pp. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  11. Bondarenko Yu.A. Trends in the development of high-temperature metal materials and technologies in the production of modern aircraft gas turbine engines. Aviacionnye materialy i tehnologii, 2019, no. 2 (55), pp. 3–11. DOI: 10.18577/2071-9140-2019-0-2-3-11.
  12. Toloraya V.N., Ostroukhova G.A. Studying of the mechanism of origin of monocrystals from Re-Ru-containing nickel heat resisting alloys with the set spatial crystallographic orientation from Ni–W–Re–C system primings with a temperature likvidusa 1550–1600 °C. Voprosy materialovedeniya, 2023 (in print).
  13. Toloraya V.N., Ostroukhova G.A. Obtaining single-crystal seeds [001] from alloys of the Ni–W system by the method of directed crystallization. Voprosy materialovedeniya, 2021, no. 2 (106), pp. 55–65.
  14. Visik E.M., Gerasimov V.V., Kolyadov E.V., Kuzmina N.A. Influence of technological modes of casting on the parameters of the structure of single crystals of new heat-resistant alloys. Metallurgiya mashinostroyeniya, 2016, no. 5, pp. 27–31.
  15. Kuzmina N.A. Growth structural defects in single crystals of nickel heat-resistant alloys. Aviation materials and technologies, 2022, no. 3 (68), paper no. 02. Available at: http://www.journal.viam.ru (accessed: May 22, 2023). DOI: 10.18577/2713-0193-2022-0-3-15-26.
  16. Sokolov A.V., Deynega G.I., Kuzmina N.A., Kuzmina I.G. Structural and mechanical properties of a composite material based on partially stabilized zirconium dioxide doped with magnesium aluminate spinel. Aviation materials and technologies, 2021, no. 3 (64), paper no. 07. Available at: http://www.journal.viam.ru (accessed: May 18, 2023). DOI: 10.18577/2713-0193-2021-0-3-78-85.
  17. Folomeikin Yu.I., Kablov E.N., Demonis I.M. Highly refractory ceramic rods and molds for casting blades by directional crystallization. Aviatsionnye materialy i tekhnologii, 2003, no. 1, pp. 33–44.
  18. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V. Research of compositions of ceramic rods based on fused quartz and their manufacturing technology. Trudy VIAM, 2021, no. 1 (95), paper no. 04. Available at: http://www.viam-works.ru (accessed: May 14, 2023). DOI: 10.18577/2307-6046-2021-0-1-34-42.
  19. Rassokhina L.I., Bityutskaya O.N., Gamazina M.V., Avdeev V.V. Investigation of the main characteristics of ceramic rods based on fused quartz for the manufacture of castings for aircraft engine blades. Liteynoye proizvodstvo, 2022, no. 10, pp. 26–30.
  20. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.