Investigation of corrosion resistance of ion-plasma coatings for the protection of intermetallic titanium alloy

Antipov V.V., Gorlov D.S., Chesnokov D.V., Juravleva P.L., Ivanov I.M.
Antipov V.V., Gorlov D.S., Chesnokov D.V., Juravleva P.L., Ivanov I.M. Investigation of corrosion resistance of ion-plasma coatings for the protection of intermetallic titanium alloy // Proceedings of VIAM. 2023. No. 6. DOI: 10.18577/2307-6046-2023-0-6-105-114. URL: https://www.viam-works.ru/en/journal/2023/6/9
Keywords
corrosion resistance, accelerated cyclic corrosion tests, ion-plasma coatings, deformable intermetallic titanium alloy
Abstract

Presents the results of comparative tests of corrosion resistance of ion-plasma layered coatings of the (Ti–TiN) + VSDP-13 system obtained after vacuum annealing and after saturation in metal plasma to protect the deformable intermetallic titanium ortho-alloy VIT6. Metallographic studies and studies of the phase composition were carried out after accelerated cyclic corrosion tests at a temperature of 700 °C on the basis of 10 cycles. An increase in the corrosion resistance of the alloy-coating composition was found when vacuum annealing was applied at a temperature of 700 °C for 5 hours relative to saturation in metal plasma.

Reference list
  1. Antipov V.V., Duyunova V.A., Oglodkov M.S., Fomina M.A., Frantsuzova T.P., Kozlov I.A. 90-year practice of anticorrosive protection. Trudy VIAM, 2022, no. 6 (112), paper no. 09. Available at: http://www.viam-works.ru (accessed: January 26, 2023). DOI: 10.18577/2307-6046-2022-0-6-108-126.
  2. Nochovnaya N.A., Bazyleva O.A., Kablov D.E., Panin P.V. Intermetallic alloys based on titanium and nickel. Ed. E.N. Kablov. Moscow: VIAM, 2018, 308 p.
  3. Nochovnaya N.A., Shiryaev A.A., Sharapkin D.S. Complex of mechanical and operational properties of rolled blanks from metastable-β-titanium alloy VT47. Aviation materials and technologies, 2022, no. 1 (66), paper no. 05. Available at: http://www.journal.viam.ru (accessed: January 26, 2023). DOI: 10.18577/2713-0193-2022-0-3-50-59.
  4. Grigorenko S.G., Grigorenko G.M., Zadorozhnyuk O.M. Titanium intermetallics. Features, application properties (review). Sovremennaya elektrometallurgiya, 2017, no. 3 (128), pp. 51–58. DOI: 10.15407/sem2017.03.08.
  5. Kablov E.N., Kashapov O.S., Medvedev P.N., Pavlova T.V. Study of a α + β-titanium alloy based on a system of Ti–Al–Sn–Zr–Si–β-stabilizing alloying elements. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 30–37. DOI: 10.18577/2071-9140-2020-0-1-30-37.
  6. Kablov E.N., Ospennikova O.G., Kucheryaev V.V. Thermomechanical behavior of intermetallic alloys of Ni–Al–Co and Ti–Al–Nb systems during isothermal deformation. Pisma o materialakh, 2016, vol. 6, no. 3 (23), pp. 189–194. DOI: 10.22226/2410-3535-2016-3-189-194.
  7. Kapustin V.I., Zakharchenko K.V., Cherepanova V.K., Shayapov V.R. Investigation of dissipative processes of VT6 alloy under fatigue. Aviation materials and technologies, 2022, no. 1 (69), paper no. 09. (accessed: January 26, 2023). DOI: 10.18577/2713-0193-2022-0-4-96-111.
  8. Polkin I.S., Grebenyuk O.N., Salenkov V.S. Intermetallic compounds based on titanium. Tekhnologiya legkikh splavov, 2010, no. 2, pp. 59–15.
  9. Kablov E.N., Nikiforov A.A., Demin S.A., Chesnokov D.V., Vinogradov S.S. Promising coatings for corrosion protection of carbon steels. Stal, 2016, no. 6, pp. 70–81.
  10. Kablov E.N., Kutyrev A.E., Vdovin A.I., Kozlov I.A., Afanasyev-Khodykin A.N. The research of possibility of galvanic corrosion in brazed connections used in aviation engine construction. Aviation materials and technologies, 2021, no. 4 (65), paper no. 01. Available at: http://www.journal.viam.ru (accessed: January 26, 2023). DOI: 10.18577/2713-0193-2021-0-4-3-13.
  11. Shubin I.Yu., Nikitin Ya.Yu., Puchkov Yu.A. et al. Investigation of resistance to high-temperature gas and salt corrosion of heat-resistant and intermetallic titanium alloy VTI-4. Vestnik MGTU im. N.E. Bauman. Ser.: Mechanical engineering, 2020, no. 6, pp. 83–105. DOI: 10.18698/0236-3941-2020-6-83-105.
  12. Eremin E.N., Yurov V.M., Laurinas V.Ch., Syzdykova A.Sh. Influence of technological parameters of application of multi-element ion-plasma coatings on their quality. Omskiy nauchnyy vestnik, 2019, no. 4 (166), pp. 9–13. DOI: 10.25206/1813-8225-2019-166-9-13.
  13. Khamin O.N., Lavro V.N. The use of ion-plasma coatings for soldering titanium alloys with steels. Sovremennye materialy, tekhnika i tekhnologii, 2019, no. 4 (26). pp. 196–201.
  14. Lavro V.N. Investigation of the influence of technological parameters of applying ion-plasma coatings on their quality. Sovremennye materialy, tekhnika i tekhnologii, 2018, no. 4 (19), pp. 63–69.
  15. Mukhin V.S., Budilov V.V., Shekhtman S.R. Methodology for creating coatings with improved performance properties and technologies for their application to the blades of a gas turbine engine compressor. Vestnik UGATU, 2012, no. 5 (50), art. 16, pp. 149–153.
  16. Terukalova N.V., Novitskaya O.S., Sizova O.V. Microstructure and tribotechnical properties of multilayer CrN–TiN ion-plasma coatings. Mezhdunarodny nauchno-issledovatelskiy zhurnal, 2021, no. 12 (114), part 1, pp. 81–85. DOI: 10.23670/IRJ.2021.114.12.011.
  17. Doronin O.N., Gorlov D.S., Azarovsky E.N., Kochetkov A.S. Study of the structure and properties of a heat-resistant coating at high-temperature deformation of samples from titanium intermetallic alloy. Aviation materials and technology, 2021, no. 1 (62), paper no. 06. Available at: http://www.journal.viam.ru (accessed: January 26, 2023). DOI: 10.18577/2713-0193-2021-0-1-61-70.
  18. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.