Modifying of cast aluminum alloys (review)
Duyunova V.A., Trapeznikov A.V., Leonov A.A., Koreneva E.A. Modifying of cast aluminum alloys (review) // Proceedings of VIAM. 2023. No. 4. DOI: 10.18577/2307-6046-2023-0-4-14-26. URL: https://www.viam-works.ru/en/journal/2023/4/2
Keywords
cast aluminum alloys, mechanical properties, microstructure, modifying, rare earth elements, flux
Abstract
The article presents and summarizes data on the modification of cast aluminum alloys. In addition to the use of standard modifiers such as sodium, strontium, titanium, zirconium, scandium and titanium diboride, a positive effect of europium and hafnium on alloys has been shown. Despite the fact that many effective modifiers belong to the rare earth elements (REE), not all REE have a strong effect. The introduction of metals such as ytterbium and erbium into aluminum alloys had almost no effect on the morphology and size of the microstructure.
Reference list
- Eskin G.I., Bochvar S.G. Modification of aluminum alloys by acoustic impact. Tekhnologiya legkikh splavov, 2018, no. 3, pp. 14–19.
- Lipchin T.N. Structure and properties of non-ferrous alloys hardened under pressure. Moscow: Metallurgiya, 1994, 128 p.
- Nikitin K.V. Modification and complex processing of silumins: textbook. 2nd ed., rev. and add. Samara: Samara State Tech. Univ., 2016, 92 p.
- Altman M.B., Stromskaya N.P. Improving the properties of standard cast aluminum alloys. Moscow: Metallurgiya, 1984, 128 p.
- Maltsev M.V. Metallography of industrial non-ferrous metals and alloys. 2nd ed. Moscow: Metallurgiya, 1970, 346 p.
- Lu L., Nogita K., Dahle A.K. Combining Sr and Na additions in hypoeutectic Al–Si foundry alloys. Material Science and Engineering A, 2005, vol. 399, pp. 244–253.
- Li J.H., Barrirero J., Engstler M. et al. Nucleation and growth of eutectic Si in Al–Si alloys with Na addition. Metallurgical and Materials Transactions A, 2015, vol. 46, pp. 1300–1311.
- Emadi D., Gruzleski J.E., Toguri J.M. The effect of Na and Sr modification on surface tension and volumetric shrinkage of A356 alloy and their influence on porosity formation. Metallurgical and Materials Transactions B, 1993, vol. 24 (6), pp. 1055–1063.
- lwahori H., Yonekura K., Yamamoto Y., Nakamura M. Occurring behavior of porosity and feeding capabilities of sodium- and strontium-modified Al–Si alloys. Transactions of the American Foundrymen’s Society, 1990, vol. 98, pp. 167–173.
- Wang Q.G. Microstructural effects on the tensile and fracture behavior of aluminum casting alloys A356/357. Metallurgical and Materials Transactions A, 2003, vol. 34 (12), pp. 2887–2899.
- Gruzleski J.E., Closset B.M. The treatment of liquid aluminum-silicon alloys. Des Plaines: American Foundrymen’s Society, Inc., 1990, 256 p.
- Wang Q.G., Apelian D., Lados D.A. Fatigue behavior of A356–T6 aluminum cast alloys. Part I. Effect of casting defects. Journal of Light Metals, 2001, vol. 1 (1), pp. 73–84.
- Wang Q.G., Apelian D., Lados D.A. Fatigue behavior of A356–T6 aluminum cast alloys. Part II. Effect of microstructural constituents. Journal of Light Metals, 2001, vol. 1 (1), pp. 85–97.
- Öztürk İ., Ağaoğlu G.H., Erzi E. et al. Effects of strontium addition on the microstructure and corrosion behavior of A356 aluminum alloy. Journal of Alloys and Compounds, 2018, vol. 763, pp. 384–391. DOI: 10.1016/j.jallcom.2018.05.341.
- Uludağ M., Çetin R., Dispinar D., Tiryakioğlu M. Characterization of the effect of melt treatments on melt quality in Al–7 wt. % Si–Mg Alloys. Metals, 2017, vol. 7 (5), pp. 157–172. DOI: 10.3390/met7050157.
- Eguskiza S., Niklas A., Fernández-Calvo A.I. et al. Study of strontium fading in Al–Si–Mg and Al–Si–Mg–Cu alloy by thermal analysis. International Journal of Metalcasting, 2015, vol. 9 (3), p. 43–50.
- Dahle A.K., Nogita K., McDonald S.D. et al. Eutectic modification and microstructure development in Al–Si Alloys. Material Science and Engineering A, 2005, vol. 413, pp. 243–248.
- Closset B., Gruzleski J.E. Structure and properties of hypoeutectic Al–Si–Mg alloys modified with pure strontium. Metallurgical and Materials Transactions A, 1982, vol. 13 (6), pp. 945–951.
- Dahle A.K., Nogita K., McDonald S.D. et al. Eutectic nucleation and growth in hypoeutectic Al–Si alloys at different strontium levels. Metallurgical and Materials Transactions B, 2001, vol. 32 (4), pp. 949–960.
- Samuel A.M., Doty H.W., Valtierra S., Samuel F.H. Effect of grain refining and Sr-modification interactions on the impact toughness of Al–Si–Mg cast alloys. Materials and Design, 2014, vol. 56, pp. 264–273.
- Lin B., Li H., Xu R. et al. Effects of Vanadium on Modification of Iron-Rich Intermetallics and Mechanical Properties in A356 Cast Alloys with 1.5 wt. % Fe. Journal of Materials Engineering and Performance, 2019, vol. 28, pp. 475–484. DOI: 10.1007/s11665-018-3798-4.
- Barrirero J., Pauly C., Engstler M. et al. Eutectic modifcation by ternary compound cluster formation in Al–Si alloys. Scientific Reports, 2019, vol. 9, art. 5506. DOI: 10.1038/s41598-019-41919-2.
- Ahmad R., Wahab N.A., Hasan S. et al. Effect of Erbium Addition on the Microstructure and Mechanical Properties of Aluminium Alloy. Key Engineering Materials, 2019, vol. 796, pp. 62–66. DOI: 10.4028/www.scientific.net/KEM.796.62.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Rare metals and rare earth elements – materials of modern and future high technologies. Trudy VIAM, 2013, no. 2, paper no. 01. Available at: http://www.viam-works.ru (accessed: December 05, 2022).
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Mazalov I.S., Mazalov P.B., Suhov D.I., Sulyanova E.A. Influence of hot isostatic pressing parameters on structure and properties of cobalt-based alloys obtained by selective laser melting. Aviation materials and technologies, 2021, no. 2 (63), paper no. 01. Available at: http://www.journal.viam.ru (accessed: May 06, 2022). DOI: 10.18577/2713-0193-2021-0-2-3-14.
- Zhang H., Wang D., Qinc K. et al. Effect of Compound Modification and Cooling Rate on Microstructure and Mechanical Properties of Al–25 % Si Alloy. Materials Science Forum, 2016, vol. 877, pp. 27–32. DOI: 10.4028/www.scientific.net/MSF.877.27.
- Li J.H., Ludwig T.H., Oberdorfer B., Schumacher P. Solidification behavior of Al–Si based alloys with controlled additions of Eu and P. International Journal of Cast Metals Research, 2018, vol. 31, no. 6, pp. 319–331. DOI: 10.1080/13640461.2018.1480891.
- Krishna N.N., Sivaprasad K., Susila P. Strengthening contributions in ultra-high strength cryorolled Al–4 % Cu–3 % TiB2 in situ composite. Transactions of Nonferrous Metals Society of China, 2014, vol. 24, pp. 641–647.
- Krishna N.N., Sivaprasad K. High temperature tensile properties of cryorolled Al–4 % Cu–3 % TiB2 in-situ composites. Transactions of the Indian Institute of Metals, 2011, vol. 64, pp. 63–66.
- Mandal A., Maiti R., Chakraborty M., Murty B.S. Effect of TiB2 particles on aging response of Al–4 % Cu alloy. Material Science and Engineering A, 2004, vol. 386, pp. 296–300.
- Wu S.Q., Zhu H.G., Tjong S.C. Wear Behavior of In Situ Al-Based Composites Containing TiB2, Al2O3, and Al3Ti Particles. Metallurgical and Materials Transactions A, 1999, vol. 30a, pp. 243–247.
- Promakhov V.V., Khmeleva M.G., Zhukov I.A. et al. Influence of Vibration Treatment and Modification of A356 Aluminum Alloy on Its Structure and Mechanical Properties. Metals, 2019, vol. 9, pp. 87. DOI: 10.3390/met9010087.
- Ogorodov D.V., Trapeznikov A.V., Popov D.A., Pentuykhin S.I. The development of casting heat-resistant aluminum alloys (To the 120th anniversary since the birth of I.F. Kolobnev). Trudy VIAM, 2017, no. 2 (50), paper no. 12. Available at: http://viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2017-0-2-12-12.
- Belousov N.N. Cast aluminum-magnesium alloys. Cast aluminum alloys. Ed. I.N. Friedlander. Moscow: Oborongiz, 1961, pр. 52–65.
- Cherkasov V.V. Foundry welded corrosion-resistant aluminum alloy VAL16: method. management. Moscow: VIAM, 1990, 84 p.
- Levchuk V.V., Trapeznikov A.V., Pentyukhin S.I. Corrosion-resistant foundry aluminum alloys (review). Trudy VIAM, 2018, no. 7 (67), paper no. 4. Available at: http://www.viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2018-0-7-33-40.
- Belov E.V., Duyunova V.A., Leonov A.A., Trapeznikov A.V. Method of increasing tightness and hardening of cast corrosion-resistant welded magnalias. Trudy VIAM, 2020, no. 6–7 (89), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2020-0-67-11-18.
- Antipov K.V., Oglodkova Yu.S., Kuryntsev S.V., Safiullin E.I. Investigation of the influence of heat treatment modes on the structure and properties of sheets of aluminum-lithium alloy V-1469. Trudy VIAM, 2022, no. 11 (117), paper no. 02. Available at: http://www.viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2022-0-11-16-26.
- Kuznetsov A.O., Oglodkov M.S., Klimkina A.A. The influence of chemical composition on structure and properties of Al–Mg–Si alloy. Trudy VIAM, 2018, no. 7 (67), paper no. 01. Available at: http://www.viam-works.ru (accessed: December 05, 2022). DOI: 10.18577/2307-6046-2018-0-7-3-9.
- Yashin V.V., Aryshenskii E.V., Drits A.M., Latushkin I.A. Influence of additives of the transition metal hafnium on the microstructure of aluminum alloy 01570. Tsvetnye metally, 2020, no. 11, pp. 84–90.
- Postnikov N.S. Corrosion resistant aluminum alloys. Moscow: Metallurgiya, 1976, 300 p.