The repair monolithic zones of polymer composite materials helicopter blades ultrasonic testing specificity
Boychuk A.S., Chertishchev V.Yu., Dikov I.A., Generalov A.S. The repair monolithic zones of polymer composite materials helicopter blades ultrasonic testing specificity // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-115-124. URL: https://www.viam-works.ru/en/journal/2023/12/10
Keywords
polymer composite materials, helicopter blade, monolithic zones, repair, nondestructive testing, ultrasonic pulse-echo technique
Abstract
A special approach is required for repair process as opposed to polymer composite materials monolithic structures testing for it production and operation. The results of repaired monolithic specimens simulating helicopter blade spar fragment research is described at the article. The researches were carried out by ultrasonic pulse-echo technique. It is shown that the repaired monolithic zone testing depending on the repair scheme can be divided into the repair patch material testing and quality testing of its gluing to the main material of the repaired object.
Reference list
- Kablov E.N., Valueva M.I., Zelenina I.V., Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: May 12, 2023). DOI: 10.18577/2307-6046-2020-0-1-68-77.
- Kablov E.N. What will the future be made of? New generation materials, technologies for their creation and processing – the basis of innovation. Krylya Rodiny, 2016, no. 5, pp. 8–18.
- Kablov E.N. Materials for aerospace technology. Vse materialy. Entsiklopedicheskiy spravochnik, 2007, no. 5, рр. 7–27.
- Sidorina A.I. Multiaxial carbon fabrics in the products of aviation technology (review). Aviation materials and technologies, 2021, no. 3 (64), paper no. 10. Available at: http://www.journal.viam.ru (accessed: May 12, 2023). DOI: 10.18577/2713-0193-2021-0-3-105-116.
- Donetskiy K.I., Karavaev R.Yu., Bystrikova D.V., Gracheva A.D. Сarbon fiber based on a volume-reinforcing braided preform for an element of a propeller blade. Trudy VIAM, 2022, no. 12 (118), paper no. 03. Available at: http://www.viam-works.ru (accessed: May 12, 2023). DOI: 10.18577/2307-6046-2022-0-12-27-38.
- Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 1. Automated Tape Laying (ATL). Aviation materials and technologies, 2021, no. 2 (63), paper no. 06. Available at: http://www.journal.viam.ru (accessed: June 06, 2023). DOI: 10.18577/2713-0193-2021-0-2-51-61.
- Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. The development of automated laying: from the beginning to our days (review). Part 2. Automated Fiber Placement (AFP). Aviation materials and technologies, 2021, no. 3 (64), paper no. 11. Available at: http://www.journal.viam.ru (accessed: June 06, 2023). DOI: 10.18577/2713-0193-2021-0-3-117-127.
- Barannikov A.A., Postnova M.V., Krasheninnikova E.V., Vasyukov A.N. Application of new technologies in the production of helicopter main rotor blades. Trudy VIAM, 2021, no. 11 (105), paper no. 09. Available at: http://www.viam-works.ru (accessed: June 06, 2023). DOI: 10.18577/2307-6046-2021-0-11-91-102.
- Basharov E.A., Vagin A.Yu. Analysis of the use of composite materials in the design of helicopter airframes. Trudy MAI, 2017, no. 92, рр. 1–33. Available at: http://cyberleninka.ru/article/n/analiz-primeneniya-kompozitsionnyh-materialov-v-konstruktsii-planerov-vertoletov (accessed: June 13, 2023).
- Doroshenko N.I. Application of PCM in the design of helicopter rotor blades. Polymer composite materials for the aerospace industry: All-Rus. materials. scientific-technical conf. Moscow: VIAM, 2019. P. 23–41. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1234.pdf (accessed: June 19, 2023).
- Rivin G.L. Repair of structures made of polymer composite materials of aircraft: a textbook. Ulyanovsk: UlSTU, 2000, 75 p.
- Katnam K.B., DaSilva L.F.M., Young T.M. Bonded repair of composite aircraft structures: A review of scientific challenges and opportunities. Progress in Aerospace Sciences, 2013, no. 61, рр. 26–42. Available at: https://www.researchgate.net/publication/258240754_Bonded_repair_of_composite_aircraft_structures_A_review_of_scientific_challenges_and_opportunities (accessed: June 19, 2023).
- Barannikov A.B. Materials, technologies and equipment of the National Research Center «Kurchatov Institute» – VIAM for the repair of structures made of PCM. New materials and technologies for deep processing of raw materials – the basis of innovative development of the Russian economy: materials of the III Int. scientific-technical conf. Moscow: National Research Center «Kurchatov Institute» – VIAM, 2022. P. 167–190. Available at: https://conf.viam.ru/sites/default/files/uploads /proceedings/1497.pdf (accessed: June 19, 2023).
- Non-destructive testing: a reference book in 7 vol. Ed. V.V. Klyueva. Moscow: Mashinostroyeniye, 2004, vol. 3: Ultrasonic testing, 864 p.
- Boychuk A.S., Generalov A.S., Dalin M.A., Dikov I.A. Inspection of monolithic parts and structures of aircraft manufactured from PCM by ultrasonic non-destructive testing using phased arrays. TestMat. Main trends, directions and prospects for the development of non-destructive testing methods in the aerospace industry: materials of the X All-Rus. conf. Moscow: VIAM, 2018, pp. 18–31. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1063.pdf (accessed: June 08, 2023).
- Dikov I.A., Boychuk A.S., Chertishchev V.Yu., Dalin M.A., Generalov A.S. Experience in automated ultrasonic testing of monolithic and honeycomb structures made of PCM. TestMat. Digital technologies, modeling and automation of non-destructive testing processes in the aerospace industry. Problems and prospects for implementation: materials of the XIII All-Rus. conf. on testing and research of materials properties. Moscow: VIAM, 2021, рр. 157–180. Available at: https://conf.viam.ru/sites/default/files/uploads/proceedings/1063.pdf (accessed: June 20, 2023).
- Chertishchev V.Yu., Ospennikova O.G., Boichuk A.S., Dikov I.A., Generalov A.S. Determina-tion of the size and depth of defects in multilayer PCM honeycomb structures based on the mechanical impedance value. Aviaсionnye materialy i tehnologii, 2020, no. 3 (60), pp. 72–94. DOI: 10.18577/2071-9140-2020-0-3-72-94.
- Rusakov D., Chernushin V., Shelkovoy A. Theoretical and practical justification of high-precision of defects in multilayer polymer honeycomb structures by the honeycomb filler height reduction method. Journal of Physics: Conference Series, 2020, vol. 1636. Available at: http://www.researchgate.net/publication/346163891_Theoretical_and_practical_justification_of_high-precision_of_defects_in_multilayer_polymer_honeycomb_structu-res_by_the_honeycomb_filler_height_reduction_method (accessed: July 19, 2023).
- Kuryatin A., Rusakov D., Chernushin V. Identification of defect type in non-destructive testing of polymer composite structures. Journal of Physics: Conference Series, 2020, vol. 1636. Available at: https://iopscience.iop.org/article/10.1088/1742-6596/1636/1/012020 (accessed: July 19, 2023).
- Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.