Features of manufacturing complex contour parts from metal-polymer composite material
Antipov V.V., Nefedova Yu.N., Sidelnikov V.V., Somov A.V. Features of manufacturing complex contour parts from metal-polymer composite material // Proceedings of VIAM. 2023. No. 12. DOI: 10.18577/2307-6046-2023-0-12-63-73. URL: https://www.viam-works.ru/en/journal/2023/12/6
Keywords
metal-polymer composite materials, shaping, helicopter engine cowling, lower wing skin, deformation
Abstract
The article discusses the main features of the process of forming parts of complex configurations such as helicopter engine hood and the lower skin of an aircraft wing panel made of metal-polymer composite material. The stages of the technological process of forming these parts are described in detail. The results of determining the mechanical and fatigue characteristics are presented. samples of various reinforcement schemes from metal-polymer composite material. It is shown that the use of metal-polymer composite materials will simplify the manufacturing technology of complex contour parts and significantly increase the material utilization rate.
Reference list
- Antipov V.V., Serebrennikova N.Yu., Konovalov A.N., Nefedova Yu.N. Perspectives of application of fiber metal laminate materials based on aluminum alloys in aircraft design. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 45–53. DOI: 10.18577/2071-9140-2020-0-1-45-53.
- Kablov E.N., Antipov V.V., Girsh R.I., Serebrennikova N.Yu., Konovalov A.N. Constructed layered materials based on sheets of aluminum-lithium alloys and fiberglass in the structures of new generation aircraft. Vestnik mashinostroyeniya, 2020, no. 12, pp. 46–52.
- Zichenkov M.Ch., Shanygin A.N. New generation hybrid aircraft structures for advanced civil aircraft. Polet, 2018, no. 11, pp. 106–114.
- Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Adhesive prepregs and layered materials on their basis. Aviacionnye materialy i tehnologii, 2013, no. 2, pp. 19–21.
- Fridlyander I.N. Modern aluminum, magnesium alloys and composite materials based on them. Metallovedeniye i termicheskaya obrabotka metallov, 2002, no. 7, pp. 24–29.
- Fridlyander I.N., Senatorova O.G., Anikhovskaya L.I., Sidelnikov V.V., Dementeva L.A. Layered metalpolymer composites. Mechanical engineering: encyclopedia in 40 vol. Moscow: Mashinostroyenie, 2001, vol. II-3: Non-ferrous metals and alloys. Composite metal materials. Ed. I.N. Friedlander et al., рр. 818–832.
- Fridlyander I.N., Senatorova O.G., Anikhovskaya L.I. et al. Glued metal and layered metal-polymer composites. Mechanical engineering: encyclopedia in 40 vol. Moscow: Mashinostroyenie, 2001, vol. II-3: Non-ferrous metals and alloys. Composite metal materials. Ed. I.N. Friedlander et al., pp. 814–818.
- Roebroeks G. GLARE features. Fibre Metal Laminates. Dordrecht: Springer, 2001, рр. 23−37.
- Beumler Th. Flying GLARE: PhD Thesis. Delft: Delft University of Technology, 2004, 460 p.
- Vlot A. GLARE history of development of a new aircraft material. Kluwer Academic Publishers, 2001, р. 222.
- Bucci R.J., Kulak M., Heinimann M.B. et al. Large Panel Validation of Advanced Metallic and Hybrid Structural Concepts for Next-Gen Transport Aircraft. AeroMat 2007. Baltimore, 2007. Available at: https://asm.confex.com/ (accessed: September 08, 2023).
- Gunnink J.W., Vlot A., De Vries T.J., Van Der Hoeven W. GLARE technology development 1997–2000. Applied Composite Materials, 2002, vol. 9, is. 4, pp. 201–219.
- Gisario A., Barletta M. Laser forming of glass laminate aluminium reinforced epoxy (GLARE): On the role of mechanical, physical and chemical interactions in the multi-layers material. Optics and Lasers in Engineering, 2018, vol. 110, pp. 364–376.
- Qi С., Zhidong G., Zengshan L. et al. Experimental investigation on impact performances of GLARE laminates. Chinese Journal of Aeronautics, 2015, vol. 28, is. 6, pp. 1784–1792.
- Sang Y.P., Won J.C., Chi H.C., Heung S.C. Effect of drilling parameters on hole quality and delamination of hybrid GLARE laminate. Composite Structures, 2018, vol. 185, pp. 684–698.
- Fredell R.S., Gunnink J.W., Bucci R.J., Hinrichsen J. «Care-free» hybrid wing structures for aging USAF transports. First International Conference on Damage Tolerance of Aircraft Structures. Delft: Delft University of Technology, 2007. Available at: https://www.researchgate.net (accessed: September 07, 2023).
- Lavrov A.V., Erasov V.S., Podzhivotov N.Yu., Avtaev V.V. Optimization of structure of hybrid composition materials for aircraft. Trudy VIAM, 2016, no. 11 (47), paper no. 07. Available at: http://www.viam-works.ru (accessed: September 07, 2023). DOI: 10.18577/2307-6046-2016-0-11-7-7.
- Antipov V.V., Zaitsev M.D., Rodchenko T.S., Stoyda Yu.M., Serebrennikova N.Yu., Sidelnikov V.V. Study of the durability of a structurally similar sample of a fuselage panel with SIAL aluminum fiberglass skin. Deformatsiya i razrusheniye materialov, 2021, no. 3, pp. 18–24.
- Oreshko E.I., Erasov V.S., Lashov O.A., Podzhivotov N.Yu., Kachan D.V. Calculation of tension in a layered material. Trudy VIAM, 2018, no. 10 (70), paper no. 11. Available at: http://viam-works.ru (accessed: September 08, 2023). DOI: 10.18577/2307-6046-2018-0-10-93-106.
- Oreshko E.I., Erasov V.S., Podjivotov N.Yu. Arrangement of high-modular layers in a multilayer hybrid plate for its greatest resistance to stability loss. Aviacionnye materialy i tehnologii, 2014, no. S4, pp. 109–117. DOI: 10.18577/2071-9140-2014-0-S4-109-117.
- Pekarsh A.I., Oleynikov A.I., Bakaev V.V., Sarykov S.E., Dolgopolik O.D. Preparation for the production of complex parts of double alternating curvature using the method of finite element analysis of the geometric model with the integrated development of forming equipment, part development and recommendations for the technological process. SAPR i grafika, 2009, no. 2, pp. 88–96.
- Antipov V.V., Samokhvalov S.V., Sidelnikov V.V., Nefedova Yu.N., Ogurtsov P.S., Solo-viev V.A. Development and research of fire-resistant aluminum fiberglass for a helicopter engine cowling. Deformatsiya i razrusheniye materialov, 2022, no. 5, pp. 19–25.
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N., Antipov V.V., Oglodkova Yu.S., Oglodkov M.S. Experience and prospects for the use of aluminum-lithium alloys in aviation and space technology products. Metallurg, 2021, no. 1, pp. 62–70.
- Oglodkova Yu.S., Selivanov A.A., Lukina E.A., Zaitsev D.V. The influence of temperature-time parameters of stepwise aging on the structure, phase composition, mechanical and corrosion properties of sheets made of alloy 1441. Metally, 2020 no. 6, pp. 12–21.
- Оглодков М.С., Щетинина Н.Д., Рудченко А.С., Пантелеев М.Д. Направления развития перспективных алюминий-литиевых сплавов для авиационно-космической техники (обзор). Авиационные материалы и технологии. 2020. № 1 (58). С. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
- Щетинина Н.Д., Рудченко А.С., Селиванов А.А. Применение методов математического моделирования при разработке режимов деформации алюминий-литиевых сплавов (обзор). Труды ВИАМ. 2020. № 8 (90). Ст. 03. URL: http://www.viam-works.ru (дата обращения: 08.09.2023). DOI: 10.18577/2307-60246-2020-0-8-20-34.
- Oglodkov M.S., Shchetinina N.D., Rudchenko A.S., Panteleev M.D. Directions of the development of promising aluminum-lithium alloys for aero-space engineering (review). Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 19–29. DOI: 10.18577/2071-9140-2020-0-1-19-29.
- Fridlyander I.N., Kolobnev N.I., Sandler V.S. Aluminum-lithium alloys. Mechanical engineering: encyclopedia in 40 vols. Moscow: Mashinostroyenie, 2001, vol. II-3: Non-ferrous metals and alloys. Composite metal materials. Ed. I.N. Fridlander et al., pp. 156–185.
- Smith А. Aluminium-lithium alloys in helicopter airframes. Aerospace materials, 2001. Available at: http://www.slideshare.net (accessed: September 08, 2023).
- Gudladt H.-J., Lendvai J., Schneider J. Precipitation strengthening and its influence in the mechanical behavior of cyclically deformed Al–Li alloys. Acta Metall, 1989, vol. 37, no. 12, pp. 3327–3333.
- Grigorev M.V., Oglodkov M.S. Influence of machining on mechanical and fatigue properties of sheets from aluminum-lithium alloys 1441 and V-1481. Trudy VIAM, 2018, no. 4 (64), paper no. 03. Available at: http://www.viam-works.ru (accessed: September 07, 2023). DOI: 10.18577/2307-6046-2018-0-4-20-27.
- Duyunova V.A., Nechaikina T.A., Oglodkov M.S., Yakovlev A.L., Leonov A.A. Promising developments in the field of light materials for modern aerospace technology. Tekhnologiya legkikh splavov, 2018, no. 4, pp. 28–43.