Trends in the development of matte wear-resistant paint coatings

Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Zheleznyak V.G.
Kuznetsova V.A., Timoshina E.A., Shapovalov G.G., Zheleznyak V.G. Trends in the development of matte wear-resistant paint coatings // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-132-144. URL: https://www.viam-works.ru/en/journal/2023/10/12
Keywords
fillers, adhesion, physical and mechanical properties, wear resistance, decorative properties
Abstract

The main development trends in the field of creating matte, wear-resistant paint and varnish coatings for painting instrument panels and aircraft cockpit elements are considered. The basic principles that should be followed when creating matte, wear-resistant paint and varnish coatings have been identified. The basic requirements that determine the selection of the main components for obtaining a matte wear-resistant coating are considered. Polymer film-forming agents and fillers have been identified for the development of coating compositions in accordance with the analysis. Leaders in the development of matte wear-resistant coatings have been identified.

Reference list
  1. Kablov E.N. Aviation materials science in the 21st century. Prospects and objectives. Aviation materials. Selected works of VIAM 1932–2002. Moscow: MISIS–VIAM, 2002, pp. 23–47.
  2. Kablov E.N. New generation materials – the basis of innovation, technological leadership and national security of Russia. Intellekt i tekhnologii, 2016, no. 2 (14), pp. 16–21.
  3. Zheleznyak V.G. Modern paint and varnish materials for use in aviation equipment products. Trudy VIAM, 2019, no. 5 (77), paper no. 07. Available at: http://www.viam-works.ru. (accessed: August 17, 2023). DOI: 10.18577/2307-6046-2019-0-5-62-67.
  4. Kondrashov E.K., Kuznetsova V.A., Semenova L.V., Lebedeva T.A. The main directions for increasing the performance properties, technological and environmental characteristics of paint and varnish coatings for aviation equipment. Rossiyskiy khimicheskiy zhurnal, 2010, vol. LIV, no. 1. pp. 96–102.
  5. Problems of protective coatings: Review of materials of the European conference “Protective coating”. Dusseldorf (Germany). Lakokrasochnyye materialy i ikh primenenie, 2013, no. 9. pp. 33–35.
  6. Kuznetsova V.A., Marchenko S.A., Emelyanov V.V., Zheleznyak V.G. Study of the influence of molecular mass of epoxy oligomers and hardeners on the operational properties of paint coatings. Aviation materials and technology, 2021, no. 1 (62), paper no. 07. Available at: http://www.journal.viam.ru (accessed: August 17, 2023). DOI: 10.18577/2713-0193-2021-0-1-71-79.
  7. Pavlyuk B.Ph. The main directions in the field of development of polymeric functional materials. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 388–392. DOI: 10.18577/2071-9140-2017-0-S-388-392.
  8. Kuznetsova V.A., Shapovalov G.G., Marchenko S.A., Kovrizhkina N.A., Silaeva A.A. Paint coatings on the basis of epoxy and acrylic diphasic polymeric system for coloring of elements of cabin of pilots and dashboards. Trudy VIAM, 2020, no. 12 (94), paper no. 09. Available at: http://www.viam-works.ru (accessed: June 27, 2023). DOI: 10.18577/2307-6046-2020-0-12-87-95.
  9. Evtyukhov N.Z., Dubnova L.N. Mashlyakovsky Matte coatings made of epoxy powder coatings with low-temperature curing. Lakokrasochnyye materialy i ikh primenenie, 2008, no. 10, pp. 20–23.
  10. Merkulova Yu.I., Kuznetsova V.A., Kodachenko E.N., Zheleznyak V.G. Study of the influence of the primer layer’s chemical nature on the properties of the coating system based on fluoropolyurethane enamel. Aviation materials and technologies, 2022, no. 1 (66), paper no. 09. Available at: http://www.journal.viam.ru (ассеssed: September 14, 2023). DOI: 10.18577/2713-0193-2022-0-1-110-119.
  11. Merkulova Yu.I., Kuznetsova V.A., Novikova T.A. Investigation of properties of coating system based on fluorine polyurethane enamel and primer with low toxical pigment content. Trudy VIAM, 2019, no. 5 (77), paper no. 08. Available at: http://www.viam-works.ru. (accessed: August 06, 2023). DOI: 10.18577/2307-6046-2019-0-5-68-75.
  12. Kuznetsova V.A., Yemelyanov V.V., Shapovalov G.G., Kovrizhkina N.A. Use of modifiers for increase of operational properties of paint coatings on the basis of the epoxy film-forming (review). Trudy VIAM, 2021, no. 12 (106), paper no. 08. Available at: http://www.viam-works.ru (accessed: June 27, 2023). DOI: 10.18577/2307-6046-2021-0-12-63-72.
  13. Chebotareva E.G., Ogrel L.Yu. Current trends in the modification of epoxy oligomers. Fundamentalnye issledovaniya, 2008, no. 4, pp. 102–104.
  14. Kablov E.N. Main directions of development of materials for aerospace technology of the 21st century. Perspektivnyye materialy, 2000, no. 3, pp. 27–36.
  15. Kablov E.N. Without new materials – there is no future // Metallurg, 2013, no. 12, pp. 23–47.
  16. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  17. Shitova T.A., Evtyukhov N.Z., Yakovlev A.D., Shibalovich V.S. Methods for obtaining matte coatings. Lakokrasochnyye materialy i ikh primenenie, 1982, no. 3, рр. 44–46.
  18. Fortunin V.I., Ovchinnikova N.G. Preparation and properties of microporous perchlorovinyl coatings. Lakokrasochnyye materialy i ikh primenenie, 1980, no. 3, pp. 21–22.
  19. Fedyakova N.V., Pavlov A.V., Zelenskaya A.D., Shcherbina A.A. Influence of degree of a pigmentirovaniye on shine of alkidno-uretanovy enamels. Lakokrasochnyye materialy i ikh primenenie, 2023, no. 14, pp. 28–32.
  20. Osovskaya I.I., Zvereva V.A. Powder polyester paint for polymer coatings. Vestnik Tverskogo gosudarstvennogo universiteta. Ser.: Khimiya, 2018, no. 2, pp. 111–117.
  21. Gorbunov D.F. Highly effective matting additives from Degussa. Lakokrasochnyye materialy i ikh primenenie, 2006, no. 2–3, pp. 18–19.
  22. Titova I.E. Organic matting agent Deuteron – a new approach to creating coatings with specified properties. Lakokrasochnyye materialy i ikh primenenie, 2008, no. 12, pp. 32–34.
  23. Kovrizhkina N.A., Kuznetsova V.A., Silaeva A.A., Marchenko S.A. Ways to improve the properties of paint coatings by adding different fillers (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 41–48. DOI: 10.18577/2071-9140-2019-0-4-41-48.
  24. Yoryu Xu, Gibelhas I. Utopia or reality? Higher dosage of matting additive with outstanding viscosity reduction in 100% UV systems. Lakokrasochnyye materialy i ikh primenenie, 2020, no. 10, pp. 18–24.
  25. Composition for coatings: pat. 2335521 Rus. Federation; appl. 04.07.07; publ. 10.10.08.
  26. Fluoroplastic paint and varnish material for coatings: pat. 2532192 Rus. Federation; appl. 07.05.13; publ. 27.10.14.
  27. Composition for barrier coating: pat. 462493 Rus. Federation; appl. 05.04.11; publ. 27.10.14.
  28. Paint and varnish composition of alkyd-urethane enamel: pat. 2351625 Rus. Federation; appl. 28.11.07; publ.10.04.09.
  29. Method for producing alkyd-urethane enamel: pat. 2346967 Rus. Federation; appl. 28.11.07; publ. 20.02.09.
  30. Polyurethane composition for coatings: pat. 2298573 Rus. Federation; appl. 11.05.05; publ. 27.06.05.
  31. Epoxy-rubber composition for protective coatings: pat. 2550864 Rus. Federation; appl. 06.08.13; publ. 20.05.15.
  32. Kuznetsova V.A., Deev I.S., Zheleznyak V.G., Silaeva A.A. Anti wear coating with quasicrystal filler. Trudy VIAM, 2018, no. 3 (63), paper no. 08. Available at: http://www.viam-works.ru (accessed: August 28, 2023). DOI: 10.18577/2307-6046-2018-0-3-68-76.
  33. Kuznetsova V.A., Marchenko S.A., Zheleznyak V.G., Emelyanov V.V. Influence of the spatial structure of reinforcing fillers on the properties of the paint coatings. Trudy VIAM, 2020, no. 9 (91), paper no. 11. Available at: http://www.viam-works.ru (accessed: August 28, 2023). DOI: 10.18577/2307-6046-2020-0-9-96-104.
  34. Silaeva A.A., Kuznetsova V.A., Kurshev E.V., Timoshina E.A. Influence of the dimensions of the reinforcing filler on the technological and functional properties of paints and varnishes. Materialovedenie, 2022, no. 2, pp. 32–38.
  35. Lygdenov V.Ts., Syzrantsev V.V., Bardakhanov S.P. et al. Study of the influence of silicon dioxide nanoparticles on the properties of paint and varnish coating made of perchlorovinyl enamel. Prikladnaya mekhanika i tekhnicheskaya fizika, 2020, vol. 61, no. 5, pp. 246–254.
  36. Nomoev A.V., Lygdenov V.Ts., Bardakhanov S.P. The influence of silicon dioxide nanopowder on the wear resistance of paint and varnish coatings. Nanotekhnologii v stroitelstve: nauchnyy internet-zhurnal, 2010, vol. 2, no. 3, pp. 19–24. URL: http://www.sciup.org (accessed: August 28, 2023).
  37. Valko N.G., Globa A.I. Kasperovich A.V., Dukhovich Yu.V. Structure and properties of paint and varnish coatings modified with hollow glass microspheres. Vestnik GGU im. Yanki Kupaly, 2020, vol. 10, no. 2, pp. 95–102.
  38. Mzhachikh E.I., Sukhareva L.V., Yakovlev V.S. Factors that determine the durability of polymer coatings. Izvestiya vysshikh uchebnykh zavedeniy. Ser.: Khimiya i khimicheskaya tekhnologiya, 2006, vol. 49, no. 2, pp. 108–109.
  39. Nitro-wear resistant matte black paint: pat. CN 102746747; appl. 28.06.12; publ. 05.12.12.
  40. Polyurethane transparent matt topcoat, preparation method and use method thereof: pat. CN 101381581; appl. 27.10.08; publ. 11.03.09.
  41. Scratch-resistant soft full-matt finishing paint as well as preparation method and application thereof: pat. CN 114702890; appl. 12.04.22; publ. 05.07.22.
  42. Polyurethane matte finishing coat for automatically coating wood ware and preparing method thereof: pat. CN 105131824; appl. 01.09.15; publ. 09.12.15.
  43. High solid anti-scratching unsaturated polyester matte top-coat for coating wooden products: pat. CN 103173109; appl. 23.12.11; publ. 26.03.13.
  44. Ma Hui, Liu Yucun, Guo Jiahu et al. Synthesis of a novel silica modified environmentally friendly waterborne polyurethane matting coating. Progress in Organic Coatings, 2020, vol. 139, pp. 231–242.
  45. Tionyou Wang, Zhe Sun, Feifei Liang et al. Poly(methylmethacrylate) microspheres with matting characteristic prepared by dispersion polymerization. International Journal of polymer Analysis and Characterization, 2019, vol. 24, pp. 731–740.
  46. Anti wear coatings: pat. US 7268179; appl. 30.09.03; publ. 11.09.07.
  47. Abrasion resistant coatings: pat. US 7736745; appl. 24.05.05; publ. 15.01.10.
  48. Method of making matte airfoil coatings: pat. US 8124235 B2; appl. 11.01.10; publ. 28.02.12.
  49. Scuff resistant and chip resistant architectural compositions: pat. US 11230645; appl. 05.05.17; publ. 25.01.22.
  50. Calvez I., Szczepanski C.R., Landry V. Preparation and characterization of low gloss UV-curable coating based on silica surface modification using an acrylate monomer. Progress in Organic Coatings, 2021, vol. 158, pp. 476–483.
  51. Fluorinate polyacrylate coating composition, the preparation method therefore and use thereof: pat. EP 3732221; appl. 21.12.18; publ. 23.02.22.
  52. Jian Zhang, Wen-Guang Lu, Hui Yan et al. Improvement of wear-resistance and anti-corrosion of waterborne epoxy coating by synergistic modification of glass flake with phytic acid and Zn2+. Ceramics International, 2023, vol. 49, no. 11, pp. 17910–17920.
  53. Two-component composition for producing flexible polyurethane gel coats: pat. WO 2005030893; appl. 23.09.03; publ. 16.09.04.
  54. Aqueous base paint for producing a coating: pat. WO 2016188655; appl. 22.05.15; publ. 01.12.16.
  55. Fluorinate polyacrylate coating composition, the preparation method therefore and use thereof: pat. EP 3732221; appl. 21.12.18; publ. 23.02.22.
  56. Scrinzi E., Rossi S., Kamarchik P., Deflorian F. Evaluation of durability of nano-silica containing clear coats for automotive applications. Progress in Organic Coatings, 2011, vol. 71, no. 4, pp. 384–390.
  57. Wittmann B., Montmitonnet P., Burr A. et al. BRDF and gloss computation of polyurethane coatings from roughness measurements: Modelling and experimental validation. Progress in Organic Coatings, 2021, vol. 156, pp. 365–373.
  58. Uribe-Padilla J., Graells-Sobre M., Salgado-Valle J. A novel contribution to the modeling of the matting efficiency of aqueous polyurethane dipersions. Progress in Organic Coatings, 2017, vol. 109, pp. 179–185.
  59. Lopez A.B., Bohуrquez S.J., Meeuwisse M. et al. Self-matting waterborne fluoropolymers. Progress in Organic Сoatings, 2018, vol. 116, pp. 57–69.