Formation of carbon coatings in the process of methane pyrolysis by the chemical vapor deposition
Sidorov D.V., Grunin А.А., Shavnev A.A. Formation of carbon coatings in the process of methane pyrolysis by the chemical vapor deposition // Proceedings of VIAM. 2023. No. 10. DOI: 10.18577/2307-6046-2023-0-10-105-118. URL: https://www.viam-works.ru/en/journal/2023/10/10
Keywords
methane pyrolysis, pyrolytic carbon, chemical reaction, reagent
Abstract
The article presents a review of the scientific and technical literature in the field of methane pyrolysis in the process of chemical vapor deposition of pyrolytic carbon, summarizes the results of studies of the process depending on the parameters of deposition and the substrates used, analyzes the compositions of pyrolysis products, mechanisms and pathways of chemical reactions.
Reference list
- Kablov E.N., Echin A.B., Bondarenko Yu.A. History of development of directional crystallization technology and equipment for casting blades of gas turbine engines. Trudy VIAM, 2020, no. 3 (87), paper no. 01. Available at: http://www.viam-works.ru (accessed: May 11, 2023). DOI: 10.18577/2307-6046-2020-0-3-3-12.
- Kablov E.N., Semenova S.N., Suleymanov R.R., Chaykun A.M. Prospects for the use of ethylene-propylenediene rubber as part of cold resistant rubber. Trudy VIAM, 2019, no. 12 (84), paper no. 4. Available at: http://www.viam-works.ru (accessed: accessed: May 11, 2023). DOI: 10.18577/2307-6046-2019-0-12-29-36.
- Kablov E.N., Valueva M.I., I.V. Zelenina, Khmelnitskiy V.V., Aleksashin V.M. Carbon plastics based on benzoxazine oligomers – perspective materials. Trudy VIAM, 2020, no. 1, paper no. 07. Available at: http://www.viam-works.ru (accessed: May 11, 2023). DOI: 10.18577/2307-6046-2020-0-1-68-77.
- Sidorov D.V., Schavnev A.A., Melentev A.A. Formation of silicon carbide coatings by chemical vapor deposition (review). Part 1. Trudy VIAM, 2021, no. 6 (100), paper no. 10. Available at: http://www.viam-works.ru (accessed: May 11, 2023). DOI: 10.18577/2307-6046-2021-0-6-100-111.
- Fialkov A.S. Carbon, interlayer compounds and composites based on it. Moscow: Aspect Press, 1997, 718 p.
- Nikolaev A.I. Preparation of carbon-carbon composite materials based on carbon nanofibers by gas-phase method. Tonkie khimicheskie tekhnologii, 2015, vol. 10, pp. 61–66.
- Jia K., Zhang J., Zhu Y. et al. Toward the commercialization of chemical vapor deposition graphene films. Applied Physics Reviews, 2021, vol. 8, pp. 400–401.
- Liu J., Hei L., Chen G. et al. Growth of ultrananocrystalline diamond films in an Ar-rich CH4/H2/Ar atmosphere with varying H2 concentrations. New Carbon Materials, 2013, vol. 28, pp. 134–138.
- Majewska J., Michalkiewicz B. Carbon nanomaterials produced by the catalytic decomposition of methane over Ni/ZSM-5: Significance of Ni content and temperature. New Carbon Materials, 2014, vol. 29, pp. 102–108.
- Park S.-S., Lee J.-Y. Nucleation behavior of diamond particles on silicon substrates in a hot-filament chemical vapour deposition. Journal of Materials Science, 1993, vol. 28, pp. 1799–1804.
- Li X., Magnuson C.W., Venugopal A. et al. Graphene Films with Large Domain Size by a Two-Step Chemical Vapor Deposition Process. Nano Letters, 2010, vol. 10, pp. 4328–4334.
- Amaral М., Oliveira F.J., Belmonte M. et al. Hot-filament chemical vapour deposition of nanodiamond on silicon nitride substrates. Diamond and Related Materials, 2004, vol. 13, pp. 643–647.
- Chen C.-J., Back M.H., Back R.A. The thermal decomposition of methane. II. Secondary reactions, autocatalysis and carbon formation; non-Arrhenius behavior in the reaction of CH3 with ethane. Canadian Journal of Chemistry, 1976, vol. 54, pp. 3175–3184.
- Palmer H.B., Lahaye J., Hou K.C. Kinetics and mechanism of the thermal decomposition of methane in a flow system. The Journal of Physical Chemistry, 1968, vol. 72, pp. 348–353.
- Knorre V.G., Kozlov G.I. Single-pulse shock tube studies on the kinetics of the thermal decomposition of methane. Combustion and Flame, 1962, vol. 6, pp. 253–263.
- Kevorkian B.V., Heath C.E., Boudart M. The decomposition of methane in shock waves. The Journal of physical chemistry, 1960, vol. 64, p. 964.
- Hartig R., Troe J., Wagner H.G.G. Thermal decomposition of methane behind reflected shock waves. Symposium (International) on Combustion, 1971, vol. 13, pp. 147–154.
- Dors M., Nowakowska H., Jasin´sk J., Mizeraczyk J. Chemical kinetics of methane pyrolysis in microwave plasma at atmospheric pressure. Plasma Chemistry and Plasma Processing, 2013, vol. 34, pp. 313–326.
- Hu C., Li H., Zhang S., Li W. A molecular-level analysis of gas-phase reactions in chemical vapor deposition of carbon from methane using a detailed kinetic model. Journal of Materials Science, 2016, vol. 51, pp. 3897–3906.
- Norinaga K., Deutschmann O. Detailed Kinetic Modeling of Gas-Phase Reactions in the Chemical Vapor Deposition of Carbon from Light Hydrocarbons. Industrial & Engineering Chemistry Research, 2007, vol. 46, pp. 3547–3557.
- Li K., Li H., Yan N. et al. Conversion of methane to benzene in CVI by density functional theory study. Scientific Reports, 2019, vol. 6, p. 19496.
- Shinde V.M., Pradeep P. Detailed Gas-Phase Kinetics and Reduced Reaction Mechanism for Methane Pyrolysis involved in CVD/CVI Processes. Journal of Analytical and Applied Pyrolysis, 2021, vol. 154, p. 104998.
- Becker A., Hüttinger K.J. Chemistry and kinetics of chemical vapour deposition of pyrocarbon: IV. Рyrocarbon deposition from methane in the low-temperature regime. Carbon, 1998, vol. 36, pp. 213–224.
- Brüggert M., Hu Z., Hüttinger K.J. Chemistry and kinetics of chemical vapour deposition of pyrocarbon: VI. Influence of temperature using methane as a carbon source. Carbon, 1999, vol. 37, pp. 2021–2030.
- Birakayala N., Evans A. A reduced reaction model for carbon CVD/CVI processes. Carbon, 2002, vol. 40, pp. 675–683.
- Li H., Li A., Bai R., Li K. Numerical simulation of chemical vapour infiltration of propylene into C/C composites with reduced multi-step kinetic models. Carbon, 2005, vol. 43, pp. 2937–2950.
- Xu W., Zhang Z.-W., Bai R.-C. et al. Kinetic model of gas-phase reactions in the chemical vapor deposition of propane. Carbon, 2014, vol. 71, p. 345.