Study mechanism formation a surface layer metal composite material based on Mo–Si–B system after high-temperature influence at different angles of attack

Lutsenko A.N., Efimochkin I.Yu., Moiseeva N.S.
Lutsenko A.N., Efimochkin I.Yu., Moiseeva N.S. Study mechanism formation a surface layer metal composite material based on Mo–Si–B system after high-temperature influence at different angles of attack // Proceedings of VIAM. 2023. No. 1. DOI: 10.18577/2307-6046-2023-0-1-84-96. URL: https://www.viam-works.ru/en/journal/2023/1/7
Keywords
metal composite material, molybdenum, high temperature heating, phase composition, surface layer
Abstract

The paper analyzes the changes phase composition of the surface layer metal composite material base on Mo–Si–B system, reinforced with dispersed particles Al2O3 oxide. The main stages formation phase composition surface layer with a thickness of 0–250 microns at an exposure temperature of 1300–2100 °C have been established by x-ray phase analysis. It is established that protective amorphous phase is formed at temperature of 1700 °C. At a heating temperature of 1900 °C and above, the glassy layer ablates, which leads to oxidation of the near-surface layers of the base material.

Reference list
  1. Grashchenkov D.V., Efimochkin I.Yu., Bolshakova A.N. High-temperature metal-matrix composite materials reinforced with particles and fibers of refractory compounds. Aviacionnye materialy i tehnologii, 2017, no. S, pp. 318–328. DOI: 10.18577/2071-9140-2017-0-S-318-328.
  2. Morgunova N.N., Klypin B.A., Boyarshnov V.A. et al. Alloys of molybdenum. Moscow: Metallurgiya, 1975, 392 p.
  3. Karashaev M.M., Bazyleva O.A., Shestakov A.V., Ovsepyan S.V. Technological principles for the development of metal composite materials reinforced with oxide and intermetallic particles. Aviacionnye materialy i tehnologii, 2020, no. 3 (60), pp. 29–36. DOI:10.18577/2071-9140-2020-0-3-29-36.
  4. Majumdar S., Schliephake D., Gorr B. et al. Effect of Yttrium Alloying on Intermediate to High-Temperature Oxidation Behavior of Mo–Si–B Alloys. Metallurgical and Materials Transactions A, 2013, vol. 44, no. 5, pp. 2243–2257.
  5. Perepezko J.H., Sakidja R. Environmental Resistance of Mo–Si–B Alloys and Coatings. Oxidation of Metals, 2013, vol. 80, no. 3, pp. 207–218. DOI: 10.1007/S11085-013-9373-3.
  6. Kablov E.N., Zhestkov B.E., Grashchenkov D.V., Sorokin O.Yu., Lebedeva Yu.E., Vaganova M.L. Investigation of the Oxidative Resistance of High-Temperature Coating Based on a SiC Material under Exposure to High-Enthalpy Flow. High Temperature, 2017, vol. 55, no. 6, pp. 873–879.
  7. Chollacoop N., Alur A.P., Kumar K.S. Microstructural Finite Element Analysis of Mo–Si–B Alloy in High Temperature Applications. Journal of Visualization, 2005, vol. 8, no. 4, p. 292.
  8. Kablov E.N. Materials of a new generation and digital technologies for their processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  9. Kablov E.N. The role of fundamental research in the creation of new generation materials. Reports of XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  10. Hönigschmid O. Über das Molydänsilicid MoSi2, das Wolframsilicid WSi2 und das Tantalsilicid TaSi2. Monatshefte für Chemie und verwandte Teile anderer Wissenschaften, 1997, vol. 28, pp. 1017–1028.
  11. Vasudevan K., Petrovic J.J. A comparative overview of MoSi2 based composites. Material Science and Engineering A-structural Materials Properties Microstructure and Processing, 1992, vol. 155, pp. 1–17.
  12. Oxidation resistant molybdenum: pat. US 6652674-B1; filed 19.07.02; publ. 25.11.03.
  13. Jung J.-I., Zhou N., Luo J. Effects of sintering aids on the densification of Mo–Si–B alloys. Journal of Materials Science, 2012, vol. 47, no. 24, pp. 8308–8319.
  14. Titov D.D., Kargin Yu.F., Lysenkov A.S. et al. Effect of WSi2 content and additives of magnesium aluminosilicates on the oxidation and strength properties of MoSi2–WSi2 composites. Materialovedenie, 2012, no. 7, pp. 45–49.
  15. Batiyenkov R.V., Bolshakova A.N., Efimochkin I.Yu. The problem of low-temperature plasticity of molybdenum and alloys based on it (review). Trudy VIAM, 2018, no. 3 (63), paper no. 02. Available at: http://www.viam-works.ru (accessed: June 28, 2022). DOI: 10.18577/2307-6046-2018-0-3-12-17.
  16. Middlemas M.R., Cochran J.K. The microstructural engineering of Mo–Si–B alloys produced by reaction synthesis. JOM, 2010, vol. 62, no. 10, pp. 20–24.
  17. Molybdenum: collection of articles. Trans. from Engl. Ed. A.K. Nathanson. Moscow: Publ. House of foreign literature, 1959, 304 p.
  18. Lutsenko A.N., Efimochkin I.Yu., Moiseeva N.S. Study mechanism of creation structure on composite material based on molybdenum after high-temperature influence. Trudy VIAM, 2022, no. 4 (110). paper no. 04. Available at: http://www.viam-works.ru (accessed: May 16, 2022). DOI: 10.18577/2307-6046-2022-0-4-32-41.
  19. Babashov V.G., Maksimov V.G., Varrik N.M., Samorodova O.N. Studying of structure and pro-perties of samples of ceramic composite materials on the basis of mullite. Aviacionnye materialy i tehnologii, 2020, no. 1 (58), pp. 54–63. DOI: 10.8577/2071-9140-2020-0-1-54-63.
  20. Schneider H., Schreuer J., Hildmann B. Structure and properties of mullite – A review. Journal of the European Ceramic Society, 2008, no. 28, pp. 329–344.