Assessment of results by means of the analysis of variance method

Podzhivotov N.Y.
Podzhivotov N.Y. Assessment of results by means of the analysis of variance method // Proceedings of VIAM. 2022. No. 8. DOI: 10.18577/2307-6046-2022-0-8-141-152. URL: https://www.viam-works.ru/en/journal/2022/8/12
Keywords
one-factor dispersion analysis, the analysis of variance method, assessment of characteristics of materials, levels of properties, statistical analysis, skill test
Abstract

The application of the method of single-factor analysis of variance is considered on the example of evaluating the results of mechanical tests of a metallic structural material (aluminum alloy). Analysis of variance is proposed to be used as a simple but effective method for the rapid assessment and/or control of the levels of material properties based on the results of physical and mechanical tests, as well as for the assessment and control of the uniformity and stability of experimental data obtained during circular interlaboratory or qualification tests.

Reference list
  1. Kablov E.N. The strategic directions of development of materials and technologies of their processing for the period to 2030. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 7–17.
  2. Kablov E.N., Podzhivotov N.Yu., Lutsenko A.N. On the need to create a unified information and analytical center for aviation materials of the Russian Federation. Problemy mashinostroyeniya i avtomatizatsii, 2019, no. 3, pp. 28–34.
  3. Kablov E.N., Grinevich A.V., Erasov V.S. Characteristics of the strength of metallic aviation materials and their calculated values. 75 years. Aviation materials. Moscow: VIAM, 2007, pp. 370–379.
  4. Mitrakov O.V., Yakovlev N.O., Yakusheva N.A., Grinevich A.V. Destruction features of steel 20ХГСН2МФА-ВД during the fracture toughness test. Aviacionnye materialy i tehnologii, 2019, no. 1 (54), pp. 49–56. DOI: 10.18577/2071-9140-2019-0-1-49-56.
  5. Dimitrienko Yu.I., Gubareva E.A., Sborshchikov S.V., Erasov V.S., Yakovlev N.O. Numerical modeling and experimental study of deformation of elastoplastic plates under collapse. Matematicheskoye modelirovaniye i chislennye metody, 2015, no. 1 (5), pp. 67–82.
  6. Oreshko E.I., Erasov V.S., Yastrebov A.S. Prediction of strength and deformation characteristics of materials during tensile and creep tests. Materialovedenie, 2019, no. 2, pp. 3–8.
  7. Yakovlev N.O., Erasov V.S., Petrova A.P. Comparison of the normative bases of various countries for testing adhesive joints of materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2014, no. 7, pp. 2–8.
  8. Grinevich A.V., Laptev A.B., Skripachev S.Yu., Nuzhnyj G.A. Matrix strength characteristics for the assessment of limit states of structural metallic materials. Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 67–74. DOI: 10.18577/2071-9140-2018-0-2-67-74.
  9. Grinevich D.V., Yakovlev N.O., Slavin A.V. The criteria of the failure of polymer matrix composites (review). Trudy VIAM, 2019, no. 7 (79), paper no. 11. Available at: http://viam-works.ru (accessed: February 25, 2022). DOI: 10.18577/2307-6046-2019-0-7-92-111.
  10. Yakovlev N.O., Gulyaev A.I., Krylov V.D., Shurtakov S.V. Microstructure and properties of structural composite materials during testing for static interlayer crack resistance. Novosti materialovedeniya. Nauka i tekhnika, 2016, no. 1 (19), paper no. 09. Available at: http://www.materialsnews.ru (accessed: February 7, 2022).
  11. Makhsidov V.V., Yakovlev N.O., Ilichev A.V. et al. Determination of the deformation of the material of a PCM structure using integrated fiber-optic sensors. Mekhanika kompozitsionnykh materialov i konstruktsii, 2016, vol. 22, no. 3, pp. 402–413.
  12. Yakovlev N.O., Grinevich D.V., Mazalov P.B. Mathematical modeling of the stress-strain state in compression of a mesh structure synthesized by the method of selective laser fusion. Vestnik Moskovskogo gosudarstvennogo tekhnicheskogo universiteta im. N.E. Baumana. Ser.: Natural sciences, 2018, no. 6 (81), pp. 113–127.
  13. Podzhivotov N.Yu. Express method of a comparative assessment properties levels of materials. Trudy VIAM, 2019, no. 10 (82), paper no. 11. Available at: http://www.viam-works.ru (accessed: February 25, 2022). DOI: 10.18577/2307-6046-2019-0-10-111-124.
  14. Podzhivotov N.Yu. On the optimization of the approach to substantiation of the minimum volume of testing of aviation structural materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2021, no. 1, pp. 28–35.
  15. Konovalov V.V., Dubinskiy S.V., Makarov A.D., Dotsenko A.M. Research of correlation dependencies between mechanical properties of aviation materials. Aviacionnye materialy
  16. i tehnologii, 2018, no. 2 (51), pp. 40–46. DOI: 10.18577/2071-9140-2018-0-2-40-46.
  17. Erasov V.S., Avtaev V.V., Oreshko E.I., Yakovlev N.O. Strain-controlled testing advantages at static tension and repeated-static tension. Trudy VIAM, 2018, no. 9 (69), paper no. 10. Available at: http://www.viam-works.ru (accessed: February 25, 2022). DOI: 10.18577/2307-6046-2018-0-9-92-104.
  18. Pachurin G.V., Gushchin A.N., Galkin V.V., Pachurin V.G. Theoretical foundations for increasing the operational durability of stamped metal products: textbook. Nizhny Novgorod: NSTU, 2006, 176 p.
  19. Stepnov M.N. Statistical methods for processing the results of mechanical tests: a reference book. Moscow: Mashinostroenie, 1985, 232 p.
  20. Gmurman V.E. Guide to solving problems in probability theory and mathematical statistics: textbook for students of higher educational institutions. 3rd ed., rev. and add. Moscow: Vysshaya shkola, 1979, 400 p.